# US 2019/0319109 A1 · Method of manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0319109 A1
- Document ID: US20190319109A1
- Status: Published application
- Kind: A1
- Application number: 16/315,067
- Filed: 2016-08-25
- Published: 2019-10-17
- Earliest claimed: 2016-08-25
- Assignees: Mitsubishi Electric Corporation
- Applicants: Mitsubishi Electric Corporation
- Inventors: Takao KACHI; Yasuhiro YOSHIURA
- Web page: https://patentgrep.com/patent/US20190319109A1

## CPC

- H10D 8/045: {of PN junction diodes}
- H10D 62/8325: {Silicon carbide}
- H10D 8/50: PIN diodes
- H10D 12/481: {having gate structures on slanted surfaces, on vertical surfaces, or in grooves, e.g. trench gate IGBTs}
- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 62/111: {Multiple RESURF structures, e.g. double RESURF or 3D-RESURF structures}
- H10D 64/011: {of electrodes ohmically coupled to a semiconductor}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/40: of conductive or resistive materials
- H10P 50/264: {by chemical means}
- H10P 50/642: {Chemical etching}
- H10D 62/051: {Forming charge compensation regions, e.g. superjunctions}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

It is an object of the present invention to easily perform an electric characteristic test for ensuring quality of a semiconductor device on an electrode pattern defect or deficiency. A method of manufacturing a semiconductor device according to the present invention performs, a first etching having a higher selected ratio with respect to a semiconductor material of a first semiconductor layer than a material of a first electrode film over the first electrode film, and removes a region in the first semiconductor layer below a pattern defective part or a deficiency part of the first electrode film at least partially to form an electrode film in the pattern defective part or the deficiency part of the first electrode film.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising:
performing, on a semiconductor device having a semiconductor substrate, a first semiconductor layer being formed on a side of a first main surface of the semiconductor substrate, and a first electrode film being formed on the first semiconductor layer to be in contact with the first semiconductor layer, a first etching having a higher selected ratio with respect to a semiconductor material of the first semiconductor layer than a material of the first electrode film over the first electrode film, and removing a region in the first semiconductor layer below a pattern defective part or a deficiency part of the first electrode film at least partially, and
forming an electrode film in the pattern defective part or the deficiency part of the first electrode film.

### Claim 2 (depends on 1)

The method of manufacturing the semiconductor device according to claim 1, wherein
a region in the first semiconductor layer below the pattern defective part or the deficiency part of the first electrode film is completely removed by the first etching.

### Claim 3 (depends on 1)

The method of manufacturing the semiconductor device according to claim 1, wherein
a region in the first semiconductor layer below the pattern defective part or the deficiency part of the first electrode film is partially removed by the first etching.

### Claim 4 (depends on 1)

The method of manufacturing the semiconductor device according to claim 1, wherein
the semiconductor device has a second semiconductor layer being formed on a side of a second main surface of the semiconductor substrate opposing the first main surface and a second electrode film being formed on the second semiconductor layer to be in contact with the second semiconductor layer,
a second etching having a higher selected ratio with respect to a semiconductor material of the second semiconductor layer than a material of the second electrode film is performed over the second electrode film, and a region in the second semiconductor layer below a pattern defective part or a deficiency part of the second electrode film is removed at least partially, and
an electrode film is formed in the pattern defective part or the deficiency part of the second electrode film.

### Claim 5 (depends on 4)

The method of manufacturing the semiconductor device according to claim 4, wherein
a region in the second semiconductor layer below the pattern defective part or the deficiency part of the second electrode film is completely removed by the second etching.

### Claim 6 (depends on 4)

The method of manufacturing the semiconductor device according to claim 4, wherein
a region in the second semiconductor layer below the pattern defective part or the deficiency part of the second electrode film is partially removed by the second etching.

### Claim 7 (depends on 4)

The method of manufacturing the semiconductor device according to claim 4, wherein
the first etching and the second etching are simultaneously performed.

### Claim 8 (depends on 4)

The method of manufacturing the semiconductor device according to claim 4, wherein
the first etching and the second etching are performed at different times.

### Claim 9 (depends on 1)

The method of manufacturing the semiconductor device according to claim 1, wherein
the first semiconductor layer has a super junction structure being made up of a semiconductor layer of a first conductivity type and a semiconductor layer of a second conductivity type.

### Claim 10 (depends on 1)

The method of manufacturing the semiconductor device according to claim 1, wherein
the first semiconductor layer is an Si layer.

### Claim 11 (depends on 1)

The method of manufacturing the semiconductor device according to claim 1, wherein
the second semiconductor layer is an Si layer.