# US 2019/0315659 A1 · Method for making a lightweight gypsum composition with internally generated foam and products made from same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0315659 A1
- Document ID: US20190315659A1
- Status: Published application
- Kind: A1
- Application number: 16/292,988
- Filed: 2019-03-05
- Published: 2019-10-17
- Earliest claimed: 2018-04-11
- Assignees: United States Gypsum Company
- Applicants: United States Gypsum Company
- Inventors: David D. PELOT; Samar EMAMI; Robert H. NEGRI; Juan Carlos Ruiz Castaneda; Christopher R. NELSON; John J. ROXBURGH; Edgar R. DE LA ROSA CRUZ; Jorge A. GARCIA TORRES; Miguel Gama Goicochea; Antonio CONTRERAS; Juan HUITZIL
- Web page: https://patentgrep.com/patent/US20190315659A1

## CPC

- C04B 28/14: containing calcium sulfate cements {(gypsum-paper plates E04C)}
- C04B 18/027: {Lightweight materials}
- C04B 22/064: {of the alkaline-earth metals}
- C04B 22/148: {Aluminium-sulfate}
- C04B 22/16: containing phosphorus in the anion, e.g. phosphates
- C04B 24/04: Carboxylic acids; Salts, anhydrides or esters thereof
- C04B 24/122: {Hydroxy amines}
- C04B 24/123: {Amino-carboxylic acids}
- C04B 24/2611: {Polyalkenes}
- C04B 24/2641: {Polyacrylates; Polymethacrylates}
- C04B 24/383: {Cellulose or derivatives thereof}
- C04B 28/145: {Calcium sulfate hemi-hydrate with a specific crystal form}
- C04B 38/02: by adding chemical blowing agents
- C04B 40/0039: {Premixtures of ingredients}
- C04B 2103/10: Accelerators; Activators
- C04B 2103/408: {Dispersants}
- C04B 2103/44: Thickening, gelling or viscosity increasing agents
- C04B 2111/00146: {Sprayable or pumpable mixtures}
- C04B 2111/00612: {as one or more layers of a layered structure}
- C04B 2111/00698: {for cavity walls}
- C04B 2111/40: Porous or lightweight materials
- C04B 2111/72: Repairing or restoring existing buildings or building materials
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Method of making foamed gypsum slurry having 15 to 90 volume percent gas bubbles including: passing first slurry including water and on dry basis 50 to 98 wt. % calcium sulfate hemihydrate, 1 to 50 wt. % calcium carbonate, and 0.1 to 10 wt. % cellulose thickener via a first hose to a Wye connector conduit first inlet opening at Rate C and passing alum solution via a second hose to a second inlet opening of the conduit at Rate D to create combined mixed stream passing from the conduit to a static mixer for mixing for Time 3 to activate at least a portion of the calcium carbonate and alum to generate CO2 and create the foamed gypsum slurry; transferring the slurry from the mixer to a cavity between two wall boards via a third hose. Allowing the slurry in the cavity to expand, harden and dry.

## Claims

### Claim 1

A method of making a foamed gypsum slurry having 15 to 90 volume percent gas bubbles, and wherein the method comprises:
passing a first slurry comprising water, 50 to 98 wt. % calcium sulfate hemihydrate on a dry basis, 1 to 50 wt. % calcium carbonate on a dry basis, and 0.1 to 10 wt. % cellulose thickener on a dry basis via a first hose to a Wye connector conduit at Rate C, wherein the first slurry has a residence time in the first hose of Time 2;
passing an alum solution comprising an aluminum compound via a second hose to the Wye connector conduit at Rate D;
passing the first slurry and the alum solution through respective inlet openings of the Wye connector conduit to combine in the Wye connector conduit to create a combined mixed stream that discharges from the Wye connector conduit through a discharge opening;
mixing the combined mixed stream in a static mixer for Time 3 to activate at least a portion of the calcium carbonate by reacting the portion of the calcium carbonate with the aluminum compound to generate CO2 and create the foamed gypsum slurry;
transferring the foamed gypsum slurry from the static mixer to a cavity between two wall boards via a third hose, wherein the residence time in the third hose is Time 4; and
allowing the foamed gypsum slurry in the cavity to expand, harden and dry.

### Claim 2 (depends on 1)

The method of claim 1 further comprising:
adding a mixture comprising the calcium sulfate hemihydrate, the calcium carbonate, and the cellulose thickener to a mixing chamber at Rate A;
adding water to the mixing chamber at Rate B; and
mixing the mixture with water in the mixing chamber for Time 1 to form the first slurry.

### Claim 3 (depends on 2)

The method of claim 2, wherein the mixture further comprises an accelerant, a retarder, and/or a chelating agent.

### Claim 4 (depends on 2)

The method of claim 2, wherein Rate A is about 15 to about 60 lbs/min, Rate B is about 10 to about 40 lbs/min, Rate C is about 2 to about 10 gpm, Rate D is about 2 to about 15 lbs/min, Time 1 is about 20 to about 75 sec, Time 2 is about 22 to about 100 sec, Time 3 is about 0.005 to about 0.040 sec, and Time 4 is about 3 to about 15.

### Claim 5 (depends on 2)

The method of claim 2, wherein Rate A is about 15 to about 25 lbs/min, Rate B is about 10 to about 20 lbs/min, Rate C is about 2 to about 4 gpm, Rate D is about 2 to about 5 lbs/min, Time 1 is about 45 to about 75 sec, Time 2 is about 50 to about 100 sec, Time 3 is about 0.020 to about 0.040 sec, and Time 4 is about 5 to about 15.

### Claim 6 (depends on 2)

The method of claim 2, wherein Rate A is about 35 to about 60 lbs/min, Rate B is about 25 to about 40 lbs/min, Rate C is about 5 to about 10 gpm, Rate D is about 5 to about 15 lbs/min, Time 1 is about 20 to about 35 sec, Time 2 is about 22 to about 38 sec, Time 3 is about 0.005 to about 0.025 sec, and Time 4 is about 3 to about 10.

### Claim 7 (depends on 2)

The method of claim 2, wherein the water to calcium sulfate hemihydrate weight ratio is 0.2-2:1 in addition to water of any optionally added latex aqueous medium

### Claim 8 (depends on 2)

The method of claim 2, wherein the mixture further comprises, based on 100 parts by weight of said ingredients of said mixture, at least one of:
0.1 to 1 wt. % chelating agent; and
0.05 to 1 wt. % biocide.

### Claim 9 (depends on 2)

The method of claim 2, wherein the mixture further comprise, based on 100 parts by weight of said ingredients of said mixture, at least one additive selected from the group consisting of:
0.1 to 10 wt. % acrylate thickener selected from at least one member of the group consisting of sodium polyacrylates and water-soluble copolymers based on acrylic and (meth)acrylic acid;
0.1 to 10 wt. % casein, gum arabic, guar gum, tragacanth gum, starch, sodium alginate;
0.02 to 1 wt. % citric acid, tartaric acid, malic acid, acetic acid, boric acid;
0.02 to 2 wt. % alkali metal salt of citric acid;
0.02 to 2 wt. % accelerator, the accelerator selected from the group consisting of potassium sulfate, an organic phosphonic compound, a phosphate-containing compound, and a calcium sulfate dihydrate and sugar-containing composition;
0.1 to 5 wt. % foaming agent;
1 to 20 wt. % latex polymer;
0.01 to 1 wt. % 2-amino-2-methyl-1-propanol;
0.05 to 2 wt. % polycarboxylate ether dispersant;
0.05 to 2 wt. % polyphosphate;
0.01 to 2 wt. % naphthalene dispersant or lignosulfonate dispersant;
0.05 to 1 wt. % biocide;
0.01 to 0.5 wt. % silicon based defoamer;
1 to 5 wt. % inorganic particles selected from clay, pigment particles, and combinations thereof;
0.05 to 1% polyethylene oxide (PEO).

### Claim 10 (depends on 1)

The method of claim 1, wherein the cellulose thickener is selected from at least one member of the group consisting of hydroxy propyl methyl cellulose, hydroxy ethyl methyl cellulose, hydroxy ethyl cellulose, methyl cellulose, methyl ethyl cellulose, ethyl cellulose, and carboxy methyl cellulose.

### Claim 11 (depends on 2)

The method of claim 2, wherein the ingredients comprise, based on 100 parts by weight of said ingredients:
50 to 98 wt. % calcium sulfate hemihydrate;
1.5 to 50 wt. % calcium carbonate;
1.5 to 30 wt. % aluminum sulfate;
0 to 2 wt. % sodium citrate;
0 to 2 wt. % the accelerator comprising calcium sulfate dihydrate and sugar;
0.2 to 3 wt. %, cellulose thickener comprising hydroxy methyl propyl cellulose;
0-3 wt. % said foaming agent, wherein said foaming agent is selected from the group consisting of alkyl benzene sulfonate, fatty acid salts, sodium lauryl sulfate, alkyl sulfate salts, sodium lauryl ether sulfate, sodium alkyl ether sulfate, (sodium C14-16 olefin sulfonate, alpha-olefin sulfonates, phosphate esters, sulphosuccinates, alkyl phenol ether sulfates, and isethionates;
0 to 20 wt. % latex comprising surfactant and latex polymer dispersed as solids in aqueous medium, said latex polymer is selected from at least one member of the group consisting of acrylic polymer and styrene butadiene polymer;
0 to 1 wt. % 2-amino-2-methyl-1-propanol;
0 to 1 wt. % modifier comprising calcium hydroxide;
0.1 to 2 wt. % dispersant selected from at least one member of the group consisting of polycarboxylate dispersant, polyphosphate dispersant, and naphthalene dispersant,
wherein the polycarboxylate dispersant comprises a polycarboxylic ether dispersant,
wherein the naphthalene dispersant is selected from at least one of beta-naphthalene sulfonate, naphthalene sulfonate formaldehyde condensate and sodium naphthalene sulfate formaldehyde condensate,
wherein the polyphosphate dispersant is selected from at least one of the group sodium trimetaphosphate (STMP), sodium tripolyphosphate (STPP), potassium tripolyphosphate (KTPP), tetrasodium pyrophosphate (TSPP), tetrapotassium pyrophosphate, and tetrapotassium pyrophosphate (TKPP);
0 to 2 wt. % acrylate thickener selected from at least one member of the group consisting of sodium polyacrylate, acrylic acid/acrylamide and (meth)acrylic acid/acrylic ester copolymers;
0 to 1 wt. % chelating agent selected from
Diethylenetriaminepentaacetic acid (DTPA)
Ethylenediaminetetraacetic acid (EDTA)
Sodium polyacrylate
Polyphosphate, wherein if the polyphosphate is also present as a dispersant the polyphosphate present as a chelating agent is in addition to the polyphosphate present as a dispersant;
0 to 0.5 wt. % silicon based defoamer;
0 to 5 wt. % inorganic particles selected from clay, pigment particles, and combinations thereof;
0-10% wt. % of lightweight aggregate.

### Claim 12 (depends on 1)

The method of claim 1, wherein the aluminum compound is selected from aluminum sulfate and potassium aluminum sulfate.

### Claim 13 (depends on 1)

The method of claim 1, wherein the aluminum compound comprises particles of powder encapsulated in a shell for a controlled release of the powder when adequate shear force is applied to the particles of powder encapsulated particles in the shell in the slurry during the mixing process.

### Claim 14 (depends on 1)

The method of claim 1, wherein the aluminum compound comprises particles coated with a water soluble coating.

### Claim 15 (depends on 2)

The method of claim 2, wherein the mixture further comprise lightweight aggregate selected from at least one of perlite and polystyrene.

### Claim 16 (depends on 1)

The method of claim 1, wherein the foamed gypsum slurry has a density of about 10 pcf to about 80 pcf.

### Claim 17

A method comprising:
filling a cavity with a first foamed gypsum slurry to a first fill vertical distance within the cavity of about 6 inches to about 10 feet, wherein the first foamed gypsum slurry is produced by the method of any one of the preceding claims;
allowing the first foamed gypsum slurry in the cavity to expand and gain significant green strength harden to create a green foamed gypsum product;
making a second foamed gypsum slurry according to the method of any one of the preceding claims;
filling the cavity with the second foamed gypsum slurry on top of the green foamed gypsum product to a second fill vertical distance within the cavity of about 6 inches to about 10 feet; and
allowing the second foamed gypsum slurry in the cavity to expand, harden and dry.

### Claim 18

A method comprising:
filling a cavity with a first foamed gypsum slurry to a first fill vertical distance within the cavity of about 6 inches to about 10 feet;
allowing the first foamed gypsum slurry in the cavity to expand and gain significant green strength harden to create a green foamed gypsum product;
making a second foamed gypsum slurry;
filling the cavity with the second foamed gypsum slurry on top of the green foamed gypsum product to a second fill vertical distance within the cavity of about 6 inches to about 10 feet;
wherein the first and second foamed gypsum slurries independently comprising water, 50 to 98 wt. % calcium sulfate hemihydrate on a dry basis, 1 to 50 wt. % calcium carbonate on a dry basis, and 0.1 to 10 wt. % cellulose thickener on a dry basis and have 15 to 90 volume percent gas bubbles; and
allowing the second foamed gypsum slurry in the cavity to expand, harden and dry.

### Claim 19 (depends on 18)

The method of claim 18, wherein the cavity comprises a wall at least partially formed by wallboard.

### Claim 20 (depends on 19)