# US 2019/0315645 A1 · Sludge composite conditioner based on iron-containing sludge pyrolysis residue as well as preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0315645 A1
- Document ID: US20190315645A1
- Status: Published application
- Kind: A1
- Application number: 16/446,037
- Filed: 2019-06-19
- Published: 2019-10-17
- Earliest claimed: 2017-09-18
- Assignees: Huazhong University of Science and Technology
- Applicants: Huazhong University of Science and Technology
- Inventors: Jiakuan YANG; Shuangyi TAO; Sha LIANG; Keke XIAO; Wenbo YU; Jingjing QIU; Quan GAN; Ruonan GUAN; Huijie HOU; Bingchuan LIU; Jingping HU
- Web page: https://patentgrep.com/patent/US20190315645A1

## CPC

- C02F 11/143: using inorganic substances (C02F11/148 takes precedence)
- C02F 11/06: by oxidation (incinerators for burning waste liquors, e.g. sulfite liquor from paper-making plant F23G7/04)
- C02F 11/10: by pyrolysis
- C02F 2209/02: Temperature
- C02F 2209/06: pH
- C02F 2209/38: Gas flow rate
- C02F 2305/023: Reactive oxygen species, singlet oxygen, OH radical
- C02F 2305/026: Fenton's reagent
- Y02W 10/40: Valorisation of by-products of wastewater, sewage or sludge processing
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present disclosure discloses a sludge composite conditioner based on iron-containing sludge pyrolysis residue as well as a preparation method and use thereof. The sludge composite conditioner comprises iron-containing sludge pyrolysis residue and an oxidant used in combination with the iron-containing sludge pyrolysis residue, in which the iron-containing sludge pyrolysis residue is pyrolysis residue obtained by dewatering iron-containing sludge to obtain an iron-containing sludge cake and then pyrolyzing the iron-containing sludge cake, the iron-containing sludge being obtained from an advanced oxidation technology involving an iron-containing reagent. In the present disclosure, through improvements of the subsequent overall treatment process, the reuse mode and specific reaction condition parameters of the respective subsequent treatment process steps of the iron-containing sludge cake, the problem of sludge cake treatment and disposal at the end of the existing sludge treatment and disposal technology can be effectively solved compared with the prior art, and then the iron-containing sludge cake is utilized to form a composite conditioner for deep dewatering of sludge, which is recycled as a sludge conditioner for sludge treatment, thereby realizing the full utilization of resources.

## Claims

### Claim 1

A sludge composite conditioner based on iron-containing sludge pyrolysis residue, comprising iron-containing sludge pyrolysis residue and an oxidant, wherein the iron-containing sludge pyrolysis residue is pyrolysis residue obtained by dewatering iron-containing sludge to obtain an iron-containing sludge cake and then pyrolyzing the iron-containing sludge cake, the iron-containing sludge being obtained from an advanced oxidation technology involving an iron-containing reagent.

### Claim 2 (depends on 1)

The sludge composite conditioner based on iron-containing sludge pyrolysis residue according to claim 1, wherein the iron-containing reagent is a Fenton reagent, a Fenton-like reagent or a persulfate-ferrous salt combination reagent; the iron-containing sludge cake has a moisture content of 0 to 60%, and the iron-containing sludge cake has an iron content of 8% to 30% in sludge dry mass; preferably, the iron-containing sludge is obtained by treating sludge with a Fenton compound conditioner.

### Claim 3 (depends on 1)

The sludge composite conditioner based on iron-containing sludge pyrolysis residue according to claim 1, wherein the iron-containing sludge pyrolysis residue mainly comprises zero-valent iron, divalent iron compounds, trivalent iron compounds and biochar.

### Claim 4 (depends on 1)

The sludge composite conditioner based on iron-containing sludge pyrolysis residue according to claim 1, wherein the oxidant is at least one of peroxide, persulfide and ozone; preferably, a mass ratio of the iron-containing sludge pyrolysis residue to the oxidant is (20 to 80):(3 to 10).

### Claim 5 (depends on 1)

A preparation method for the sludge composite conditioner based on iron-containing sludge pyrolysis residue according to claim 1, comprising:
(S11) treating sludge or sewage with an advanced oxidation technology involving an iron-containing reagent to obtain iron-containing sludge, and then dewatering the iron-containing sludge to obtain an iron-containing sludge cake;
(S12) subjecting the iron-containing sludge cake obtained in the step (S11) to pyrolysis treatment to obtain pyrolysis residue, i.e., iron-containing sludge pyrolysis residue; and
(S13) compounding the iron-containing sludge pyrolysis residue obtained in the step (S12) with an oxidant to obtain a sludge composite conditioner based on iron-containing sludge pyrolysis residue.

### Claim 6 (depends on 5)

The preparation method according to claim 5, wherein in the step (S12), the pyrolysis treatment is performed by pyrolyzing the iron-containing sludge cake under the atmosphere of protective gas at 600 to 1000° C. for 30 to 90 minutes; the protective gas is at least one of nitrogen gas and argon gas, and a flow rate of the protective gas is 0.1 to 0.3 L/min.

### Claim 7 (depends on 1)

Use of the sludge composite conditioner based on iron-containing sludge pyrolysis residue according to claim 1 as a sludge conditioner.

### Claim 8 (depends on 7)

The use according to claim 7, comprising:
(S21) adjusting a pH of sludge to be treated to be 1 to 6.5;
(S22) adding the iron-containing sludge pyrolysis residue to the sludge obtained in the step (S21), and then performing stirring for 2 to 8 minutes; and
(S23) adding the oxidant used in combination with the iron-containing sludge pyrolysis residue to the sludge obtained in the step (S22), and then performing stirring for 15 to 50 minutes, thereby obtaining conditioned sludge.

### Claim 9 (depends on 8)

The use according to claim 8, wherein in the step (S21), the sludge to be treated has a moisture content of 90 to 99%; in the step (S21), the pH of the sludge to be treated is adjusted by adding an acid to the sludge to be treated; the acid is at least one of hydrochloric acid, sulfuric acid, nitric acid, oxalic acid and citric acid.

### Claim 10 (depends on 8)

The use according to claim 8, wherein in the step (S22), an additive amount of the iron-containing sludge pyrolysis residue is 20 to 80% in sludge dry mass of the sludge to be treated; and in the step (S23), an additive amount of the oxidant is 3 to 10% in sludge dry basis of the sludge to be treated.