# US 2019/0314787 A1 · Methods of Preparing a Catalyst with Low HRVOC Emissions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0314787 A1
- Document ID: US20190314787A1
- Status: Published application
- Kind: A1
- Application number: 15/953,927
- Filed: 2018-04-16
- Published: 2019-10-17
- Earliest claimed: 2018-04-16
- Assignees: Chevron Phillips Chemical Company LP
- Applicants: Chevron Phillips Chemical Company LP
- Inventors: Max P. McDaniel; Kathy S. Clear; Eric D. Schwerdtfeger; Jeremy M. Praetorius
- Web page: https://patentgrep.com/patent/US20190314787A1

## CPC

- B01J 21/08: Silica
- C08F 110/02: Ethene
- B01J 23/26: Chromium
- B01J 37/0217: {Pretreatment of the substrate before coating}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/024: {Multiple impregnation or coating}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C08F 2410/01: Additive used together with the catalyst, excluding compounds containing Al or B
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A method of preparing a catalyst comprising a) drying a chrominated-silica support followed by contacting with a titanium(IV) alkoxide to form a metalized support, b) drying a metalized support followed by contacting with an aqueous alkaline solution comprising from about 3 wt. % to about 20 wt. % of a nitrogen-containing compound to form a hydrolyzed metalized support, and c) drying the hydrolyzed metalized support followed by calcination at a temperature in a range of from about 400° C. to about 1000° C. and maintaining the temperature in the range of from about 400° C. to about 1000° C. for a time period of from about 1 minute to about 24 hours to form the catalyst.

## Claims

### Claim 1

A method of preparing a hydrolyzed pre-catalyst comprising:
a) drying a silica support by heating the silica support to a temperature in a range of from about 150° C. to about 250° C. and maintaining the temperature of the silica support in the range of from about 150° C. to about 250° C. for a time period of from about 1 hour to about 24 hours to form a dried support;
b) contacting the dried support and a titanium(IV) alkoxide to form a titanated support;
c) drying the titanated support by heating the titanated support to a temperature in a range of from about 50° C. to about 200° C. and maintaining the temperature of the titanated support in the range of from about 50° C. to about 200° C. for a time period of from about 30 minutes to about 6 hours to form a dried titanated support;
d) contacting the dried titanated support and an aqueous alkaline solution comprising from about 3 wt. % to about 20 wt. % of a nitrogen-containing compound for a time period of from about 10 minutes to about 6 hours to form a mixture comprising a hydrolyzed titanated support wherein a weight ratio of the amount of aqueous alkaline solution to the amount of titanium(IV) alkoxide in the dried titanated support is from about 30:1 to about 3:1; and
e) removing the hydrolyzed titanated support from the mixture comprising the hydrolyzed titanated support and drying the hydrolyzed titanated support by heating the hydrolyzed titanated support to a temperature in a range of from about 50° C. to about 200° C. and maintaining the temperature of the hydrolyzed titanated support in the range of from about 50° C. to about 200° C. for a time period of from about 30 minutes to about 6 hours to form the hydrolyzed pre-catalyst.

### Claim 2 (depends on 1)

The method of claim 1 further comprising: contacting, to form a pre-catalyst, a chromium-containing compound and at least one material selected from the group consisting of the silica support, the dried support, the titanated support, the dried titanated support, the mixture comprising the hydrolyzed titanated support, and the hydrolyzed pre-catalyst; and
calcining the pre-catalyst by heating the pre-catalyst to a temperature in a range of from about 400° C. to about 1000° C. and maintaining the temperature of the pre-catalyst in the range of from about 400° C. to about 1000° C. for a time period of from about 1 minute to about 24 hours to form a catalyst.

### Claim 3 (depends on 2)

The method of claim 2 wherein an amount of highly reactive volatile organic compounds (HRVOC) emitted during calcining the pre-catalyst is reduced by from about 80% to about 95%, as determined by combustion analysis in accordance with EPA Method 18-type/ASTM D1946, when compared to the amount of HRVOC emitted during calcining an otherwise similar pre-catalyst prepared in the absence of an aqueous alkaline solution.

### Claim 4 (depends on 2)

The method of claim 2 wherein an amount of HRVOC emitted during calcining the pre-catalyst is less than about 1 wt. % as determined by combustion analysis in accordance with EPA Method 18-type/ASTM D1946.

### Claim 5 (depends on 1)

The method of claim 1 wherein the nitrogen-containing compound comprises an amide, an amidine, an amine, a diamine, a triamine, an amino acid, an ammonium hydroxide, a formamide, a hydrazine, a hydroxylamine, an imidazole, a piperazine, a piperidine, a pyrazine, a pyrazole, a pyridine, a pyrimidine, a pyrrole, a urea, or a combination thereof.

### Claim 6 (depends on 1)

The method of claim 1 wherein the nitrogen-containing compound comprises ammonia, ammonium hydroxide, tetraethylammonium hydroxide, tetramethylammonium hydroxide, hydrazine, hydroxylamine, triethyl amine, trimethyl amine, acetamide, creatine, 1,4-diazabicyclo[2.2.2]octane (DABCO), 1,5-diazabicyclo[4.3.0]non-5-ene (DBN), 1,8-diazabicyclo[5.4.0]undec-7-ene (DBU), N,N-diisopropylethylamine (DIPEA), dimethyl carbamate, formamide, methyl formamide, dimethyl formamide, dimethyl glycine, 1,4-dimethylpiperazine (DMP), 1,3-dimethyl urea, imidazole, piperazine, piperidine, pyrazine, pyrazole, pyridine, pyrimidine, pyrrole, tetramethylethylenediamine (TMEDA), triazine, 1,3,5-triazacyclohexane, 1,3,5-trimethyl-1,3,5-triazacyclohexane (TMTAC), or a combination thereof.

### Claim 7 (depends on 1)

The method of claim 1 wherein the titanium(IV) alkoxide comprises titanium(IV) ethoxide, titanium(IV) isopropoxide, titanium(IV) n-propoxide, titanium(IV) n-butoxide, titanium(IV) isobutoxide, or a combination thereof.

### Claim 8 (depends on 1)

The method of claim 1 wherein the silica support is characterized by a surface area of from about 100 m2/gram to about 1000 m2/gram and a pore volume of from about 1.0 cm3/gram to about 2.5 cm3/gram.

### Claim 9 (depends on 2)

The method of claim 2 wherein the chromium-containing compound comprises chromium trioxide, chromium acetate, chromium nitrate, tertiary butyl chromate, biscyclopentadienyl chromium(II), chromium(III) acetylacetonate, or a combination thereof.

### Claim 10 (depends on 2)

The method of claim 2 wherein an amount of titanium present in the catalyst ranges from about 0.01% to about 10% by total weight of the catalyst.

### Claim 11 (depends on 2)

The method of claim 2 wherein an amount of chromium present in the catalyst ranges from about 0.01% to about 10% by total weight of the catalyst.

### Claim 12 (depends on 2)

A method of forming an ethylene polymer comprising contacting the catalyst prepared by the method of claim 2 with an ethylene monomer under conditions suitable for formation of the ethylene polymer and recovering the ethylene polymer.

### Claim 13 (depends on 12)

The method of claim 12 wherein the ethylene polymer has a high load melt index (HLMI) that is from about 10% to about 100% greater than the HLMI of an ethylene polymer produced by utilizing an otherwise similar catalyst produced in the absence of an aqueous alkaline solution.

### Claim 14

A method of preparing a hydrolyzed pre-catalyst comprising:
a) drying a silica support by heating the silica support to a temperature in a range of from about 150° C. to about 250° C. and maintaining the temperature of the silica support in the range of from about 150° C. to about 250° C. for a time period of from about 1 hour to about 24 hours to form a dried support;
b) contacting the dried support and a titanium(IV) alkoxide to form a titanated support;
c) heating the titanated support to a temperature in a range of from about 50° C. to about 200° C. and maintaining the temperature in the range of from about 50° C. to about 200° C. while contacting the titanated support and an alkaline material for a time period of from about 2 hours to about 48 hours;
d) ceasing contacting of the titanated support and the alkaline material to provide a hydrolyzed support having a temperature in a range of from about 50° C. to about 200° C.; and
e) maintaining the temperature of the hydrolyzed support in the range of from about 50° C. to about 200° C. for a time period of from about 30 minutes to about 6 hours to form the hydrolyzed pre-catalyst.

### Claim 15 (depends on 14)

The method of claim 14 further comprising contacting, to form a pre-catalyst, a chromium-containing compound and at least one material selected from the group consisting of the silica support, the dried support, the titanated support, the hydrolyzed support, and the hydrolyzed pre-catalyst; and
calcining the pre-catalyst by heating the pre-catalyst to a temperature in a range of from about 400° C. to about 1000° C. and maintaining the temperature of the pre-catalyst in the range of from about 400° C. to about 1000° C. for a time period of from about 1 minute to about 24 hours to form a catalyst.

### Claim 16 (depends on 15)

The method of claim 15 wherein an amount HRVOC emitted during calcining the pre-catalyst is reduced by from about 80% to about 95%, as determined by combustion analysis in accordance with EPA Method 18-type/ASTM D1946, when compared to the amount of HRVOC emitted during calcining an otherwise similar pre-catalyst prepared in the absence of an alkaline material.

### Claim 17 (depends on 15)

The method of claim 15 wherein an amount HRVOC emitted during calcining the pre-catalyst is less than about 1 wt. % as determined by combustion analysis in accordance with EPA Method 18-type/ASTM D1946.

### Claim 18 (depends on 14)

The method of claim 14 wherein the alkaline material comprises a vapor associated with a basic liquid wherein the basic liquid comprises an aqueous solution of a nitrogen-containing compound and optionally an alcohol wherein an amount of nitrogen-containing compound in the aqueous solution is from about 3 wt. % to about 20 wt. % wherein a volumetric ratio of the aqueous solution to the alcohol is from about 7:3 to about 3:7 and wherein the alcohol is methanol, ethanol, n-propanol, isopropanol, or a combination thereof.

### Claim 19 (depends on 14)

The method of claim 14 wherein the alkaline material is an aqueous alkaline solution comprising a nitrogen-containing compound in an amount from about 3 wt. % to about 20 wt. % wherein a weight ratio of the amount of aqueous alkaline solution to the amount of titanium(IV) alkoxide in the titanated support is from about 30:1 to about 3:1.

### Claim 20 (depends on 14)

The method of claim 14 wherein the alkaline material comprises an amide, an amidine, an amine, a diamine, a triamine, an amino acid, an ammonium hydroxide, a formamide, a hydrazine, a hydroxylamine, an imidazole, a piperazine, a piperidine, a pyrazine, a pyrazole, a pyridine, a pyrimidine, a pyrrole, a urea, or a combination thereof.

### Claim 21 (depends on 14)

The method of claim 14 wherein the titanium(IV) alkoxide comprises titanium(IV) ethoxide, titanium(IV) isopropoxide, titanium(IV) n-propoxide, titanium(IV) n-butoxide, titanium(IV) isobutoxide, or a combination thereof.

### Claim 22

A method of preparing a catalyst comprising:
a) drying a silica support by heating the silica support to a temperature in a range of from about 150° C. to about 250° C. and maintaining the temperature of the silica support in the range of from about 150° C. to about 250° C. for a time period of from about 1 hour to about 24 hours to form a dried support;
b) contacting the dried support and a titanium(IV) alkoxide to form a titanated support;
c) drying the titanated support by heating the titanated support to a temperature in a range of from about 50° C. to about 200° C. and maintaining the temperature of the titanated support in the range of from about 50° C. to about 200° C. for a time period of from about 30 minutes to about 6 hours to form a dried titanated support;
d) contacting the dried titanated support and an aqueous alkaline solution comprising from about 3 wt. % to about 20 wt. % of a nitrogen-containing compound for a time period of from about 10 minutes to about 6 hours to form a mixture comprising a hydrolyzed titanated support wherein a weight ratio of the amount of aqueous alkaline solution to the amount of titanium(IV) alkoxide in the dried titanated support is from about 30:1 to about 3:1;
e) removing the hydrolyzed titanated support from the mixture comprising the hydrolyzed titanated support and drying the hydrolyzed titanated support by heating the hydrolyzed titanated support to a temperature in a range of from about 50° C. to about 200° C. and maintaining the temperature of the hydrolyzed titanated support in the range of from about 50° C. to about 200° C. for a time period of from about 30 minutes to about 6 hours to form a hydrolyzed pre-catalyst;
f) contacting, to form a pre-catalyst, a chromium-containing compound and at least one material selected from the group consisting of the silica support, the dried support, the titanated support, the dried titanated support, the mixture comprising the hydrolyzed titanated support, and the hydrolyzed pre-catalyst; and
g) calcining the pre-catalyst by heating the pre-catalyst to a temperature in a range of from about 400° C. to about 1000° C. and maintaining the temperature of the pre-catalyst in the range of from about 400° C. to about 1000° C. for a time period of from about 1 minute to about 24 hours to form the catalyst.