# US 2019/0316022 A1 · Settable, form-filling loss circulation control compositions comprising in situ foamed non-hydraulic sorel cement systems and method of use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0316022 A1
- Document ID: US20190316022A1
- Status: Published application
- Kind: A1
- Application number: 16/454,925
- Filed: 2019-06-27
- Published: 2019-10-17
- Earliest claimed: 2018-01-24
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: B. Raghava Reddy
- Web page: https://patentgrep.com/patent/US20190316022A1

## CPC

- C09K 8/487: Fluid loss control additives; Additives for reducing or preventing circulation loss
- C04B 9/00: Magnesium cements or similar cements
- C04B 9/02: Magnesium cements containing chlorides, e.g. Sorel cement
- C04B 9/04: Magnesium cements containing sulfates, nitrates, phosphates or fluorides
- C04B 12/025: {Phosphates of ammonium or of the alkali or alkaline earth metals}
- C04B 28/32: Magnesium oxychloride cements, e.g. Sorel cement
- C04B 28/34: containing cold phosphate binders
- C04B 38/02: by adding chemical blowing agents
- C09K 8/473: Density reducing additives, e.g. for obtaining foamed cement compositions
- C04B 2111/00689: {of the setting type}
- E21B 33/13: Methods or devices for cementing, for plugging holes, crevices or the like
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

This document relates to settable, non-hydraulic foamed cement compositions comprising nitrogen gas-generating compositions used for loss circulation control.

## Claims

### Claim 1

A method of treating a lost circulation zone, the method comprising:
a) forming a foamed cementitious composition comprising:
magnesium oxide (MgO);
a salt comprising at least one of magnesium chloride (MgCl2), magnesium sulfate (MgSO4), ammonium hydrogen phosphate (NH4H2PO4), or a hydrate thereof;
a nitrogen gas-generating compound; and
a foam surfactant; and
b) introducing the foamed cementitious composition into the lost circulation zone.

### Claim 2 (depends on 1)

The method of claim 1, wherein the nitrogen gas-generating compound comprises an azo compound.

### Claim 3 (depends on 2)

The method of claim 2, wherein the azo compound is about 1% to about 10% by weight of the MgO.

### Claim 4 (depends on 2)

The method of claim 2, comprising an amine activator comprising at least one of carbohydrazide (CHZ), tetraethylenepentamine (TEPA), or hydrazine sulfate.

### Claim 5 (depends on 4)

The method of claim 4, wherein the weight ratio of the azo compound to the amine activator is about 5:1 to about 1:5.

### Claim 6

A method of treating a lost circulation zone fluidly connected to a wellbore, the method comprising:
a) forming a foamed cementitious composition comprising:
magnesium oxide (MgO);
a salt comprising at least one of magnesium chloride (MgCl2), magnesium sulfate (MgSO4), ammonium hydrogen phosphate (NH4H2PO4), or a hydrate thereof;
a hydrazide or a semi-carbazide, or both;
an oxidizer; and
a foam surfactant; and
b) introducing the foamed cementitious composition into the lost circulation zone.

### Claim 7 (depends on 6)

The method of claim 6, wherein the oxidizer comprises at least one of peroxide, persulfate, percarbonate, perbromate, perborate salts of ammonium, alkali earth metals, or alkaline earth metals.

### Claim 8 (depends on 7)

The method of claim 7, wherein the weight ratio of the hydrazide or semi-carbazide to the oxidizer is about 1:0.25 to about 1:5.