# US 2019/0316266 A1 · Electrolytic copper foil for secondary battery, having enhanced flexural resistance, and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0316266 A1
- Document ID: US20190316266A1
- Status: Published application
- Kind: A1
- Application number: 16/343,553
- Filed: 2017-03-28
- Published: 2019-10-17
- Earliest claimed: 2016-11-11
- Assignees: Iljin Materials Co., Ltd.
- Applicants: Iljin Materials Co., Ltd.
- Inventors: Sun Hyoung Lee; Tae Jin Jo; Seul-Ki Park; Ki Deok Song
- Web page: https://patentgrep.com/patent/US20190316266A1

## CPC

- C22C 9/00: Alloys based on copper
- C25D 3/38: of copper
- C25D 1/04: Wires; Strips; Foils
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0452: {from solutions}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/38: of elements or alloys
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to an electrolytic copper foil for a secondary battery, having excellent flexural resistance, and a method for producing the electrolytic copper foil. The electrolytic copper foil for a secondary battery has excellent flexural resistance even without the use of many additives in a copper electrolyte when producing a copper foil. The electrolytic copper foil for a secondary battery according to the present invention is an electrolytic copper foil for a secondary battery, which is produced from a plating solution, containing total organic carbon (TOC), cobalt and arsenic, by using a drum and is coated with a cathode active material, wherein the ratio between the TOC, cobalt and arsenic contained in the electrolytic copper foil follows the following formula 1: [Formula 1] TOC/(cobalt+arsenic)=1.30-1.55.

## Claims

### Claim 1

An electrolytic copper foil for a secondary battery, wherein the electrolytic copper foil is produced using a drum in a plating solution containing copper, total organic carbon (TOC), cobalt, and arsenic, wherein the electrolytic copper foil is coated with a cathode active material, wherein a content of TOC and contents of cobalt, and arsenic contained in the electrolytic copper foil satisfy a following Equation 1:
TOC content/(cobalt content+arsenic content)=1.30 to 1.55. [Equation 1]

### Claim 2 (depends on 1)

The electrolytic copper foil of claim 1, wherein the electrolytic copper foil has bending times greater than or equal to 110 in a MIT bending test.

### Claim 3 (depends on 1)

The electrolytic copper foil of claim 1, wherein a concentration of the TOC contained in the plating solution is 100 ppm or greater.

### Claim 4 (depends on 1)

The electrolytic copper foil of claim 1, wherein the electrolytic copper foil has one face in direct contact with the drum and the other face opposite to said one face, wherein a Rz roughness of each of said one and other faces is smaller than or equal to 2.0 μm.

### Claim 5 (depends on 1)

The electrolytic copper foil of claim 1, wherein a tensile strength of the electrolytic copper foil is in a range of 30 kgf/mm2 to 51 kgf/mm2.

### Claim 6 (depends on 1)

The electrolytic copper foil of claim 1, wherein an elongation of the electrolytic copper foil is in a range of 2% to 15%.

### Claim 7 (depends on 1)

The electrolytic copper foil of claim 1, wherein a thickness of the electrolytic copper foil is in a range of 4 μm to 10 μm.

### Claim 8

A method for producing an electrolytic copper foil for a secondary battery, the method comprising:
(1) preparing a plating solution containing copper, total organic carbon (TOC), cobalt, and arsenic;
(2) performing electrolytic-plating of the plating solution using a drum at a temperature of 30° C. to 70° C. by applying a current at a current density 30 ASD to 150 ASD to the drum, thereby to form an electrolytic copper foil; and
(3) coating a cathode active material with the electrolytic copper foil,
wherein a content of TOC and contents of cobalt, and arsenic contained in the electrolytic copper foil satisfy a following Equation 1:
TOC content/(cobalt content+arsenic content)=1.30 to 1.55. [Equation 1]

### Claim 9 (depends on 8)

The method of claim 8, wherein each of a tensile strength and an elongation at −30° C. of the electrolytic copper foil is maintained to be greater than or equal to 80% of each of a tensile strength and an elongation at a room temperature of the electrolytic copper foil.

### Claim 10 (depends on 8)

The method of claim 8, wherein a concentration of the TOC contained in the plating solution is 100 ppm or greater.

### Claim 11 (depends on 8)

The method foil of claim 8, wherein the electrolytic copper foil formed by the electrolytic-plating in (2) has one face in direct contact with the drum and the other face opposite to said one face, wherein a Rz roughness of each of said one and other faces is smaller than or equal to 2.0 μm.

### Claim 12 (depends on 8)

The method of claim 8, wherein a tensile strength of the electrolytic copper foil is in a range of 30 kgf/mm2 to 51 kgf/mm2.

### Claim 13 (depends on 8)

The method of claim 8, wherein an elongation of the electrolytic copper foil is in a range of 2% to 15%.

### Claim 14 (depends on 8)

The method of claim 8, wherein a thickness of the electrolytic copper foil is in a range of 4 μm to 10 μm.