# US 2019/0316219 A1 · Thick steel plate having excellent cryogenic impact toughness and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0316219 A1
- Document ID: US20190316219A1
- Status: Published application
- Kind: A1
- Application number: 16/472,246
- Filed: 2017-12-20
- Published: 2019-10-17
- Earliest claimed: 2016-12-22
- Assignees: Posco
- Applicants: Posco
- Inventors: Mo-Chang Kang; Jong-In Choi
- Web page: https://patentgrep.com/patent/US20190316219A1

## CPC

- C21D 8/0226: {Hot rolling}
- C21D 9/46: for sheet metals
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0263: {following hot rolling}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 2211/005: Ferrite
- C21D 2211/009: Pearlite
- C22C 38/14: containing titanium or zirconium
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The purpose of one aspect of the present invention is to provide: a thick steel plate capable of removing a conventional normalizing treatment required for ensuring toughness low temperature and cryogenic environments, and having properties equal to or better than those of a conventional steel subjected to the normalizing treatment; and a method for manufacturing the method.

## Claims

### Claim 1

A thick steel plate having excellent cryogenic impact toughness, comprising:
by weight %, 0.02% to 0.10 of carbon (C), 0.6 to 1.7% of manganese (Mn), 0.5% or less (excluding 0%) of silicon (Si), 0.02% or less of phosphorus (P), 0.015% or less of sulfur (S), 0.005 to 0.05% of niobium (Nb), 0.005 to 0.07% of vanadium (V), and a remainder of iron (Fe) and other unavoidable impurities,
wherein the thick steel plate has, by area fraction, a mixed structure of ferrite of 85 to 95% and pearlite of 5 to 15%, as a microstructure.

### Claim 2 (depends on 1)

The thick steel plate of claim 1, wherein the thick steel plate further comprises, by weight %, at least one of not more than 0.5% of nickel (Ni) and not more than 0.5% of chromium (Cr).

### Claim 3 (depends on 1)

The thick steel plate of claim 1, wherein the thick steel plate further comprises 0.005 to 0.035 weight % of titanium (Ti).

### Claim 4 (depends on 1)

The thick steel plate of claim 1, wherein a grain size of ferrite is 7.5 or more of ASTM grain size number.

### Claim 5 (depends on 1)

The thick steel plate of claim 1, wherein the thick steel plate has impact toughness of 300 J or more at −60° C.

### Claim 6

A method of manufacturing a thick steel plate having excellent cryogenic impact toughness, comprising:
reheating a steel slab at a temperature of 1100° C. or higher, the steel slab including, by weight %, 0.02% to 0.10 of carbon (C), 0.6 to 1.7% of manganese (Mn), 0.5% or less (excluding 0%) of silicon (Si), 0.02% or less of phosphorus (P), 0.015% or less of sulfur (S), 0.005 to 0.05% of niobium (Nb), 0.005 to 0.07% of vanadium (V), and a remainder of iron (Fe) and other unavoidable impurities,
finishing hot-rolling the reheated steel slab at a temperature of 850 to 910° C. to produce a hot-rolled steel plate; and
air-cooling the hot-rolled steel plate to a room temperature after the finishing hot-rolling.

### Claim 7 (depends on 6)

The method of claim 6, wherein the steel slab further comprises, by weight %, at least one of not more than 0.5% of nickel (Ni) and not more than 0.5% of chromium (Cr).

### Claim 8 (depends on 6)

The method of claim 6, wherein the steel slab further comprises 0.005 to 0.035 weight % of titanium (Ti).