# US 2019/0314784 A1 · Method for producing an adsorbent material and method for extracting lithium from saline solutions using the material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0314784 A1
- Document ID: US20190314784A1
- Status: Published application
- Kind: A1
- Application number: 16/314,107
- Filed: 2017-06-30
- Published: 2019-10-17
- Earliest claimed: 2016-06-30
- Assignees: Eramet; Ifp Energies Nouvelles
- Applicants: Eramet; Ifp Energies Nouvelles
- Inventors: Vincent LECOCQ; Fabien André Pierre BURDET; Yohan Florent OUDART; Guillaume Patrick André MAILLET
- Web page: https://patentgrep.com/patent/US20190314784A1

## CPC

- B01J 20/041: {Oxides or hydroxides}
- B01J 20/08: comprising aluminium oxide or hydroxide; comprising bauxite
- B01J 20/3007: {Moulding, shaping or extruding}
- B01J 20/3014: {Kneading}
- B01J 20/3042: {Use of binding agents; addition of materials ameliorating the mechanical properties of the produced sorbent}
- B01J 20/305: {Addition of material, later completely removed, e.g. as result of heat treatment, leaching or washing, e.g. for forming pores}
- B01J 20/3071: {Washing or leaching}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3085: {Chemical treatments not covered by groups B01J20/3007 - B01J20/3078}
- B01J 39/10: Oxides or hydroxides
- C01D 15/00: Lithium compounds
- C01F 7/141: from aqueous aluminate solutions by neutralisation with an acidic agent
- C01F 7/34: Preparation of aluminium hydroxide by precipitation from solutions containing aluminium salts
- C01F 7/78: Compounds containing aluminium, with or without oxygen or hydrogen, and containing two or more other elements (aluminates C01F7/02; compounds containing aluminium, fluorine and alkali or alkaline earth metals C01F7/54; nitrates containing other cations besides aluminium C01F7/66; sulfides, sulfites or sulfates containing other cations besides aluminium C01F7/70 - C01F7/74)
- C22B 26/12: Obtaining lithium
- C01P 2002/60: Compounds characterised by their crystallite size
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/60: Particles characterised by their size
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- Y02E 60/10: Energy storage using batteries
- Y02P 10/20: Recycling
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to the field of solid materials for the adsorption of lithium. In particular, the present invention relates to a new method for the preparation of a crystallized and shaped solid material, preferably in extruded form, of the formula (LiCl)x.2Al(OH)3,nH2O, wherein n is between 0.01 and 10, x is between 0.4 and 1, wherein it comprises a step a) of precipitation of boehmite under specific temperature and pH conditions, a step of bringing into contact the precipitate obtained with LiCl, at least one acid extrusion-kneading shaping step, wherein the method also comprises a final hydrothermal treatment step, all of which makes it possible to increase the lithium adsorption capacity, the adsorption kinetics, as well as the lithium/boron selectivity of the materials obtained with respect to the materials of the prior art, when it is used in a lithium extraction method of saline solutions.

## Claims

### Claim 1

Method for preparing a crystalline solid material of formula (LiCl)x.2Al(OH)3,nH2O, wherein n is between 0.01 and 10, x is between 0.4 and 1, and wherein the method comprises at least the following steps:
a) precipitating boehmite, in an aqueous medium, comprising bringing into contact at least one basic precursor and at least one acidic precursor, wherein at least one of the basic or acidic precursors comprises aluminum, in order to obtain a boehmite suspension, wherein step a) is carried out at a temperature of between 5 and 35° C., and the amount of the basic precursor is chosen in order to obtain a pH of the end of precipitation in the reaction medium of between 7.5 and 9.5,
b) bringing into contact the precipitate obtained in step a) with at least lithium chloride (LiCl) as lithium source,
c) filtering the suspension obtained in step b) to obtain a paste,
d) a drying the paste obtained at the end of step c) at a temperature between 20 and 80° C.,
e) shaping the paste dried by acid extrusion-kneading, wherein the dried paste resulting from step d) is kneaded in the presence of an amount of acid of between 0.05 and 5% by weight relative to the dry material, wherein the dry material is the weight of the paste resulting from step d) dried in an autoclave at 200° C., wherein the acid is an organic or inorganic acid, and wherein the paste is then subjected to in an extrusion step, the step e) of shaping by acid extrusion-kneading that is carried out in the absence of a binder or in the presence of a binder except for a binder chosen from solid precursors of alumina chosen from among aluminum oxides, aluminum hydroxides and aluminum oxyhydroxides which are soluble or dispersible in a solution of phosphoric acid,
f) drying the shaped material obtained at the end of step e) at a temperature between 20 and 200° C.

### Claim 2 (depends on 1)

Method according to claim 1, wherein the basic precursor is sodium hydroxide (NaOH).

### Claim 3 (depends on 1)

Method according to claim 1, wherein the amount of the basic precursor is chosen in order to obtain an end of precipitation pH of step a) in the reaction medium of between 7.7 and 8.8.

### Claim 4 (depends on 1)

Method according to claim 1, wherein the step b) is carried out in the presence of a quantity of lithium chloride equivalent to a molar ratio Li/Al between 0.3 and 4.

### Claim 5 (depends on 1)

Method according to claim 1, wherein the organic acid used in step e) is a carboxylic acid or derivative thereof selected from the group consisting of carboxylic acid salts, alkaline salts and earth salts, alkali metal salts, ammonium salts, and acid anhydrides, while the inorganic acid used in step e) is selected from the group consisting of nitric acid, phosphoric acid, sulfuric acid and hydrochloric acid alone and any mixtures thereof.

### Claim 6 (depends on 5)

Method according to claim 5 wherein the acid is an organic acid selected from the group consisting of oxalic acid, malonic acid, succinic acid, glutaric acid, adipic acid, alone and any mixtures thereof.

### Claim 7 (depends on 6)

Method according to claim 6, wherein the shaping step e) is carried out in the presence of oxalic acid.

### Claim 8 (depends on 7)

Method according to claim 7, wherein the dried paste is kneaded in the presence of an amount of acid of between 0.1 and 2.5% by weight relative to the dry material, wherein the dry material is the weight of the paste from step e), dried in an autoclave at 200° C., in the shaping step e).

### Claim 9 (depends on 1)

Method according to claim 1, wherein in step e) shaping by acid extrusion-kneading is carried out in the absence of binder.

### Claim 10 (depends on 1)

Method for extracting lithium from saline solutions, wherein the method uses the solid material of formula (LiCl)x.2Al(OH)3,nH2O, wherein n is between 0.01 and 10, x is between 0.4 and 1, prepared according to the method as defined in claim 1, for the extraction of lithium from saline solutions.

### Claim 11 (depends on 10)

Extraction method according to claim 10, wherein the lithium extraction method comprises at least the following steps:
activating the solid crystallized material of formula (LiCl)x.2Al(OH)3,nH2O,
loading the activated material by adsorption, carried out by passing the saline solution on the activated material,
optionally at least one time washing the saline solution by impregnating the material by passing a washing solution on the material,
desorbing lithium by passing water or an aqueous solution of lithium salt on the material, and
obtaining an eluate comprising at least lithium.

### Claim 12 (depends on 11)

Extraction method according to claim 11, wherein the activating step is carried out by the upward or downward passage of water or a solution of lithium chloride (LiCl) having a concentration of between 0.001 mol/L and 0.1 mol/L.

### Claim 13 (depends on 11)

Extraction method according to claim 11, wherein the activating step is carried out by the upward or downward passage of water or a solution of lithium chloride (LiCl), wherein the activation step is carried out at a temperature between 0° C. and 90° C., and with a residence time of the solution of lithium chloride or water in the column between 0.03 and 10 h.

### Claim 14 (depends on 11)

Extraction method according to claim 11, wherein the loading step is carried out at a temperature between 0° C. and 90° C., and with a residence time of the salt solution in the column between 0.03 and 10 h.

### Claim 15 (depends on 11)

Extraction method according to claim 11, wherein the washing solution used in the washing step is water or an aqueous solution of sodium chloride (NaCl), optionally comprising lithium chloride (LiCl).

### Claim 16 (depends on 11)

Extraction method according to claim 11, wherein the washing step is carried out at a temperature between 0° C. and 90° C., and with a residence time of the washing solution in the column between 0.03 and 10 h.

### Claim 17 (depends on 11)

Extraction method according to claim 11, wherein the desorption step is carried out by upward or downward passage of a desorption solution chosen from water and a solution of lithium chloride (LiCl) containing from 0.001 mol/L to 2 mol/L LiCl.

### Claim 18 (depends on 11)

Extraction method according to claim 11, wherein the desorption step is carried out at a temperature between 0° C. and 90° C., and with a residence time of the desorption solution in the column between 0.03 and 10 h.

### Claim 19 (depends on 1)

Lithium extraction device characterized in that it comprises a unit comprising at least one column, wherein the column comprises at least one lining comprising the solid crystallized material prepared by the method as defined according to claim 1.

### Claim 20 (depends on 1)

Method according to claim 1, wherein the basic precursor is selected from among sodium aluminate, potassium aluminate, ammonia, hydroxide, sodium and potassium hydroxide.

### Claim 21 (depends on 1)

Method according to claim 1, wherein the acidic precursor is aluminum chloride or hydrochloric acid.