# US 2019/0316019 A1 · Drill fluid and method for tunneling

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0316019 A1
- Document ID: US20190316019A1
- Status: Published application
- Kind: A1
- Application number: 16/317,259
- Filed: 2018-06-22
- Published: 2019-10-17
- Earliest claimed: 2007-03-02
- Assignees: Canadian Energy Services L.P.
- Applicants: Canadian Energy Services L.P.
- Inventors: Carl Keith SMITH; Josh GAWRYLUK
- Web page: https://patentgrep.com/patent/US20190316019A1

## CPC

- C09K 8/05: containing inorganic compounds only, e.g. mixtures of clay and salt
- C09K 8/203: {Wood derivatives, e.g. lignosulfonate, tannin, tall oil, sulfite liquor}
- C09K 8/206: {Derivatives of other natural products, e.g. cellulose, starch, sugars}
- E21B 21/003: {Means for stopping loss of drilling fluid (plastering the borehole wall E21B33/138)}
- E21B 21/062: {by mixing components}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

A method for drilling a tunnel through a formation must address environmental concerns. One tunneling method comprises the steps of: preparing a mixed metal-viscosified drilling fluid including bentonite, a mixed metal viscosifier and controlling pH to 8.5 to 9.5 to permit a reaction between the bentonite and the mixed metal viscosifier; adding at least one of: (i) calcium sulfate and (ii) a potassium salt; and pumping the drilling fluid while drilling the tunnel with the pH lowered to 7-9. The amount of mixed metal viscosifier used can be limited such that the weight ratio of mixed metal viscosifier to MBT reaches up to 1:30. In the event that there is a problematic increase in viscosity, a non-toxic anionic thinner can be added to the drilling fluid. One such anionic thinner is a polyacrylate.

## Claims

### Claim 1

A method for drilling a tunnel through a formation, the method comprising:
preparing a mixed metal-viscosified drilling fluid including bentonite, a mixed metal viscosifier and controlling pH to 8.5 to 9.5 to permit a reaction between the bentonite and the mixed metal viscosifier;
adding at least one of: (i) calcium sulfate and (ii) a potassium salt; and
pumping the drilling fluid while drilling the tunnel with the pH lowered to 7-9.

### Claim 2 (depends on 1)

The method of claim 1 wherein preparing the mixed metal-viscosified drilling fluid includes mixing water, 15 to 45 kg/m3 bentonite and the mixed metal viscosifier at a weight ratio of 1:3 to 1:20, viscosifier to bentonite, and pumping proceeds with a clay load increasing from incorporated clay such that the weight ratio of the mixed metal viscosifier:total clay is up to 1:30.

### Claim 3 (depends on 1)

The method of claim 1 wherein the potassium salt is selected from potassium sulfate or potassium chloride and adding adds the potassium salt for a concentration of 1 to 5% w/v.

### Claim 4 (depends on 1)

The method of claim 1 wherein adding brings the calcium sulfate to 0.05 to 1.0% w/v.

### Claim 5 (depends on 1)

The method of claim 1 further comprising adding a non-toxic anionic thinner when the drilling fluid shows a problematic increase in viscosity as indicated by:
a) a funnel viscosity of 70 seconds/L;
b) a yield point of 30 Pa; or
c) an MBT of 60 kg/m3.

### Claim 6 (depends on 1)

The method of claim 1 wherein the non-toxic anionic thinner is selected from the group consisting of: coal fines, lignite, lignite resin, humalite, poly-anionic cellulose, tetra potassium pyrophosphate (TKPP), sodium acid pyrophosphate, tetra sodium pyrophosphate, polyacrylic acid, polyacrylates, polyacrylate co-polymers or xanthan gum.

### Claim 7 (depends on 1)

The method of claim 1 further comprising adding a polyacrylate anionic thinner when the drilling fluid shows a problematic increase in viscosity as indicated by:
a) a funnel viscosity of 70 seconds/L;
b) a yield point of 30 Pa; or
c) an MBT of 60 kg/m3.

### Claim 8 (depends on 1)

The method of claim 1 wherein:
preparing the mixed metal-viscosified drilling fluid includes mixing water, 15 to 45 kg/m3 bentonite and the mixed metal viscosifier at a weight ratio of 1:3 to 1:20, viscosifier to bentonite,
pumping proceeds with a clay load increasing from incorporated drilled clay and limited addition of further mixed metal viscosifier such that the weight ratio of the mixed metal viscosifier:total clay is up to 1:30; and
further comprising adding humalite or a polyacrylate anionic thinner when the drilling fluid shows a problematic increase in viscosity as indicated by:
a) a funnel viscosity of 70 seconds/L;
b) a yield point of 30 Pa; or
c) an MBT of 60 kg/m3.

### Claim 9

A method for drilling a tunnel through a formation, the method comprising:
providing a mixed metal-viscosified drilling fluid; circulating the drilling fluid through the tunnel while drilling into the formation; monitoring the drilling fluid for a condition of drilling indicative of a problematic increase in viscosity of the drilling fluid; adding to the drilling fluid at least 1% w/v potassium salt; and adding a non-toxic anionic thinner to the drilling fluid to adjust the viscosity of the drilling fluid.

### Claim 10 (depends on 9)

The method of claim 9 wherein providing the mixed metal-viscosified drilling fluid includes providing an aqueous-based drilling fluid including 15 to 45 kg/m3 bentonite, mixed metal viscosifier at a weight ratio of 1:3 to 1:30, viscosifier to bentonite and a base to maintain the pH above 7.0.

### Claim 11 (depends on 9)

The method of claim 9 wherein adding a potassium salt occurs during the step of providing.

### Claim 12 (depends on 9)

The method of claim 9 wherein adding a potassium salt occurs after identifying the condition of drilling indicative of a problematic increase in viscosity of the drilling fluid.

### Claim 13 (depends on 9)

The method of claim 9 wherein adding a potassium salt brings the concentration of potassium salt to 1 to 5% w/v.

### Claim 14 (depends on 9)

The method of claim 9 wherein providing the mixed metal-viscosified drilling fluid includes: mixing bentonite in water to form a bentonite mixture; adding a mixed metal viscosifier to the bentonite mixture; adjusting pH to pH 8.5-9.5; and adding the potassium salt.

### Claim 15 (depends on 9)

The method of claim 9 further comprising adding any of fluid loss control additives and/or lost circulation materials.

### Claim 16 (depends on 9)

The method of claim 9 wherein providing the mixed metal-viscosified drilling fluid provides a drilling fluid with a yield point greater than 10 Pa.

### Claim 17 (depends on 9)

The method of claim 9 wherein adding an anionic thinner is initiated after identifying the condition of drilling indicative of a problematic increase in viscosity of the drilling fluid.

### Claim 18 (depends on 9)

The method of claim 9 wherein adding an anionic thinner brings the fluid yield point to between 10 and 60 Pa.

### Claim 19 (depends on 9)

The method of claim 9 wherein circulating the drilling fluid is initiated prior to drilling into a clay deposit.

### Claim 20 (depends on 9)

The method of claim 9 wherein circulating the drilling fluid is maintained while a clay deposit is open to the drilling fluid.

### Claim 21 (depends on 9)

The method of claim 9 wherein circulating the drilling fluid is initiated substantially at surface.

### Claim 22 (depends on 9)

The method of claim 9 wherein monitoring includes determining the viscosity of the drilling fluid.

### Claim 23 (depends on 9)

The method of claim 9 wherein monitoring includes determining the clay concentration in the drilling fluid.

### Claim 24 (depends on 9)

The method of claim 9 wherein monitoring includes considering the location of the tunnel relative to a known location of a clay deposit.

### Claim 25 (depends on 9)

The method of claim 9 wherein the condition of drilling indicative of a problematic increase in viscosity includes at least one of:
a) a funnel viscosity of 70 seconds/L;
b) a yield point of 30 Pa; and
c) an MBT of 60 kg/m3.

### Claim 26 (depends on 9)

The method of claim 9 wherein the non-toxic anionic thinner is selected from the group consisting of: coal fines, lignite, lignite resin, humalite, poly-anionic cellulose, tetra potassium pyrophosphate (TKPP), sodium acid pyrophosphate, tetra sodium pyrophosphate, polyacrylic acid, polyacrylates, polyacrylate co-polymers or xanthan gum.

### Claim 27 (depends on 9)

The method of claim 9 wherein the potassium salt is selected from the group consisting of potassium sulfate, potassium chloride, potassium acetate and potassium formate.

### Claim 28 (depends on 9)

The method of claim 9 wherein the potassium salt is potassium sulfate.

### Claim 29 (depends on 9)

The method of claim 9 wherein the potassium salt is potassium chloride.

### Claim 30 (depends on 14)

The method of claim 14 wherein the pH is adjusted using lime.

### Claim 31

A method for drilling a tunnel through a formation, the method comprising:
providing a mixed metal-viscosified drilling fluid; circulating the drilling fluid through the tunnel while drilling into the formation; monitoring the drilling fluid for a condition of drilling indicative of a problematic increase in viscosity of the drilling fluid; adding calcium sulfate to the drilling fluid to bring the concentration to at least 0.05% w/v calcium sulfate in the drilling fluid; and
adding a non-toxic anionic thinner to the drilling fluid to adjust the viscosity of the drilling fluid.

### Claim 32 (depends on 31)

The method of claim 31 wherein providing the mixed metal-viscosified drilling fluid includes providing an aqueous-based drilling fluid including 15 to 45 kg/m3 bentonite, mixed metal viscosifier at a weight ratio of 1:3 to 1:30, viscosifier to bentonite and a base to maintain the pH above 7.0.

### Claim 33 (depends on 31)

The method of claim 31 wherein adding a calcium sulfate occurs during the step of providing.

### Claim 34 (depends on 31)

The method of claim 31 wherein adding a calcium sulfate occurs after identifying the condition of drilling indicative of a problematic increase in viscosity of the drilling fluid.

### Claim 35 (depends on 31)

The method of claim 31 wherein adding calcium sulfate brings the concentration of calcium sulfate to 0.05 to 1.0% w/v.

### Claim 36 (depends on 31)

The method of claim 31 wherein providing the mixed metal-viscosified drilling fluid includes:
mixing bentonite in water to form a bentonite mixture;
adding a mixed metal viscosifier to the bentonite mixture;
adjusting pH to pH 8.5-9.5; and
adding the calcium sulfate.

### Claim 37 (depends on 31)

The method of claim 31 further comprising adding any of fluid loss control additives and/or lost circulation materials.

### Claim 38 (depends on 31)

The method of claim 31 wherein providing the mixed metal-viscosified drilling fluid provides a drilling fluid with a yield point greater than 10 Pa.

### Claim 39 (depends on 31)

The method of claim 31 wherein adding an anionic thinner is initiated after identifying the condition of drilling indicative of a problematic increase in viscosity of the drilling fluid.

### Claim 40 (depends on 31)

The method of claim 31 wherein adding an anionic thinner brings the fluid yield point to between 10 and 60 Pa.

### Claim 41 (depends on 31)

The method of claim 31 wherein circulating the drilling fluid is initiated prior to drilling into a clay deposit.

### Claim 42 (depends on 31)

The method of claim 31 wherein circulating the drilling fluid is maintained while a clay deposit is open to the drilling fluid.

### Claim 43 (depends on 31)

The method of claim 31 wherein circulating the drilling fluid is initiated substantially at surface.

### Claim 44 (depends on 31)

The method of claim 31 wherein monitoring includes determining the viscosity of the drilling fluid.

### Claim 45 (depends on 31)

The method of claim 31 wherein monitoring includes determining the clay concentration in the drilling fluid.

### Claim 46 (depends on 31)

The method of claim 31 wherein monitoring includes considering the location of the tunnel relative to a known location of a clay deposit.

### Claim 47 (depends on 31)

The method of claim 31 wherein a condition of drilling indicative of a problematic increase in viscosity includes at least one of:
a) a funnel viscosity of 70 seconds/L;
b) a yield point of 30 Pa; and
c) an MBT of 60 kg/m3.

### Claim 48 (depends on 31)

The method of claim 31 wherein the non-toxic anionic thinner is selected from the group consisting of: coal fines, lignite, lignite resin, humalite, poly-anionic cellulose, tetra potassium pyrophosphate (TKPP), sodium acid pyrophosphate, tetra sodium pyrophosphate, polyacrylic acid, polyacrylates, polyacrylate co-polymers or xanthan gum.

### Claim 49 (depends on 47)

The method of claim 47 wherein the pH is adjusted using lime.

### Claim 50

A mixed metal-viscosified drilling fluid comprising:
water;
15 to 45 kg/m3 bentonite;
a mixed metal viscosifier at a weight ratio of 1:3 to 1:30, viscosifier to bentonite;
at least 0.05% w/v calcium sulfate and/or at least 1% w/v potassium salt;
a polyacrylate anionic thinner; and
a base to maintain the pH above 7.0.

### Claim 51 (depends on 50)

The mixed metal-viscosified drilling fluid of claim 50 wherein the polyacrylate anionic thinner is selected from polyacrylic acid, polyacrylate or polyacrylate co-polymer.