# US 2019/0316240 A1 · Cold-rolled steel sheet having excellent corrosion resistance and formability, and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0316240 A1
- Document ID: US20190316240A1
- Status: Published application
- Kind: A1
- Application number: 16/472,252
- Filed: 2017-12-11
- Published: 2019-10-17
- Earliest claimed: 2016-12-22
- Assignees: Posco
- Applicants: Posco
- Inventors: Min-Ho JO; Jong-Hwa Kim
- Web page: https://patentgrep.com/patent/US20190316240A1

## CPC

- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- B32B 15/012: {one layer being formed of an iron alloy or steel, another layer being formed of aluminium or an aluminium alloy}
- C21D 1/02: Hardening articles or materials formed by forging or rolling, with no further heating beyond that required for the formation
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 9/46: for sheet metals
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/26: with niobium or tantalum
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

Disclosed are a cold rolled steel sheet and a method for manufacturing same, the cold-rolled steel sheet: comprising, by wt %, 0.01% or less of C, 0.5% or less of Si, 0.1-0.5% of Mn, 0.1% or less of Al, 0.01% or less of P, 0.01% or less of S, 0.005% or less of N and 0.2-0.8% of Nb; comprising one or more of 0.5% or less of Sb, 3.0% or less of Cr, 1.0% or less of Mo and 0.5% or less of W; comprising the balance of Fe and inevitable impurities; and satisfying the following relation 1. [relation 1] 0.2≤[Sb]/0.5+[Cr]/3.0+[Mo]/1.0+[W]/0.5≤1.5 (Here, [Sb], [Cr], [Mo], and [W] respectively mean the amounts (wt %) of the corresponding elements contained.)

## Claims

### Claim 1

A cold rolled steel sheet comprising:
by wt %, 0.01% or less (excluding 0%) of carbon (C), 0.5% or less (excluding 0%) of silicon (Si), 0.1 to 0.5% of manganese (Mn), 0.1% or less (excluding 0%) of aluminum (Al), 0.01% or less (excluding 0%) of phosphorus (P), 0.01% or less of sulfur (S), 0.005% or less of nitrogen (N) and 0.2 to 0.8% of niobium (Nb), the cold rolled steel sheet comprising one or more of 0.5% or less of antimony (Sb), 3.0% or less of chromium (Cr), 1.0% or less of molybdenum (Mo) and 0.5% or less of tungsten (W), comprising a remainder of iron (Fe) and inevitable impurities, and satisfying the following relational expression 1: 0.2≤[Sb]/0.5+[Cr]/3.0+[Mo]/1.0+[W]/0.5≤1.5, where [Sb], [Cr], [Mo] and [W] are the amounts (wt %) of relevant elements, respectively.

### Claim 2 (depends on 1)

The cold rolled steel sheet of claim 1, wherein a composite enriched layer of Nb and one or more of Sb, Cr, Mo and W is formed in a subsurface region of the cold rolled steel sheet in a thick direction in a corrosive environment,
wherein the composite enriched layer has a thickness of 1 μm or less (excluding 0 μm).

### Claim 3 (depends on 2)

The cold rolled steel sheet of claim 2, wherein a Nb content in the composite enriched layer of Nb and one or more of Sb, Cr, Mo and W is 10 atomic % or more, and a sum of the contents of one or more of Sb, Cr, Mo and W is 20 atomic % or more, when a corrosion test is performed by Method B of JASO M 611-92.

### Claim 4 (depends on 1)

The cold rolled steel sheet of claim 1, wherein an average grain size of crystal grains constituting the cold-rolled steel sheet is 9 μm or more.

### Claim 5 (depends on 1)

The cold rolled steel sheet of claim 1, wherein the cold-rolled steel sheet has a corrosion loss of 200 mg/cm2 or less when subjected to a corrosion test by Method B of JASO M 611-92.

### Claim 6 (depends on 1)

The cold rolled steel sheet of claim 1, wherein the cold rolled steel sheet has an average value (rm) of a plasticity Lankford value of 1.8 or more and an elongation of 38% or more.

### Claim 7 (depends on 1)

The cold rolled steel sheet of claim 1, wherein the cold rolled steel sheet is provided with an aluminum-based plating layer formed on a surface thereof.

### Claim 8

A method of manufacturing a cold rolled steel sheet, comprising:
reheating a slab at a temperature of 1200° C. or higher, the slab including, by wt %, 0.01% or less (excluding 0%) of carbon (C), 0.5% or less (excluding 0%) of silicon (Si), 0.1 to 0.5% (excluding 0%) of manganese (Mn), 0.1% or less (excluding 0%) of aluminum (Al), 0.01% or less of phosphorus (P), 0.01% or less of sulfur (S), 0.005% or less of nitrogen (N) and 0.2 to 0.8% of niobium (Nb),
the slab comprising one or more of 0.5% or less of antimony (Sb), 3.0% or less of chromium (Cr), 1.0% or less of molybdenum (Mo) and 0.5% or less of tungsten (W), comprising a remainder of iron (Fe) and inevitable impurities, and satisfying the following relational expression 1: 0.2≤[Sb]/0.5+[Cr]/3.0+[Mo]/1.0+[W]/0.5≤1.5, where [Sb], [Cr], [Mo] and [W] are the amounts (wt %) of relevant elements, respectively;
finish rolling the reheated slab at a temperature of Ar3° C. or higher to obtain a hot-rolled steel sheet;
coiling the hot-rolled steel sheet at a temperature ranging from 550 to 750° C.;
cold rolling the coiled hot-rolled steel sheet at a reduction ratio of 50 to 95% to obtain a cold-rolled steel sheet; and
continuously annealing the cold-rolled steel sheet at a temperature ranging from 600 to 900° C.

### Claim 9 (depends on 8)

The method of manufacturing a cold rolled steel sheet of claim 8, further comprising forming an aluminum-based plating layer on a surface of the continuously annealed cold-rolled steel sheet after the continuously annealing.