# US 2019/0319259 A1 · Methods of preparing lithium metal anodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0319259 A1
- Document ID: US20190319259A1
- Status: Published application
- Kind: A1
- Application number: 15/955,319
- Filed: 2018-04-17
- Published: 2019-10-17
- Earliest claimed: 2018-04-17
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Michael P. Balogh; Hongliang Wang; Fang Dai; Tengjiao Qi
- Web page: https://patentgrep.com/patent/US20190319259A1

## CPC

- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/043: {involving compressing or compaction}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/405: {Alloys based on lithium}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lithium-based electrode assembly and methods of formation relating thereto are provided. The lithium-based electrode assembly comprises a metal current collector, an electrode comprising lithium metal, and an intermediate layer disposed therebetween. The intermediate layer comprising an intermetallic compound comprising the lithium metal of the electrode and a metal selected from the group consisting of: aluminum, silver, gold, barium, bismuth, boron, calcium, cadmium, carbon, gallium, germanium, mercury, indium, iridium, lead, palladium, platinum, rhodium, antimony, selenium, silicon, tin, strontium, sulfur, tellurium, zinc, and combinations thereof. The method of forming the lithium assembly includes coating a surface of the metal current collector with the intermediate layer; disposing the electrode onto an exposed surface of the intermediate layer; and heating the electrode, the intermediate layer, and the metal current collector to form the lithium intermetallic compound, which joins the metal current collector and the electrode together.

## Claims

### Claim 1

A method of forming a lithium-based electrode assembly, the method comprising:
coating a surface of a metal current collector with an intermediate layer comprising a metal selected from the group consisting of: silver (Ag), aluminum (Al), gold (Au), barium (Ba), bismuth (Bi), boron (B), calcium (Ca), cadmium (Cd), carbon (C), gallium (Ga), germanium (Ge), mercury (Hg), indium (In), iridium (Ir), lead (Pb), palladium (Pd), platinum (Pt), rhodium (Rh), antimony (Sb), selenium (Se), silicon (Si), tin (Sn), strontium (Sr), sulfur (S), tellurium (Te), zinc (Zn), and combinations thereof;
disposing an electrode comprising lithium metal onto an exposed surface of the intermediate layer; and
forming a lithium intermetallic compound comprising lithium metal from the electrode and the metal of the intermediate layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming comprises applying heat to the electrode and the intermediate layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the applied heat is from about 100° C. to about 300° C. and the heat is applied for a time ranging from about 1 minute to about 15 minutes.

### Claim 4 (depends on 2)

The method of claim 2, wherein the forming further comprises applying pressure to the electrode, the intermediate layer, and the metal current collector.

### Claim 5 (depends on 4)

The method of claim 4, wherein the applied pressure ranges from about 0.1 MPa to about 0.6 MPa and the pressure is applied for a time ranging from about 1 minute to about 15 minutes.

### Claim 6 (depends on 1)

The method of claim 1, wherein the metal current collector is selected from the group consisting of: copper (Cu), nickel (Ni), iron (Fe), titanium (Ti), chromium (Cr), and combinations thereof; and the metal current collector has a thickness ranging from about 1 μm to about 25 μm.

### Claim 7 (depends on 6)

The method of claim 6, wherein the intermediate layer has a thickness less than about 1 μm.

### Claim 8 (depends on 7)

The method of claim 7, wherein coating the surface of the metal current collector with the intermediate layer comprises depositing the metal of the intermediate layer on the surface of the current collector using a coating method selected from the group consisting of: electroplating, sputter coating, vacuum metallization, plasma vapor deposition, chemical vapor deposition, and combinations thereof.

### Claim 9 (depends on 7)

The method of claim 7, wherein the electrode has a thickness ranging from about 1 μm to about 20 μm.

### Claim 10 (depends on 9)

The method of claim 9, wherein disposing the electrode onto the exposed surface of the intermediate layer comprises contacting the electrode to the surface of the intermediate layer using a joining method selected from the group consisting of: lamination, thermal bonding, hot dipping, spot welding, laser welding, ultrasonic welding, and combinations thereof.

### Claim 11

A method of forming a lithium-based electrode assembly, the method comprising:
forming an intermediate layer on a surface of a metal current collector, wherein the intermediate layer comprises a metal selected from the group consisting of: silver (Ag), aluminum (Al), tin (Sn), zinc (Zn), and combinations thereof, and the metal current collector is selected from the group consisting of: copper (Cu), nickel (Ni), iron (Fe), titanium (Ti), and combinations thereof;
contacting an electrode comprising lithium metal and an exposed surface of the intermediate layer; and
heating the electrode and the intermediate layer to form a lithium intermetallic compound comprising lithium metal from the electrode and the metal of the intermediate layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the electrode and the intermediate layer are heated at a temperature ranging from about 100° C. to about 300° C. for a time ranging from about 1 minute to about 15 minutes; and
wherein forming the lithium intermetallic compound further comprises applying pressure to the electrode, the intermediate layer, and the metal current collector, wherein the applied pressure ranges from about 0.1 MPa to about 0.6 MPa and the pressure is applied for a time ranging from about 1 minute to about 15 minutes.

### Claim 13 (depends on 12)

The method of claim 12, wherein the electrode and the intermediate layer are heated at a temperature ranging from about 140° C. to about 180° C.

### Claim 14 (depends on 12)

The method of claim 12, wherein forming the intermediate layer on the surface of the metal current collector comprises depositing the metal on the surface of the current collector using a coating method selected from the group consisting of: electroplating, sputter coating, vacuum metallization, plasma vapor deposition, chemical vapor deposition, and combinations thereof; and
wherein contacting the electrode and the exposed surface of the intermediate layer comprises bonding the electrode to the surface of the intermediate layer using a joining method selected from the group consisting of: lamination, thermal bonding, hot dipping, spot welding, laser welding, ultrasonic welding, and combinations thereof.

### Claim 15

A lithium-based electrode assembly comprising:
a metal current collector;
an electrode comprising lithium metal; and
an intermediate layer disposed therebetween, wherein the intermediate layer comprises an intermetallic compound comprising the lithium metal of the electrode and a metal selected from the group consisting of: silver (Ag), aluminum (Al), gold (Au), barium (Ba), bismuth (Bi), boron (B), calcium (Ca), cadmium (Cd), carbon (C), gallium (Ga), germanium (Ge), mercury (Hg), indium (In), iridium (Ir), lead (Pb), palladium (Pd), platinum (Pt), rhodium (Rh), antimony (Sb), selenium (Se), silicon (Si), tin (Sn), strontium (Sr), sulfur (S), tellurium (Te), zinc (Zn), and combinations thereof.

### Claim 16 (depends on 15)

The electrode assembly of claim 15, wherein the metal current collector has a thickness ranging from about 1 μm to about 25 μm; the intermediate layer has a thickness less than about 1 μm; and the electrode has a thickness ranging from about 1 μm to about 20 μm.

### Claim 17 (depends on 16)

The electrode assembly of claim 16, wherein the metal is silver (Ag) and the lithium intermetallic compound is Li4Ag.

### Claim 18 (depends on 16)

The electrode assembly of claim 16, wherein the metal is zinc (Zn) and the lithium intermetallic compound is LiZn.

### Claim 19 (depends on 16)

The electrode assembly of claim 16, wherein the metal is aluminum (Al) and the lithium intermetallic compound is Li9Al4.

### Claim 20 (depends on 16)

The electrode assembly of claim 16, wherein the metal is tin (Sn) and the lithium intermetallic compound is Li17Sn4.