# US 2019/0318840 A1 · Flexible, uv-resistant poly(phenylene ether) composition, and insulated conductor and jacketed cable comprising same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0318840 A1
- Document ID: US20190318840A1
- Status: Published application
- Kind: A1
- Application number: 16/474,175
- Filed: 2018-01-02
- Published: 2019-10-17
- Earliest claimed: 2017-01-05
- Assignees: Sabic Global Technologies B.V.
- Applicants: SABIC Global Technologies B.V.
- Inventors: Hui Peng; Wei Shan
- Web page: https://patentgrep.com/patent/US20190318840A1

## CPC

- H01B 3/427: {Polyethers}
- C08L 53/025: {modified}
- C08L 71/12: Polyphenylene oxides
- C09D 5/00: Coating compositions, e.g. paints, varnishes or lacquers, characterised by their physical nature or the effects produced {(electrically insulating plastics, resins or waxes H01B3/30)}; Filling pastes
- C09D 171/12: Polyphenylene oxides
- H01B 3/441: {from alkenes}
- H01B 3/442: {from aromatic vinyl compounds}
- H01B 7/295: using material resistant to flame
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A composition contains specific amounts of a poly(phenylene ether), a hydrogenated block copolymer of an alkenyl aromatic monomer and a conjugated diene, a flame retardant that includes an organophosphate ester with a melting point of 60 to 150° C., and an ultraviolet absorbing agent. The high-melting organophosphate ester permits reduction of the ultraviolet absorbing agent content, which in turn reduces color shift under storage conditions. The composition is useful as an insulating material and a jacketing material for wire and cable.

## Claims

### Claim 1

A composition, comprising:
15 to 40 parts by weight of a poly(phenylene ether);
20 to 50 parts by weight of a hydrogenated block copolymer of an alkenyl aromatic monomer and a conjugated diene;
5 to 30 parts by weight of a flame retardant comprising 3 to 15 parts by weight of an organophosphate ester having a melting point of 60 to 150° C.; and
0.5 to 5 parts by weight of an ultraviolet absorbing agent;
wherein all parts by weight are based on 100 parts by weight total of polymers and flame retardants.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the hydrogenated block copolymer comprises 25 to 35 parts by weight of a polystyrene-poly(ethylene-butylene-styrene)-polystyrene tapered block copolymer.

### Claim 3 (depends on 2)

The composition of claim 2, wherein the polystyrene-poly(ethylene-butylene-styrene)-polystyrene tapered block copolymer comprises 10 to 20 parts by weight of a first polystyrene-poly(ethylene-butylene-styrene)-polystyrene tapered block copolymer having a polystyrene content of 34 to 48 weight percent, and 10 to 20 parts by weight of a second polystyrene-poly(ethylene-butylene-styrene)-polystyrene tapered block copolymer having a polystyrene content of 50 to 65 weight percent.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the organophosphate ester has structure (1) or (2)
wherein
m is independently at each occurrence 0, 1 or 2, provided that at least one occurrence of m is 1;
p is on average 1 to 3;
R1 is independently at each occurrence C1-C4 alkyl;
n is independently at each occurrence 0, 1 or 2;
q is on average 1 to 3; and
R2 is independently at each occurrence C1-C4 alkyl.

### Claim 5 (depends on 4)

The composition of claim 4, wherein the organophosphate ester has structure (1), m is 2, p is on average 1 to 2, and R1 is methyl.

### Claim 6 (depends on 4)

The composition of claim 4, wherein the organophosphate ester has structure (2), n is 0, and p is on average 1 to 2.

### Claim 7 (depends on 1)

The composition of claim 1, wherein the flame retardant comprises 3 to 10 parts by weight of the organophosphate ester and further comprises 5 to 12 parts by weight of a metal dialkylphosphinate and 5 to 12 parts by weight of melamine polyphosphate.

### Claim 8 (depends on 1)

The composition of claim 1, wherein the ultraviolet absorbing agent is selected from the group consisting of benzophenones, benzotriazoles, cinnamates, oxanilides, triazines, benzoxazinones, and combinations thereof.

### Claim 9 (depends on 1)

The composition of claim 1, wherein the ultraviolet absorbing agent comprises a 2-(2′-hydroxyphenyl)benzotriazole.

### Claim 10 (depends on 1)

The composition of claim 1, wherein the ultraviolet absorbing agent comprises a 2-(2′-hydroxyphenyl)-1,3,5-triazine.

### Claim 11 (depends on 1)

The composition of claim 1, further comprising 2 to 15 parts by weight of an ethylene homopolymer, a propylene homopolymer, or a combination thereof.

### Claim 12 (depends on 1)

The composition of claim 1, further comprising 2 to 10 parts by weight of a polybutene having a number average molecular weight of 500 to 1500 grams/mole.

### Claim 13 (depends on 1)

The composition of claim 1, wherein
the poly(phenylene ether) comprises a poly(2,6-dimethyl-1,4-phenylene ether) having an intrinsic viscosity of 0.3 to 0.6 deciliter per gram, measured by Ubbelohde viscometer in chloroform at 25° C.;
the hydrogenated block copolymer comprises 25 to 35 weight percent of a polystyrene-poly(ethylene-butylene-styrene)-polystyrene tapered block copolymer;
the organophosphate ester comprises an organophosphate ester having structure (1)
wherein m is 2, p is on average 1 to 2, and R1 is methyl; an organophosphate ester having structure (2)
wherein n is 0, and p is on average 1 to 2; or a combination of the organophosphate ester having structure (1) and the organophosphate ester having structure (2);
the ultraviolet absorbing agent comprises a 2-(2′-hydroxyphenyl)benzotriazole, a 2-(2′-hydroxyphenyl)-1,3,5-triazine, or a combination thereof;
the composition comprises
18 to 30 parts by weight of the poly(phenylene ether),
25 to 40 parts by weight of the hydrogenated block copolymer,
3 to 10 parts by weight of the organophosphate ester, and
1 to 3 parts by weight of the ultraviolet absorbing agent;
the composition further comprises
5 to 15 parts by weight of a propylene homopolymer, and
6 to 10 parts by weight of a polybutene having a number average molecular weight of 500 to 1500 grams/mole; and
the flame retardant further comprises
5 to 12 parts by weight of a metal dialkylphosphinate, and
5 to 12 parts by weight of melamine polyphosphate.

### Claim 14

An insulated conductor, comprising:
a conductor; and
an insulating covering disposed over the conductor;
wherein the insulating covering comprises a composition comprising
15 to 40 parts by weight of a poly(phenylene ether);
20 to 50 parts by weight of a hydrogenated block copolymer of an alkenyl aromatic monomer and a conjugated diene;
5 to 30 parts by weight of a flame retardant comprising 3 to 15 parts by weight of an organophosphate ester having a melting point of 60 to 150° C.; and
0.5 to 5 parts by weight of an ultraviolet absorbing agent;
wherein all parts by weight are based on 100 parts by weight total of polymers and flame retardants.

### Claim 15 (depends on 14)

The insulated conductor of claim 14, wherein
the poly(phenylene ether) comprises a poly(2,6-dimethyl-1,4-phenylene ether) having an intrinsic viscosity of 0.3 to 0.6 deciliter per gram, measured by Ubbelohde viscometer in chloroform at 25° C.;
the hydrogenated block copolymer comprises 25 to 35 weight percent of a polystyrene-poly(ethylene-butylene-styrene)-polystyrene tapered block copolymer;
the organophosphate ester comprises an organophosphate ester having structure (1)
wherein m is 2, p is on average 1 to 2, and R1 is methyl; or an organophosphate ester having structure (2)
wherein n is 0, and p is on average 1 to 2; or a combination of the organophosphate ester having structure (1) and the organophosphate ester having structure (2);
the ultraviolet absorbing agent comprises a 2-(2′-hydroxyphenyl)benzotriazole, a 2-(2′-hydroxyphenyl)-1,3,5-triazine, or a combination thereof;
the composition comprises
18 to 30 parts by weight of the poly(phenylene ether),
25 to 40 parts by weight of the hydrogenated block copolymer,
3 to 10 parts by weight of the organophosphate ester, and
1 to 3 parts by weight of the ultraviolet absorbing agent;
the composition further comprises
5 to 15 parts by weight of a propylene homopolymer, and
6 to 10 parts by weight of a polybutene having a number average molecular weight of 500 to 1500 grams/mole; and
the flame retardant further comprises
5 to 12 parts by weight of a metal dialkylphosphinate, and
5 to 12 parts by weight of melamine polyphosphate.

### Claim 16

A jacketed cable, comprising:
a conductor;
an insulating covering surrounding the conductor; and
a jacket surrounding the insulating covering;
wherein the jacket comprises a composition comprising
15 to 40 parts by weight of a poly(phenylene ether);
20 to 50 parts by weight of a hydrogenated block copolymer of an alkenyl aromatic monomer and a conjugated diene;
5 to 30 parts by weight of a flame retardant comprising 3 to 15 parts by weight of an organophosphate ester having a melting point of 60 to 150° C.; and
0.5 to 5 parts by weight of an ultraviolet absorbing agent;
wherein all parts by weight are based on 100 parts by weight total of polymers and flame retardants.

### Claim 17 (depends on 16)

The jacketed cable of claim 16, wherein
the poly(phenylene ether) comprises a poly(2,6-dimethyl-1,4-phenylene ether) having an intrinsic viscosity of 0.3 to 0.6 deciliter per gram, measured by Ubbelohde viscometer in chloroform at 25° C.;
the hydrogenated block copolymer comprises 25 to 35 weight percent of a polystyrene-poly(ethylene-butylene-styrene)-polystyrene tapered block copolymer;
the organophosphate ester comprises an organophosphate ester having structure (1)
wherein m is 2, p is on average 1 to 2, and R1 is methyl; or an organophosphate ester having structure (2)
wherein n is 0, and p is on average 1 to 2; or a combination of the organophosphate ester having structure (1) and the organophosphate ester having structure (2);
the ultraviolet absorbing agent comprises a 2-(2′-hydroxyphenyl)benzotriazole, a 2-(2′-hydroxyphenyl)-1,3,5-triazine, or a combination thereof;
the composition comprises
18 to 30 parts by weight of the poly(phenylene ether),
25 to 40 parts by weight of the hydrogenated block copolymer,
3 to 10 parts by weight of the organophosphate ester, and
1 to 3 parts by weight of the ultraviolet absorbing agent;
the composition further comprises
5 to 15 parts by weight of a propylene homopolymer, and
6 to 10 parts by weight of a polybutene having a number average molecular weight of 500 to 1500 grams/mole; and
the flame retardant further comprises
5 to 12 parts by weight of a metal dialkylphosphinate, and
5 to 12 parts by weight of melamine polyphosphate.