# US 2019/0315047 A1 · Biaxially oriented polypropylene film, metallized film, and capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0315047 A1
- Document ID: US20190315047A1
- Status: Published application
- Kind: A1
- Application number: 16/470,127
- Filed: 2017-12-28
- Published: 2019-10-17
- Earliest claimed: 2016-12-28
- Assignees: Oji Holdings Corporation
- Applicants: Oji Holdings Corporation
- Inventors: Takeshi TOMINAGA; Michiko SUEYOSHI; Yoshimune OKUYAMA; Yoshikazu FUJISHIRO; Masahiro NAKATA; Tadakazu ISHIWATA
- Web page: https://patentgrep.com/patent/US20190315047A1

## CPC

- B29C 55/14: successively
- C08J 7/06: with compositions not containing macromolecular substances
- B32B 15/085: comprising polyolefins
- C08J 5/18: Manufacture of films or sheets
- H01G 4/18: of synthetic material, e.g. derivatives of cellulose (H01G4/16 takes precedence)
- B32B 2457/16: Capacitors
- C08J 2323/12: Polypropene
- C08J 2423/12: Polypropene
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A biaxially oriented polypropylene film containing a polypropylene resin, the film having a thickness of 1.0 to 3.0 μm, and a molecular orientation coefficient ΔNx of 0.013 to 0.016, as calculated according to ΔNx=(ΔNxy+ΔNxz)/2 on the basis of a birefringence value ΔNxy in the slow axis direction with respect to the fast axis direction and a birefringence value ΔNxz in the slow axis direction with respect to the thickness direction, as measured via optical birefringence measurement.

## Claims

### Claim 1

A biaxially stretched polypropylene film comprising a polypropylene resin, the biaxially stretched polypropylene film having a thickness of 1.0 to 3.0 μm and having a molecular orientation coefficient ΔNx of 0.013 to 0.016, as calculated according to formula (1):
[Formula 1]
Molecular orientation coefficient ΔNx=(ΔNxy+ΔNxz)/2 (1)
on a basis of a birefringence value ΔNxy in a slow axis direction with respect to a fast axis direction and a birefringence value ΔNxz in the slow axis direction with respect to a thickness direction, as measured via optical birefringence measurement.

### Claim 2 (depends on 1)

The biaxially stretched polypropylene film according to claim 1, which is for capacitors.

### Claim 3 (depends on 1)

The biaxially stretched polypropylene film according to claim 1, wherein a ratio MTD/MMD of a tensile elastic modulus in a TD direction and a tensile elastic modulus in an MD direction is 0.85 or more and 1.8 or less.

### Claim 4 (depends on 1)

The biaxially stretched polypropylene film according to claim 1, comprising a polypropylene resin A having a difference (DM), as obtained by subtracting a differential distribution value when a logarithmic molecular weight Log(M)=6.0 from a differential distribution value when Log(M)=4.5 on a molecular weight distribution curve, of 10% or more and 18% or less based on 100% of the differential distribution value when Log(M)=6.0.

### Claim 5 (depends on 1)

The biaxially stretched polypropylene film according claim 1, comprising a polypropylene resin B having a difference (DM), as obtained by subtracting a differential distribution value when a logarithmic molecular weight Log(M)=6.0 from a differential distribution value when Log(M)=4.5 on a molecular weight distribution curve, of −1% or more and less than 10% based on 100% of the differential distribution value when Log(M)=6.0.

### Claim 6 (depends on 1)

A metallized film having a metal film on one surface or on both surfaces of the biaxially stretched polypropylene film according to claim 1.

### Claim 7 (depends on 6)

A capacitor comprising the metallized film according to claim 6.