# US 2019/0318947 A1 · Low Thermal Budget Annealing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0318947 A1
- Document ID: US20190318947A1
- Status: Published application
- Kind: A1
- Application number: 16/376,031
- Filed: 2019-04-05
- Published: 2019-10-17
- Earliest claimed: 2018-04-12
- Assignees: Mattson Technology, Inc.
- Applicants: Mattson Technology, Inc.
- Inventors: Paul J. Timans
- Web page: https://patentgrep.com/patent/US20190318947A1

## CPC

- H10P 72/0436: {mainly by radiation}
- F27B 17/0025: {specially adapted for treating semiconductor wafers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10P 72/0432: {mainly by conduction}
- H10P 72/0462: {characterised by the construction of the processing chambers, e.g. modular processing chambers}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P 95/904: {of Group III-V semiconductors}
- H10P 72/0602: {Temperature monitoring}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS

## Abstract

Methods and systems for providing a short-duration anneal are provided. In one example, the methods and systems can include placing a workpiece in a thermal processing chamber. The workpiece can include a device side surface and an opposing non-device side surface. The methods and systems can include delivering an energy pulse from at least one heat source to the non-device side surface of the workpiece. In another example, the methods and systems can include depositing a layer of semiconductor material onto the semiconductor workpiece at the device side of the semiconductor workpiece. The methods and systems can include doping the layer of semiconductor material with a doping species and annealing the layer for crystallization using solid phase epitaxy.

## Claims

### Claim 1

A method for thermal processing of a workpiece, the method comprising:
placing the workpiece in a thermal processing chamber, the workpiece comprising a device side surface and an opposing non-device side surface, the workpiece having a thickness between the device side surface and the opposing non-device side surface;
delivering an energy pulse from at least one heat source to the non-device side surface of the workpiece, the energy pulse having a pulse duration;
wherein the pulse duration is less than a thermal conduction time for heat from the energy pulse to diffuse through the thickness of the workpiece and is such that a rate of heating the device side surface is greater than 1000 K/s;
wherein a rate of cooling the device side surface is less than about 1000 K/s.

### Claim 2 (depends on 1)

The method of claim 1, wherein the device side surface comprises one or more device structures, films, or layers that are annealed during the energy pulse and the non-device side surface includes no device structures.

### Claim 3 (depends on 1)

The method of claim 1, wherein the pulse duration is less than about 100 ms.

### Claim 4 (depends on 1)

The method of claim 1, wherein prior to delivering the energy pulse, the method comprises heating the workpiece to an intermediate temperature, wherein the intermediate temperature is in the range of about 20° C. to about 800° C.

### Claim 5 (depends on 4)

The method of claim 4, wherein heating the workpiece to the intermediate temperature comprises heating the device side surface of the workpiece.

### Claim 6 (depends on 1)

The method of claim 1, wherein the at least one heat source comprises an arc lamp.

### Claim 7 (depends on 1)

The method of claim 1, wherein the at least one heat source comprises a laser.

### Claim 8 (depends on 1)

The method of claim 1, wherein the energy pulse causes the device side surface to have a peak temperature in the range of about 40% to about 80% of a peak temperature of the non-device side temperature.

### Claim 9 (depends on 1)

The method of claim 1, wherein the energy pulse causes the non-device side surface to have a peak temperature of about 1200° C. and the device side surface to have a peak temperature of about 850° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the pulse duration is such that a 50° temperature peak width of a temperature of the device side surface is about 1.3 seconds or less.

### Claim 11 (depends on 1)

The method of claim 1, wherein the non-device side surface of the workpiece comprises a compensating film, wherein one or more compensating properties of the compensating film correspond to non-uniform characteristics of one or more device structures on the device side surface.

### Claim 12 (depends on 1)

The method of claim 1, wherein a mask structure is disposed between the at least one heat source and the non-device side surface.

### Claim 13 (depends on 1)

The method of claim 1, wherein the device side surface is in thermal communication with a heat sink, wherein the heat sink comprises a hot plate in the thermal processing chamber.

### Claim 14 (depends on 13)

The method of claim 13, wherein the method comprises supporting the workpiece on a gas cushion disposed between the hot plate and the workpiece, wherein the gas cushion has a thickness of about 0.02 mm to about 2 mm.

### Claim 15

A method for processing a workpiece in a thermal processing system, the workpiece comprising a device side surface and a non-device side surface separated by a thickness, the method comprising:
placing a workpiece on a workpiece support in a processing chamber of the thermal processing system such that the non-device side surface faces one or more arc lamps;
heating the workpiece to an intermediate temperature using one or more heat sources;
providing an irradiance flash to the non-device side surface of the workpiece using the one or more arc lamps, the irradiance flash having a duration of less than about 100 ms such that a rate of heating the device side surface is greater than 1000 K/s and a rate of cooling the device side surface is less than about 1000 K/s.

### Claim 16 (depends on 15)

The method of claim 15, wherein the irradiance flash creates a temperature gradient between the device side surface of the workpiece and the non-device side surface of the workpiece.

### Claim 17 (depends on 15)

The method of claim 15, wherein the irradiance flash causes the non-device side surface to achieve a peak temperature of about 1200° C.

### Claim 18 (depends on 17)

The method of claim 17, wherein the irradiance flash causes the device side surface to have a 50° temperature peak width of about 1.3 seconds or less.

### Claim 19

A method for processing a semiconductor workpiece, the method comprising:
depositing a layer of semiconductor material onto the semiconductor workpiece at the device side of the semiconductor workpiece, the layer having an amorphous structure;
doping the layer of semiconductor material with a dopant species;
annealing the layer for crystallization using solid phase epitaxy;
wherein during crystallization, the dopant species becomes incorporated into crystalline material
wherein annealing the layer for crystallization comprises:
placing a workpiece on a workpiece support in a processing chamber of the thermal processing system such that the non-device side surface faces one or more arc lamps;
heating the workpiece to an intermediate temperature using one or more heat sources;
providing an irradiance flash to the non-device side surface of the workpiece using the one or more arc lamps, the irradiance flash having a duration of less than about 100 ms such that a rate of heating the device side surface is greater than 1000 K/s and a rate of cooling the device side surface is less than about 1000 K/s;

### Claim 20 (depends on 19)

The method of claim 19, wherein the irradiance flash causes the non-device side surface to achieve a peak temperature of about 1200° C.