# US 2019/0316265 A1 · A process for obtaining copper from waste fishing nets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0316265 A1
- Document ID: US20190316265A1
- Status: Published application
- Kind: A1
- Application number: 16/471,691
- Filed: 2016-12-22
- Published: 2019-10-17
- Earliest claimed: 2016-12-22
- Assignees: AquafilSLO d.o.o.
- Applicants: AquafilSLO d.o.o.
- Inventors: Denis Jahic
- Web page: https://patentgrep.com/patent/US20190316265A1

## CPC

- C22B 15/0067: {with acids or salts thereof}
- C22B 7/007: {by acid leaching}
- C25C 1/12: of copper
- C09D 5/1606: {characterised by the anti-fouling agent}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention refers to a method for recovering copper from waste fishing nets. The method of the invention includes washing of nets in a washing liquid, wherein an antifouling coating and other impurities are removed from the surface of the nets to a largest extent possible. The washing liquid is water; NaOH can also be added into the water in order to improve the efficiency of washing, such that the NaOH concentration in the water is up to 20%. The suspension of the washing liquid, sludge and other impurities, resulting from the washing step, is led to a separation step. The sludge obtained in the separation step is led to the dissolution step in an acidic medium. A strong mineral acid is selected as the acidic medium, such as H2SO4, HNO3, HCl, a mixture of strong mineral acids or a mixture of one or several strong mineral acids with H2O2. Then, the non-dissolved sludge is separated from the solution of copper ions Cu2+ in the acidic medium, the solution of copper ions Cu2+ in the acidic medium is led to electrolysis, wherein elementary copper having a purity of more than 94% is deposited on the cathode. The non-dissolved residual sludge can be optionally led to thermal treatment to the reactor, where the residual paraffins and co-polymers are removed at a temperature ranging from 500° C. to 900° C. The remaining ash may contain up to 30% by weight of copper compounds based on the weight of the ash, particularly in the form of copper(ll) oxide CuO, less in the form of copper(l) oxide Cu2O and copper phosphates Cu(H2PO4)2, Na6Cu9(PO4)8. This ash is then led to dissolution in the acidic medium and to further steps of the method. The proposed method of the invention improves the method for recycling waste nets, such that not only pure polyamide is obtained from the nets but also elementary copper, which has a double benefit: elementary copper in a sufficiently pure form is a useful raw material, moreover, the quantity of copper in final waste is reduced, consequently a negative impact on the environment is reduced and the cost of waste disposal of the method is reduced as well.

## Claims

### Claim 1

A method for recovering copper from waste nets, preferably from waste fish farming nets protected by copper-based antifouling coatings and containing predominantly copper(I) oxide Cu2O, pigments, binders and waxes, characterized by including the following steps:
A) washing of nets in a washing liquid containing between 80 to 100% of water and between 0 to 20% of a washing additive; wherein a result of the washing is a suspension of a washing liquid, sludge and other impurities such as paraffins and copolymers, wherein the sludge contains copper compounds in the form of Cu2O, CuO and Cu2Cl(OH)3, impurities and rests of the antifouling coating, particularly paraffins and the EVA co-polymer;
B) separation of the sludge from the suspension from step A, wherein the sludge, after the separation, comprises:
copper compounds in the form of copper oxides Cu2O and CuO and copper oxychloride Cu2Cl(OH)3,
unseparated washing liquid, and
a rest containing especially impurities accumulated on the nets and residues of the antifouling coating, especially paraffins and EVA co-polymers;
C) dissolution of the sludge in an acidic medium at temperatures ranging from 0 to 100° C. for 1 to 4 hours, wherein the acidic medium is a strong mineral acid, a mixture of strong mineral acids or a mixture of one or several strong mineral acids with H2O2, where the copper compounds contained in the sludge get dissolved, wherewith a solution is obtained, wherein the concentration of copper ions Cu2+ in the acidic medium amounts to at least 20 g/L, and a non-dissolved residual sludge;
D) separation of the non-dissolved residual sludge from the solution, wherewith a solution of Cu2+ ions in the acidic medium is obtained, said medium representing an electrolyte that is then led to an electrolytic cell;
E) electrolysis of the solution of copper ions Cu2+ in the acidic medium, obtained in step D, in the electrolytic cell, where elementary copper gets deposited on the cathode.

### Claim 2 (depends on 1)

The method according to claim 1, characterized in that the non-dissolved residual sludge which remains after the separation in step D, is led to thermal treatment to a reactor, where residual paraffins and co-polymers are removed at T ranging from 500 to 900° C.; wherewith ash is obtained that contains up to 30% by weight of copper compounds particularly in the form of copper(II) oxide CuO, less in the form of copper(I) oxide Cu2O and copper phosphates Cu(H2PO4)2, Na6Cu9(PO4)8 calculated based on the weight of the ash, and is led to dissolution in the acidic medium under the conditions specified in step C and to further steps of the method D and E.

### Claim 3 (depends on 2)

The method according to claim 2, characterized in that the ash, after having been thermally treated, is added to the sludge from step B and the method continues according to steps C to E.

### Claim 4 (depends on 1)

The method according to claim 1, characterized in that the washing additive is NaOH, wherein the NaOH concentration in the water is preferably 2%.

### Claim 5 (depends on 1)

The method according to claim 1, characterized in that the washing of the nets in the washing solution is carried out by friction.

### Claim 6 (depends on 1)

The method according to claim 1, characterized in that the mineral acids are selected among H2SO4 or HNO3 or HCl or a mixture of HNO3 and HCl.

### Claim 7 (depends on 1)

The method according to claim 1, characterized in that the acidic medium is H2SO4 with a concentration from and including 0.5 up to and including 4 M, preferably with the H2SO4 concentration of 1 M, the temperature is room temperature, dissolution time is 3 hours, dissolution yield is between 50 and 95%, wherein a solution with a concentration of copper ions Cu2+ of at least 40 g/L is obtained.

### Claim 8 (depends on 1)

The method according to claim 1, characterized in that, if the concentration of copper ions Cu2+ is less than 40 g/L, the concentration is increased to at least 40 g/L by using Cu2+ ion selective ion exchangers.

### Claim 9 (depends on 1)

The method according to claim 1, characterized in that prior to the electrolysis the solution of copper ions in the acid is filtered by filtration with active carbon, wherein organic substances are removed from the solution.

### Claim 10 (depends on 1)

The method according to claim 1, characterized in that the electrolysis is carried out at an initial current density of at least 500 A/m2, which is reduced gradually to 200 A/m2 based on the quantity of the deposited copper, in a temperature range from 0 to 95° C., and elementary copper with a purity of at least 94% is deposited on the cathode.

### Claim 11

A method of recovering copper from waste nets, preferably from waste fish farming nets protected by copper-based antifouling coatings and containing predominantly copper(I) oxide Cu2O, pigments, binders and waxes, characterized in that the waste nets are directly led to thermal treatment in a reactor, where at a temperature ranging from 500° C. to 900° C. all organic substances, such as paraffins, co-polymers and synthetic polymers, from which the nets are made, are removed, the ash which remains after the thermal treatment and contains copper compounds particularly in the form of copper (II) oxide CuO, less in the form of copper(I) oxide Cu2O and copper phosphates Cu(H2PO4)2, Na6Cu9(PO4)8 is then processed according to steps C to E of the method.