Back to results
US 2019/0337841 A1Published application
Coated articles with optical coatings having residual compressive stress
AssigneeCorning Incorporated
InventorsShandon Dee Hart, Guangli Hu, Charles Andrew Paulson, James Joseph Price
Life of this patent
Estimating the term…
Abstract
A coated article includes a substrate having a major surface, and an optical coating disposed on the major surface of the substrate. At least a portion of the optical coating includes a residual compressive stress of about 50 MPa or more. The coated article has strain-to-failure of about 0.5% or more as measured by a Ring-on-Ring Tensile Testing Procedure. The coated article has an average photopic transmission of about 80% or greater.
Claims18
A coated article comprising:
- a substrate comprising a major surface;
- an optical coating disposed on the major surface of the substrate and forming an air-side surface, the optical coating comprising one or more layers of deposited material;
- wherein:
- at least a portion of the optical coating comprises a residual compressive stress of more than about 50 MPa;
- the optical coating comprises a strain-to-failure of about 0.4% or more as measured by a Ring-on-Ring Tensile Testing Procedure;
- the optical coating comprises a maximum hardness of 12 GPa or more as measured on the air-side surface by a Berkovich Indenter Hardness Test along an indentation depth of about 50 nm and greater;
- and
- the coated article comprises an average photopic transmission of about 80% or greater.
5 more elements
A method for making a coated article, the method comprising:
- depositing an optical coating onto a major surface of a substrate, the optical coating forming an air-side surface and comprising one or more layers of deposited material;
- wherein:
- at least a portion of the optical coating comprises a residual compressive stress of more than about 50 MPa;
- the optical coating comprises a strain-to-failure of about 0.4% or more as measured by a Ring-on-Ring Tensile Testing Procedure;
- the optical coating comprises a maximum hardness of 12 GPa or more as measured on the air-side surface by a Berkovich Indenter Hardness Test along an indentation depth of about 50 nm and greater;
- and
- the coated article comprises an average photopic transmission of about 80% or greater.
4 more elements
Dependencies are inferred from the claim text.