# US 2019/0314893 A1 · Method for producing metal powder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0314893 A1
- Document ID: US20190314893A1
- Status: Published application
- Kind: A1
- Application number: 16/461,739
- Filed: 2017-11-09
- Published: 2019-10-17
- Earliest claimed: 2016-11-16
- Assignees: Shoei Chemical Inc.
- Applicants: Shoei Chemical Inc.
- Inventors: Mineto Iwasaki; Tetsuya Kimura
- Web page: https://patentgrep.com/patent/US20190314893A1

## CPC

- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- B22F 1/16: Metallic particles coated with a non-metal (coated with lubricating or binding agents or with organic material B22F1/10)
- B22F 9/026: {Spray drying of solutions or suspensions}
- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- B22F 9/30: with decomposition of metal compounds, e.g. by pyrolysis
- C23D 5/02: by wet methods
- B22F 1/065: Spherical particles
- B22F 2201/01: Reducing atmosphere
- B22F 2301/15: Nickel or cobalt
- B22F 2301/35: Iron
- B22F 2302/25: Oxide
- B22F 2302/256: Silicium oxide (SiO2)
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C23D: ENAMELLING OF, OR APPLYING A VITREOUS LAYER TO, METALS

## Abstract

A method for producing a metal powder provided on the surface thereof with a glassy thin film, wherein a glassy substance is produced in the vicinity of the surface of the metal powder by spray pyrolysis from a solution that contains a thermally decomposable metal compound and a glass precursor that produces a glassy substance that does not form a solid solution with the metal produced from the metal compound by thermal decomposition, so as to form the metal powder provided on the surface thereof with the glassy thin film. The glass precursor is prepared such that the melting temperature TmM of the metal and the liquid phase temperature TmG of the mixed oxide of the glassy substance satisfy the following formula (1): −100 [° C.]≤(TmM−TmG)≤500 [° C.] (1).

## Claims

### Claim 1

A method for producing a metal powder containing iron provided on a surface thereof with a glassy thin film, the method comprising:
converting a solution into microfine droplets, wherein the solution contains a thermally decomposable metal compound comprising an iron compound and a glass precursor that produces a glassy substance that does not form a solid solution with a metal produced from the thermally decomposable metal compound by thermal decomposition; and
heating the droplets, while the droplets are dispersed in a carrier gas, at a temperature higher than a decomposition temperature of the thermally decomposable metal compound, higher than a decomposition temperature of the glass precursor, and higher than a melting point of the metal produced from the thermally decomposable metal compound, to produce the metal powder comprising the metal and to produce a glassy substance in a vicinity of the surface of the metal powder, wherein
the glassy substance contains at least 40 mass % of SiO2 in terms of oxide, and
the glass precursor is prepared such that a melting temperature (TmM) of the metal and a liquid phase temperature (TmG) of a mixed oxide of the glassy substance satisfy the following formula (1):
−100[° C.]≤(TmM−TmG)≤500[° C.] (1).

### Claim 2 (depends on 1)

The method according to claim 1, wherein
the melting temperature TmM and the liquid phase temperature TmG satisfy the following formula (2):
−50[° C.]≤(TmM−TmG)≤300[° C.] (2).

### Claim 3 (depends on 1)

The method according to claim 1, wherein
the melting temperature TmM and the liquid phase temperature TmG are both at least 1100° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein
the solution contains 5 to 30 mass %, as the mass % with respect to the overall solution, of a reducing agent that is soluble in the solution and exhibits a reducing activity during the aforementioned heating.

### Claim 5 (depends on 4)

The method according to claim 4, wherein
the reducing agent comprises at least one selected from the group consisting of methanol, ethanol, propanol, ethylene glycol, propylene glycol, diethylene glycol, and tetraethylene glycol.

### Claim 6 (depends on 1)

The method according to claim 1, wherein
the total content in the solution of the thermally decomposable metal compound comprising the iron compound and the glass precursor is 20 to 100 g/L as a total concentration of the two components as an amount of metal components produced from the thermally decomposable metal compound by thermal decomposition and an amount of glass components in terms of oxide produced from the glass precursor by thermal decomposition.

### Claim 7

(canceled)

### Claim 8 (depends on 1)

The method according claim 1, wherein
the metal comprises nickel and iron.

### Claim 9 (depends on 8)

The method according to claim 8, wherein a mass ratio between the nickel and iron is nickel:iron=40:60 to 85:15.

### Claim 10 (depends on 1)

The method according to claim 1, wherein
an iron component originating from the iron compound is present in the glassy thin film.

### Claim 11

(canceled)

### Claim 12 (depends on 1)

The method according to claim 1, wherein
the glassy substance contains at least one selected from MgO, CaO, SrO, and BaO in terms of oxide.

### Claim 13 (depends on 1)

The method according to claim 1, wherein
1 to 20 volume % of a reducing gas is present in the carrier gas.

### Claim 14 (depends on 13)

The method according to claim 13, wherein
the reducing gas is at least one selected from hydrogen, carbon monoxide, methane, and ammonia gas.

### Claim 15 (depends on 2)

The method according to claim 2, wherein
the melting temperature TmM and the liquid phase temperature TmG are both at least 1100° C.