# US 2019/0319193 A1 · Auto-polymerization electric storage material based on dopamine, preparation method thereof and application to electric storage device thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0319193 A1
- Document ID: US20190319193A1
- Status: Published application
- Kind: A1
- Application number: 16/380,809
- Filed: 2019-04-10
- Published: 2019-10-17
- Earliest claimed: 2018-04-11
- Assignees: Soochow University
- Applicants: Soochow University
- Inventors: Jianmei LU; Jinghui HE
- Web page: https://patentgrep.com/patent/US20190319193A1

## CPC

- H10K 85/113: {Heteroaromatic compounds comprising sulfur or selene, e.g. polythiophene}
- C08G 73/026: {Wholly aromatic polyamines}
- C08J 5/18: Manufacture of films or sheets
- H10K 10/80: Constructional details
- H10K 71/70: Testing, e.g. accelerated lifetime tests
- H10K 85/111: {comprising aromatic, heteroaromatic, or aryl chains, e.g. polyaniline, polyphenylene or polyphenylene vinylene}
- C08J 2379/02: Polyamines
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10K 2102/103: {comprising indium oxides, e.g. ITO}
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

The invention discloses a dopamine-based self-polymerization electric storage material and a preparation method thereof and the application thereof in an electric storage device, and the self-polymerization of dopamine is generated by solving the problems of complicated preparation process, poor environment and high temperature stability of the current organic electric storage material. The organic electric storage device prepared by the polymer into a sandwich structure successfully realizes the organic electric storage behavior. In the preparation process, the molecular synthesis and the device preparation are completed simultaneously, the device environment and the high temperature stability are good, and it is of great significance to the research progress of the organic electric storage technology and practical value.

## Claims

### Claim 1

A preparation method of a self-polymerization electric storage material, comprising the following steps: mixing a dopamine hydrochloride solution having a pH of 8 to 9 with copper sulfate pentahydrate and hydrogen peroxide to obtain a mixed solution; then forming a film with the mixed solution and annealing, to obtain the self-polymerization electric storage material.

### Claim 2

A preparation method of an electric storage device, comprising the following steps: mixing a dopamine hydrochloride solution having a pH of 8 to 9 with copper sulfate pentahydrate and hydrogen peroxide to obtain a mixed solution; then forming a film on the conductive surface of a conductive substrate with the mixed solution and annealing, and finally preparing electrodes, to obtain the electric storage device.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein the pH of said dopamine hydrochloride solution is adjusted to 8 to 9 by hydrochloric acid buffer, said dopamine hydrochloride solution is a dopamine hydrochloride aqueous solution, the concentration of said dopamine hydrochloride solution is 8 mg/mL to 11 mg/mL.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the temperature of annealing is 30° C., time of annealing is 11 to 13 hours.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein said film is formed by dipping method at room temperature.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein the mass ratio of the dopamine hydrochloride, copper sulfate pentahydrate and hydrogen peroxide is 1000:(120 to 130):(66 to 67).

### Claim 7 (depends on 2)

The preparation method according to claim 2, wherein the conductive substrate is sequentially washed with washing powder, acetone, ethanol, and a cleaning solution, said cleaning solution is selected from concentrated sulfuric acid and hydrogen peroxide.

### Claim 8 (depends on 1)

A self-polymerization electric storage material or an electric storage device obtained by the preparation method according to claim 1.

### Claim 9 (depends on 8)

The application in the preparation of electric storage device of the self-polymerization electric storage material according to claim 8.

### Claim 10

The application of dopamine hydrochloride in the preparation of electric storage device; or the application of dopamine hydrochloride in the preparation of self-polymerization electric storage material for electric storage device.

### Claim 11 (depends on 2)

The preparation method according to claim 2, wherein the pH of said dopamine hydrochloride solution is adjusted to 8 to 9 by hydrochloric acid buffer, said dopamine hydrochloride solution is a dopamine hydrochloride aqueous solution, the concentration of said dopamine hydrochloride solution is 8 mg/mL to 11 mg/mL.

### Claim 12 (depends on 2)

The preparation method according to claim 2, wherein the temperature of annealing is 30° C., time of annealing is 11 to 13 hours.

### Claim 13 (depends on 2)

The preparation method according to claim 2, wherein said film is formed by dipping method at room temperature.

### Claim 14 (depends on 2)

The preparation method according to claim 2, wherein the mass ratio of the dopamine hydrochloride, copper sulfate pentahydrate and hydrogen peroxide is 1000:(120 to 130):(66 to 67).

### Claim 15 (depends on 2)

A self-polymerization electric storage material or an electric storage device obtained by the preparation method according to claim 2.