# US 2019/0316237 A1 · Ferritic stainless steel having excellent ridging property and excellent surface quality and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0316237 A1
- Document ID: US20190316237A1
- Status: Published application
- Kind: A1
- Application number: 16/468,883
- Filed: 2017-07-04
- Published: 2019-10-17
- Earliest claimed: 2016-12-13
- Assignees: Posco
- Applicants: Posco
- Inventors: Soo Ho PARK; Kye Man LEE
- Web page: https://patentgrep.com/patent/US20190316237A1

## CPC

- C21D 8/04: to produce plates or strips for drawing, e.g. for deep-drawing
- C22C 38/18: containing chromium
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 8/0263: {following hot rolling}
- C21D 8/0268: {between cold rolling steps}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 8/0426: {Hot rolling}
- C21D 8/0436: {Cold rolling}
- C21D 8/0473: {Final recrystallisation annealing}
- C21D 9/0081: {for slabs; for billets}
- C21D 9/48: deep-drawing sheets
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/40: with nickel
- C21D 2211/005: Ferrite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Disclosed herein are a ferritic stainless steel having excellent ridging properties and excellent surface quality of a final product by modifying a microstructure of a central area of a cross-section by further performing cold rolling before hot annealing. A ferritic stainless steel according to the present disclosure includes, by wt %, 0.005 to 0.1% of carbon (C), 0.01 to 2.0% of silicon (Si), 0.01 to 1.5% of manganese (Mn), 0.05% or less of phosphorus (P), 0.005% or less of sulfur (S), 10 to 30% of chromium (Cr), 0.005 to 0.1% of nitrogen (N), 0.005 to 0.2% of aluminum (Al), and the remainder of iron (Fe) and other impurities, wherein a γmax value is in the range of 20% to less than 50%, and a surface microgroove area ratio is 2.0% or less.

## Claims

### Claim 1

A ferritic stainless steel having excellent ridging properties and excellent surface quality comprising, by wt %, 0.005 to 0.1% of carbon (C), 0.01 to 2.0% of silicon (Si), 0.01 to 1.5% of manganese (Mn), 0.05% or less of phosphorus (P), 0.005% or less of sulfur (S), 10 to 30% of chromium (Cr), 0.005 to 0.1% of nitrogen (N), 0.005 to 0.2% of aluminum (Al), and the remainder of iron (Fe) and other impurities,
wherein a γmax value represented by Formula 1 below is in the range of 20% to less than 50%,
420×C+470×N+10×Mn+180−11.5×Cr−11.5×Si−52.0×Al (1)
wherein C, N, Mn, Cr, Si, and Al refer to amounts of respective elements (wt %).

### Claim 2 (depends on 1)

The ferritic stainless steel according to claim 1, wherein the stainless steel has a surface microgroove area ratio of 2.0% or less.

### Claim 3 (depends on 1)

The ferritic stainless steel according to claim 1, wherein the stainless steel has a ridging height of 12 μm or less.

### Claim 4 (depends on 1)

The ferritic stainless steel according to claim 1, wherein the stainless steel has an r-bar value of 1.2 or greater.

### Claim 5

A method of manufacturing a ferritic stainless steel having excellent ridging properties and excellent surface quality, the method comprising:
preparing a slab comprising, by wt %, 0.005 to 0.1% of carbon (C), 0.01 to 2.0% of silicon (Si), 0.01 to 1.5% of manganese (Mn), 0.05% or less of phosphorus (P), 0.005% or less of sulfur (S), 10 to 30% of chromium (Cr), 0.005 to 0.1% of nitrogen (N), 0.005 to 0.2% of aluminum (Al), and the remainder of iron (Fe) and other impurities and having a γmax value represented by Formula 1 below and satisfying 20% to less than 50%;
hot rolling the slab by reheating;
coiling the hot rolled steel sheet; and
cold rolling the coiled hot rolled steel sheet before conducting hot annealing:
420×C+470×N+10×Mn+180−11.5×Cr−11.5×Si−52.0×Al (1)
wherein C, N, Mn, Cr, Si, and Al refer to amounts of respective elements (wt %).

### Claim 6 (depends on 5)

The method according to claim 5, wherein a coiling temperature is 750° C. or higher in the coiling of the hot rolled steel sheet.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the cold rolling is performed by asymmetric cold rolling.

### Claim 8 (depends on 5)

The method according to claim 5, wherein the cold rolling or the asymmetric cold rolling is performed with a reduction ratio of 30% or more.

### Claim 9 (depends on 7)

The method according to claim 7, wherein the asymmetric cold rolling is performed under rolling conditions of a speed ratio between upper and lower rolling rolls (Vh/Vl) of 1.25 or greater and a rolling shape factor (l/d) of 1.7 or greater.
wherein
Vh: speed of fast roll,
Vl: speed of slow roll,
rolling shape factor: l/d=2√{square root over (r(h0−h))}/(h0+h),
l: length to which contact arc between roll and steel sheet in rolling roll bite is projected,
d: average thickness of the steel sheet, d=(h0+h)/2,
r: radius of rolling roll,
h0: initial thickness of steel sheet, and
h: final thickness of steel sheet.

### Claim 10 (depends on 9)

The method according to claim 9, wherein a height of a stainless steel prepared by performing hot annealing, secondary cold rolling, and cold annealing after the asymmetric cold rolling is 10 μm or less.

### Claim 11 (depends on 5)

The method according to claim 5, further comprising hot annealing after the cold rolling.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the hot annealing is performed in a temperature range of 550 to 950° C. for 60 minutes or less.

### Claim 13 (depends on 11)

The method according to claim 11, wherein an average aspect ratio of a structure of a thickness center of a cross-section of the hot annealed steel sheet is 4.0 or less after the hot annealing.