# US 2019/0319031 A1 · Bit line gate and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0319031 A1
- Document ID: US20190319031A1
- Status: Published application
- Kind: A1
- Application number: 15/972,216
- Filed: 2018-05-06
- Published: 2019-10-17
- Earliest claimed: 2018-04-17
- Assignees: United Microelectronics Corp.; Fujian Jinhua Integrated Circuit Co., Ltd.
- Applicants: United Microelectronics Corp.; Fujian Jinhua Integrated Circuit Co., Ltd.
- Inventors: Pin-Hong Chen; Yi-Wei Chen; Chun-Chieh Chiu; Chih-Chieh Tsai; Tzu-Chieh Chen; Chih-Chien Liu
- Web page: https://patentgrep.com/patent/US20190319031A1

## CPC

- H10B 12/09: {with simultaneous manufacture of the peripheral circuit region and memory cells}
- H10B 12/482: {Bit lines}
- H10D 64/01312: {the additional layer comprising a metal or metal silicide formed by deposition, i.e. without a silicidation reaction, e.g. sputter deposition}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/44: Physical vapour deposition [PVD]
- H10P 32/00: Diffusion of dopants within, into or out of wafers, substrates or parts of devices (during formation of materials H10P14/00)
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a bit line gate structure comprising a substrate, an amorphous silicon layer disposed on the substrate, a first doped region located in the amorphous silicon layer, a titanium silicon nitride (TiSiN) layer, located in the amorphous silicon layer, and a second doped region located in the TiSiN layer, the first doped region contacts the second doped region directly.

## Claims

### Claim at position 1

1-7. (canceled)

### Claim 8

A method for forming a bit line gate structure, comprising:
providing a substrate;
forming an amorphous silicon layer on the substrate;
performing an ion doping step to form a first doped region in the amorphous silicon layer, wherein an oxide layer is formed on the surface of the amorphous silicon layer after the ion doping step is performed;
performing an etching step to completely remove the oxide layer;
forming a titanium silicon nitride (TiSiN) layer on the amorphous silicon layer; and
performing a rapid thermal process (RTP) to diffuse the first doped region into the TiSiN layer, and to form a second doped region within the TiSiN layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the first doped region contacts the second doped region directly.

### Claim 10 (depends on 8)

The method of claim 8, further comprising forming a metal layer on the TiSiN layer.

### Claim 11 (depends on 8)

The method of claim 8, further comprising forming a silicon nitride layer on the metal layer.

### Claim 12 (depends on 8)

The method of claim 8, wherein the temperature of the RTP is between 800-900° C.

### Claim 13 (depends on 8)

The method of claim 8, wherein a doping depth of the ion doping step is between 150-200 angstroms.

### Claim at position 8

14-15. (canceled)

### Claim 16 (depends on 8)

The method of claim 8, wherein the etching step comprises soaking in a dilute hydrofluoric acid (DHF) solution.