# US 2019/0314793 A1 · Method for manufacturing low-temperature oxidation catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0314793 A1
- Document ID: US20190314793A1
- Status: Published application
- Kind: A1
- Application number: 16/469,895
- Filed: 2017-12-21
- Published: 2019-10-17
- Earliest claimed: 2016-12-26
- Assignees: Clariant Catalysts (Japan) K.K.
- Applicants: Clariant Catalysts (Japan) K.K.
- Inventors: Yuuki Kasama; Wataru Fujii; Hyun-Joong Kim; Kazuhiro Yamada
- Web page: https://patentgrep.com/patent/US20190314793A1

## CPC

- B01J 23/58: with alkali- or alkaline earth metals
- B01J 27/138: with alkaline earth metals, magnesium, beryllium, zinc, cadmium or mercury
- B01D 53/86: Catalytic processes
- B01J 23/8906: {Iron and noble metals}
- B01J 27/13: Platinum group metals
- B01J 37/02: Impregnation, coating or precipitation ({B01J37/0009 and B01J37/0018 take precedence } ; protection by coating B01J33/00)
- B01J 37/0219: {the coating containing organic compounds}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/18: with gases containing free hydrogen
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

A method for manufacturing a catalyst that oxidatively decomposes ethylene, carbon monoxide, formaldehyde, etc., at high efficiency even at low temperatures, wherein discharge of harmful gases such as halogens during the manufacture is reduced. Further, a method for manufacturing a low-temperature oxidation catalyst including: (1) a step for causing a non-halogen-containing noble metal compound to be supported on a carrier; (2) a step for reducing the noble metal compound on the carrier obtained in step (1); (3) a step for causing a halide to be supported on the carrier obtained in step (2); and (4) a step for drying the carrier obtained in step (3) and obtaining a low-temperature oxidation catalyst.

## Claims

### Claim 1

A method for producing a low temperature oxidation catalyst, comprising steps of:
(1) loading a noble metal compound not containing a halogen onto a carrier;
(2) reducing the noble metal compound on the carrier obtained in step (1);
(3) loading a halide onto the carrier obtained in step (2); and
(4) drying the carrier obtained in step (3) to obtain the low temperature oxidation catalyst.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in step (1), the noble metal compound not containing halogen is loaded onto the carrier by impregnating the carrier with a solution of the noble metal compound not containing halogen and then drying the resulting carrier.

### Claim 3 (depends on 1)

The method according to claim 1, wherein, in step (3), the halide is loaded onto the carrier obtained in step (2), by treating said carrier with a solution of the halide.

### Claim 4 (depends on 3)

The method according to claim 3, wherein, in step (3), the halide is loaded onto the carrier obtained in step (2), by spray-coating said carrier with the solution of the halide.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the noble metal is at least one element selected from the group consisting of platinum, gold, palladium, ruthenium, rhodium and iridium.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the noble metal compound not containing halogen in step (1) comprises dinitrodiammine platinum.

### Claim 7 (depends on 1)

The method according to claim 1, wherein a halogen in the halide comprises chlorine.

### Claim 8 (depends on 3)

The method according to claim 3, wherein the solution of the halide comprises an aqueous solution of hydrogen chloride.

### Claim 9 (depends on 3)

The method according to claim 3, wherein the solution of the halide comprises a solution of a chloride of a metal other than noble metals.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the metal chloride is one or more metal chlorides selected from the group consisting of alkali metal chlorides, alkaline earth metal chlorides, transition metal chlorides and chlorides of Group XIII elements except boron.

### Claim 11 (depends on 10)

The method according to claim 10, wherein a metal in the metal chloride is one or more elements selected from the group consisting of calcium, magnesium, iron and aluminum.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising, between steps (1) and (2), a step of:
(1-a) heating the carrier comprising the noble metal compound not containing halogen supported on said carrier.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the reduction in step (2) is a hydrogen reduction.

### Claim 14 (depends on 1)

The method according to claim 1, wherein, the carrier comprises a silica-containing carrier, wherein the silica content of which is 70% by weight or more based on the total weight of the carrier.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the carrier has a specific surface area of 300 m2/g to 2000 m2/g.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the carrier comprises a silica produced by a sol-gel method.

### Claim 17 (depends on 14)

The method according to claim 14, wherein the carrier comprises silica gel or mesoporous silica.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the loading amount of the noble metal compound is 0.1 to 5% by weight based on the content a noble metal element, relative to the total weight of the carrier and the noble metal compound.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the loading amount of the halide is 0.02% by weight or more based on the content a halogen element in the halide, relative to the total weight of the carrier and the noble metal compound.

### Claim 20 (depends on 2)

The method according to claim 2, wherein, in step (1), 0.1 to 5% by weight of the noble metal compound based on the content of a noble metal element in the noble metal compound, relative to the total weight of the carrier and the noble metal compound, is loaded onto the carrier by impregnating the carrier with a solution containing the noble metal compound at a concentration of 0.05 to 10% by weight based on the content of the noble metal element.

### Claim 21 (depends on 3)

The method according to claim 3, wherein, in step (3), 0.02% by weight or more of halogen based on the content of a halogen element in the halide, relative to the total weight of the carrier and the noble metal compound, is loaded onto the carrier obtained in step (2) by spray-coating said carrier with a solution containing the halide at a concentration of 0.1 to 5% by weight based on the content of the halogen element.