# US 2019/0317249 A1 · Infrared Cut-off Filter and Preparation Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0317249 A1
- Document ID: US20190317249A1
- Status: Published application
- Kind: A1
- Application number: 16/081,343
- Filed: 2017-12-15
- Published: 2019-10-17
- Earliest claimed: 2016-12-26
- Assignees: Xinyang Sunny Optics Co., Ltd.
- Applicants: Xinyang Sunny Optics Co., Ltd.
- Inventors: Lei Wang; Weihong Ding; Rui Du
- Web page: https://patentgrep.com/patent/US20190317249A1

## CPC

- G02B 1/115: Multilayers
- G02B 5/003: {Light absorbing elements}
- G02B 5/208: {for use with infrared or ultraviolet radiation, e.g. for separating visible light from infrared and/or ultraviolet radiation}
- G02B 5/223: {containing organic substances, e.g. dyes, inks or pigments}
- G03B 11/00: Filters or other obturators specially adapted for photographic purposes
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G03B: APPARATUS OR ARRANGEMENTS FOR TAKING PHOTOGRAPHS OR FOR PROJECTING OR VIEWING THEM; APPARATUS OR ARRANGEMENTS EMPLOYING ANALOGOUS TECHNIQUES USING WAVES OTHER THAN OPTICAL WAVES; ACCESSORIES THEREFOR (optical parts of such apparatus G02B; photosensitive materials or processes for photographic purposes G03C; apparatus for processing exposed photographic materials G03D)

## Abstract

The application relates to an infrared cut-off filter, which includes: a substrate composed of white glass and an infrared cut-off film layer plated on one surface of the white glass; a spin-coated layer plated on the other surface of the white glass; and a reflection-reducing film layer plated on the spin-coated layer; the spin-coated layer includes a bottom layer and an absorbing layer each composed of an organic substance. The infrared cut-off filter has a stable structure, a high degree of firmness between layers, and a low cost.

## Claims

### Claim 1

An infrared cut-off filter, comprising:
a substrate composed of white glass and an infrared cut-off film layer plated on one surface of the white glass;
a spin-coated layer plated on the other surface of the white glass;
and a reflection-reducing film layer plated on the spin-coated layer;
wherein the spin-coated layer comprises a bottom layer and an absorbing layer each composed of an organic substance.

### Claim 2 (depends on 1)

The infrared cut-off filter according to claim 1, wherein the infrared cut-off film layer and the reflection-reducing film layer are each formed by alternately plating high refractive index material layer and low refractive index material layer.

### Claim 3 (depends on 2)

The infrared cut-off filter according to claim 2, wherein the high refractive index material layer may be composed of one or more of TiO2, Ti3O5, Ta2O5 and H4.

### Claim 4 (depends on 2)

The infrared cut-off filter according to claim 2, wherein the low refractive index material layer may be composed of one or both of SiO2 and MgF2.

### Claim 5 (depends on 4)

The infrared cut-off filter according to claim 4, wherein the number of plated layers of the infrared cut-off film layer is 43-50.

### Claim 6 (depends on 5)

The infrared cut-off filter according to claim 5, wherein the infrared cut-off film layer has a plated thickness of 5 μm to 7 μm.

### Claim 7 (depends on 4)

The infrared cut-off filter according to claim 4, wherein the number of plated layers of the reflection-reducing film layer is 8-10.

### Claim 8 (depends on 7)

The infrared cut-off filter according to claim 7, wherein the reflection-reducing film layer has a plated thickness of 0.4 μm to 0.7 μm.

### Claim 9

A method for preparing an infrared cut-off filter, comprising the steps of:
(a) using an ultrasonic cleaning process to clean white glass;
(b) plating an infrared cut-off film layer on one surface of the white glass;
(c) cleaning the substrate using a plasma cleaning process;
(d) cleaning the substrate using an ultrasonic cleaning process;
(e) plating a spin-coated layer on a surface of the substrate which is not plated with the infrared cut-off film layer; and
(f) evaporate plating a reflection-reducing film layer on the spin-coated layer.

### Claim 10 (depends on 9)

The method of preparing the infrared cut-off filter according to claim 9, wherein in the step (b), the infrared cut-off film layer is plated by electron gun evaporation and ion source assisted vacuum plating.

### Claim 11 (depends on 9)

The method of preparing the infrared cut-off filter according to claim 9, wherein in the step (c), the plasma cleaning process has a power of 300 W-450 W and an action time of 100 s-600 s.

### Claim 12 (depends on 9)

The method of preparing the infrared cut-off filter according to claim 9, wherein the step (e) comprises the steps of:
(e1) dripping a small amount of binder on the surface of the substrate (1) which is not plated with the infrared cut-off film layer, rotating the substrate at a high speed, uniformly coating the binder on the surface of the substrate by centrifugal force, and simultaneously throwing out excessive binder to form a bottom layer;
(e2) baking the substrate, on which the bottom layer is formed;
(e3) dripping infrared absorbing glue on the bottom layer, rotating at a low speed, uniformly coating the infrared absorbing glue on the bottom layer by centrifugal force, and simultaneously throwing out excessive infrared absorbing glue to form an absorbing layer;
(e4) baking the substrate, on which the absorbing layer is formed; and
(e5) using an ultrasonic cleaning process to clean the baked substrate.

### Claim 13 (depends on 12)

The method of preparing the infrared cut-off filter according to claim 12, wherein in the step (e1), the rotation speed is 3,000 rpm-5,500 rpm.

### Claim 14 (depends on 12)

The method of preparing the infrared cut-off filter according to claim 12, wherein in the step (e2), a dust-free oven is used for baking at a baking temperature of 80° C.-200° C. and a baking time of 2 min-10 min.

### Claim 15 (depends on 12)

The method of preparing the infrared cut-off filter according to claim 12, wherein in the step (e3), the rotation speed is 200 rpm-1,000 rpm, and the rotation time is 8 s-15 s.

### Claim 16 (depends on 12)

The method of preparing the infrared cut-off filter according to claim 12, wherein in the step (e4), a dust-free oven is used for baking at a baking temperature of 80° C.-200° C. and a baking time of 60 min-120 min.