# US 2019/0319153 A1 · Solar cell including conductive amorphous semiconductor layer and method of manufacturing solar cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0319153 A1
- Document ID: US20190319153A1
- Status: Published application
- Kind: A1
- Application number: 16/447,737
- Filed: 2019-06-20
- Published: 2019-10-17
- Earliest claimed: 2016-12-21
- Assignees: Panasonic Intellectual Property Management Co., Ltd.
- Applicants: Panasonic Intellectual Property Management Co., Ltd.
- Inventors: Daiki WATANABE; Hiroyuki YAMADA; Minato SENO; Akinori TSURUTA
- Web page: https://patentgrep.com/patent/US20190319153A1

## CPC

- H10F 10/166: the Group IV-IV heterojunctions being heterojunctions of crystalline and amorphous materials, e.g. silicon heterojunction [SHJ] photovoltaic cells
- H10F 77/1662: {including only Group IV materials}
- H10F 71/103: {including only Group IV materials}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/127: {The active layers comprising only Group III-V materials, e.g. GaAs or InP}
- H10F 77/244: {made of transparent conductive layers, e.g. transparent conductive oxide [TCO] layers}
- Y02E 10/544: Solar cells from Group III-V materials
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02E 10/548: Amorphous silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An i-type layer is formed on a side of one surface of a crystalline semiconductor substrate. An n-type layer or a p-type layer is formed on the i-type layer and includes a conductive impurity. A TCO is formed on the n-type layer or the p-type layer. A density in a proximate portion of the n-type layer or the p-type layer closer to the TCO than a remote portion of the n-type layer or the p-type layer is smaller than a density in the remote portion.

## Claims

### Claim 1

A solar cell comprising:
a crystalline semiconductor substrate;
an intrinsic amorphous semiconductor layer formed on a side of one surface of the crystalline semiconductor substrate;
a conductive amorphous semiconductor layer formed on the intrinsic amorphous semiconductor layer and including a conductive impurity; and
a transparent conductive film layer formed on the conductive amorphous semiconductor layer, wherein
a density in a second portion of the conductive amorphous semiconductor layer closer to the transparent conductive film layer than a first portion of the conductive amorphous semiconductor layer is smaller than a density in the first portion.

### Claim 2 (depends on 1)

The solar cell according to claim 1, wherein
a dopant concentration in the second portion of the conductive amorphous semiconductor layer is smaller than a dopant concentration in the first portion.

### Claim 3 (depends on 1)

The solar cell according to claim 1, further comprising:
a further intrinsic amorphous semiconductor layer;
a further conductive amorphous semiconductor layer including a conductive impurity; and
a further transparent conductive film layer, wherein
the further intrinsic amorphous semiconductor layer, the further conductive amorphous semiconductor layer, and the further transparent conductive film layer are formed on a side of the crystalline semiconductor substrate opposite to the intrinsic amorphous semiconductor layer, the conductive amorphous semiconductor layer, and the transparent conductive film layer,
a conductivity type of the impurity included in the further conductive amorphous semiconductor layer is different from a conductivity type of the impurity included in the conductive amorphous semiconductor layer, and
a density in a fourth portion of the further conductive amorphous semiconductor layer closer to the further transparent conductive film layer than a third portion of the further conductive amorphous semiconductor layer is smaller than a density in the third portion.

### Claim 4 (depends on 2)

The solar cell according to claim 2, further comprising:
a further intrinsic amorphous semiconductor layer;
a further conductive amorphous semiconductor layer including a conductive impurity; and
a further transparent conductive film layer, wherein
the further intrinsic amorphous semiconductor layer, the further conductive amorphous semiconductor layer, and the further transparent conductive film layer are formed on a side of the crystalline semiconductor substrate opposite to the intrinsic amorphous semiconductor layer, the conductive amorphous semiconductor layer, and the transparent conductive film layer,
a conductivity type of the impurity included in the further conductive amorphous semiconductor layer is different from a conductivity type of the impurity included in the conductive amorphous semiconductor layer, and
a density in a fourth portion of the further conductive amorphous semiconductor layer closer to the further transparent conductive film layer than a third portion of the further conductive amorphous semiconductor layer is smaller than a density in the third portion.

### Claim 5

A method of manufacturing a solar cell comprising:
forming an intrinsic amorphous semiconductor layer on a side of one surface of a crystalline semiconductor substrate masked at least in part;
forming a conductive amorphous semiconductor layer including a conductive impurity on the intrinsic amorphous semiconductor layer; and
forming a transparent conductive film layer on the conductive amorphous semiconductor layer, wherein
a deposition speed for forming a second portion of the conductive amorphous semiconductor layer closer to the transparent conductive film layer than a first portion of the conductive amorphous semiconductor layer is higher than a deposition speed for forming the first portion.

### Claim 6 (depends on 5)

The method of manufacturing a solar cell according to claim 5, wherein
the deposition speed for forming the second portion of the conductive amorphous semiconductor layer is 1.01 times-5.00 times the deposition speed for forming the first portion.