# US 2019/0319241 A1 · Method for producing nonaqueous electrolyte secondary battery separator

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0319241 A1
- Document ID: US20190319241A1
- Status: Published application
- Kind: A1
- Application number: 16/451,775
- Filed: 2019-06-25
- Published: 2019-10-17
- Earliest claimed: 2015-11-30
- Assignees: Sumitomo Chemical Company, Limited
- Applicants: Sumitomo Chemical Company, Limited
- Inventors: Daizaburo YASHIKI
- Web page: https://patentgrep.com/patent/US20190319241A1

## CPC

- B29C 67/202: {comprising elimination of a solid or a liquid ingredient}
- B29C 48/0019: {combined with shaping by flattening, folding or bending}
- B29C 53/005: {characterised by the choice of material (B29C53/36 and B29C53/56 take precedence)}
- B29C 55/02: of plates or sheets
- B29C 55/04: uniaxial, e.g. oblique
- H01M 10/05: Accumulators with non-aqueous electrolyte (H01M10/39 takes precedence)
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 50/406: Moulding; Embossing; Cutting
- H01M 50/417: Polyolefins
- H01M 50/423: Polyamide resins
- H01M 50/449: having a layered structure
- H01M 50/491: Porosity
- B29C 48/0011: {combined with compression moulding}
- B29C 48/08: flexible, e.g. films
- B29K 2023/00: Use of polyalkenes {or derivatives thereof} as moulding material
- B29K 2105/04: cellular or porous
- B29K 2995/0065: Permeability to gases
- B29L 2031/3468: {Batteries, accumulators or fuel cells (battery cases B29L2031/7146)}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A nonaqueous electrolyte secondary battery separator, which includes a porous film containing a polyolefin-based resin as a main component, has a difference of not more than 2.5 between (a) a white index measured on a surface of the porous film which has not been irradiated with ultraviolet light having 255 W/m2 and (b) a white index measured on the surface of the porous film which has been irradiated, for 75 hours, with the ultraviolet light having 255 W/m2.

## Claims

### Claim at position 1

1-7. (canceled)

### Claim 8

A method for producing a nonaqueous electrolyte secondary battery separator comprising a porous film containing a polyolefin-based resin as a main component,
the method comprising the steps of:
extruding a resin from an outlet of an extrusion machine; and
causing a pair of rollers to roll the resin so as to form the resin into a thin film, the resin being extruded from the outlet at a temperature of not lower than 200° C. and not higher than 250° C., and
the resin being exposed to air for not longer than 3.6 seconds after being extruded from the outlet and then brought into contact with the pair of rollers,
the nonaqueous electrolyte secondary battery separator having ΔWI defined by the following Equation (1) of not more than 2.5:
ΔWI=WI1−WI0 Equation (1)
wherein WI is a white index defined by American Standard Test Method (ASTM) E313; WI0 is WI that is measured, by use of a spectrocolorimeter, on a surface of the porous film which has not been irradiated with ultraviolet light having 255 W/m2; and WI1 is WI that is measured, by use of the spectrocolorimeter, on the surface of the porous film which has been irradiated, for 75 hours, with the ultraviolet light having 255 W/m2.

### Claim 9 (depends on 8)

The method as set forth in claim 8, wherein the resin is extruded from the outlet at an extrusion speed of 1 m/min to 10 m/min.

### Claim 10 (depends on 8)

The method as set forth in claim 8, wherein the pair of rollers has a surface temperature of 120° C. to 160° C.

### Claim 11 (depends on 8)

The method as set forth in claim 8, further comprising a step of allowing a sheet that has been formed by being rolled by the pair of rollers to pass through a cleaning liquid containing a surfactant, and removing a pore forming agent from the sheet.

### Claim 12 (depends on 11)

The method as set forth in claim 11, wherein the surfactant is a non-ionic surfactant.

### Claim 13 (depends on 11)

The method as set forth in claim 11, wherein the surfactant is contained in the cleaning liquid in an amount of not less than 0.1% by weight and not more than 15% by weight.

### Claim 14 (depends on 11)

The method as set forth in claim 11, wherein the cleaning liquid has a temperature of not lower than 25° C. and not higher than 60° C.

### Claim 15 (depends on 11)

The method as set forth in claim 11, further comprising a step of further cleaning, with water, the sheet from which the pore forming agent has been removed.

### Claim 16 (depends on 8)

A method for producing a nonaqueous electrolyte secondary battery laminated separator, comprising a step of applying a coating solution containing a resin to the nonaqueous electrolyte secondary battery separator obtained by a method recited in claim 8.

### Claim 17 (depends on 16)

The method as set forth in claim 16, wherein the resin contains aromatic polyamide.