# US 2019/0316272 A1 · Aluminum nitride bulk crystals having high transparency to ultraviolet light and methods of forming them

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0316272 A1
- Document ID: US20190316272A1
- Status: Published application
- Kind: A1
- Application number: 16/395,543
- Filed: 2019-04-26
- Published: 2019-10-17
- Earliest claimed: 2006-03-30
- Assignees: Crystal IS, Inc.
- Applicants: Crystal IS, Inc.
- Inventors: Sandra B. Schujman; Shailaja P. Rao; Robert T. Bondokov; Kenneth E. Morgan; Glen A. Slack; Leo J. Schowalter
- Web page: https://patentgrep.com/patent/US20190316272A1

## CPC

- C30B 23/066: {Heating of the material to be evaporated}
- C30B 23/00: Single-crystal growth by condensing evaporated or sublimed materials
- C30B 23/002: {Controlling or regulating}
- C30B 23/02: Epitaxial-layer growth
- C30B 29/403: {AIII-nitrides}
- H10P 14/2908: {Nitrides}
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C30B 35/00: Apparatus not otherwise provided for, specially adapted for the growth, production or after-treatment of single crystals or of a homogeneous polycrystalline material with defined structure
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

In various embodiments, methods of forming single-crystal AlN include providing a substantially undoped polycrystalline AlN ceramic having an oxygen concentration less than approximately 100 ppm, forming a single-crystal bulk AlN crystal by a sublimation-recondensation process at a temperature greater than approximately 2000° C., and cooling the bulk AlN crystal to a first temperature between approximately 1500° C. and approximately 1800° C. at a first rate less than approximately 250° C./hour.

## Claims

### Claim at position 1

-15. (canceled)

### Claim 16

A doped single-crystalline structure comprising Al1-xSixN, wherein the doped single-crystalline structure (i) has a conductivity greater than approximately 10−2 Ω−1 cm−1 at room temperature, (ii) has the form of a wafer having a thickness no less than 100 μm, and (iii) has a diameter no less than 1 cm.

### Claim 17 (depends on 16)

The structure of claim 16, wherein an oxygen concentration of the doped single-crystalline structure is less than 50 ppm by weight.

### Claim 18 (depends on 16)

The structure of claim 16, wherein an oxygen concentration of the doped single-crystalline structure is less than 5 ppm by weight.

### Claim 19 (depends on 16)

The structure of claim 16, wherein a thermal conductivity of the doped single-crystalline structure is greater than 270 W/m·K, as measured by the ASTM Standard E1461-01.

### Claim 20 (depends on 16)

The structure of claim 16, wherein the doped single-crystalline structure is substantially free of Si3VAlN4, VAl representing an aluminum vacancy.

### Claim 21 (depends on 16)

The structure of claim 16, wherein, within the doped single-crystalline structure, an amount of Si present as SiN exceeds an amount of Si present as Si3N4.

### Claim 22

A single-crystalline bulk AlN crystal having (i) a conductivity greater than approximately 10−2 Ω−1 cm−1 at room temperature, (ii) the form of a wafer having a thickness no less than 100 μm, and (iii) a diameter no less than 1 cm.

### Claim 23 (depends on 22)

The crystal of claim 22, wherein the conductivity is n-type.

### Claim 24 (depends on 22)

The crystal of claim 22, wherein an oxygen concentration of the AlN crystal is less than 50 ppm by weight.

### Claim 25 (depends on 22)

The crystal of claim 22, wherein an oxygen concentration of the AlN crystal is less than 5 ppm by weight.

### Claim 26 (depends on 22)

The crystal of claim 22, wherein a thermal conductivity of the AlN crystal is greater than 270 W/m·K, as measured by the ASTM Standard E1461-01.

### Claim 27 (depends on 22)

The crystal of claim 22, wherein the AlN crystal is doped with silicon.

### Claim 28 (depends on 22)

The crystal of claim 22, wherein (i) the AlN crystal is substantially free of extrinsic electron-donating dopants, (ii) the conductivity is n-type, and (iii) the conductivity of the AlN crystal arises at least in part from the presence of excess Al atoms and nitrogen vacancies therein.

### Claim 29

An AlN single crystal having (i) a thickness no less than 100 μm, (ii) a diameter no less than 1 cm, and (iii) a coefficient of optical absorption no more than 20 cm−1 over the entire wavelength range of 215 nm to 4500 nm.

### Claim 30 (depends on 29)

The AlN single crystal of claim 29, wherein the coefficient of optical absorption is less than 10 cm−1 over the entire wavelength range of 250 nm to 400 nm.

### Claim 31 (depends on 29)

The AlN single crystal of claim 29, wherein the coefficient of optical absorption is less than 10 cm−1 over the entire wavelength range of 300 nm to 350 nm.

### Claim 32 (depends on 29)

The AlN single crystal of claim 29, wherein an oxygen concentration of the AlN single crystal is less than 50 ppm by weight.

### Claim 33 (depends on 29)

The AlN single crystal of claim 29, wherein an oxygen concentration of the AlN single crystal is less than 5 ppm by weight.

### Claim 34 (depends on 29)

The AlN single crystal of claim 29, wherein a thermal conductivity of the AlN single crystal is greater than 270 W/m·K, as measured by the ASTM Standard E1461-01.