# US 2019/0314543 A1 · Degradable and absorbable hemostatic fiber material, preparation method therefor, and hemostatic fiber article thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0314543 A1
- Document ID: US20190314543A1
- Status: Published application
- Kind: A1
- Application number: 16/345,560
- Filed: 2017-11-14
- Published: 2019-10-17
- Earliest claimed: 2016-11-15
- Assignees: Medprin Regenerative Medical Technologies Co., Ltd.
- Applicants: Medprin Regenerative Medical Technologies Co., Ltd.
- Inventors: Guangyao Li; Linjing Li; Kunxue Deng; Yuyu Yuan
- Web page: https://patentgrep.com/patent/US20190314543A1

## CPC

- A61L 15/28: Polysaccharides or their derivatives {(A61L15/225 takes precedence)}
- A61L 15/64: specially adapted to be resorbable inside the body
- A61L 26/0023: {Polysaccharides}
- A61L 15/62: {Compostable,} hydrosoluble or hydrodegradable materials
- A61L 26/009: {Materials resorbable by the body}
- A61L 2400/04: Materials for stopping bleeding
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)

## Abstract

A degradable and absorbable hemostatic fiber material, a preparation method therefor, and a hemostatic fiber article thereof. The carboxylation degree of the hemostatic fiber material is 10-25%, and the polymerization degree of the hemostatic fiber material is 10-250. The hemostatic fiber material comprises fiber filaments, the linear density of the fiber filament being 0.8-4.5 dtex, and the dry strength of the fiber filament being 10-150 cN/tex. The degradable and absorbable hemostatic fiber material has a higher carboxylation degree and a lower polymerization degree, while the strength and completeness of the fiber filament can be well maintained, such that the hemostatic effect is better and the hemostasis is faster. Further, the hemostatic fiber material can be degraded and absorbed, and thus is safer.

## Claims

### Claim 1

A degradable and absorbable hemostatic fiber material, wherein the hemostatic fiber material has a degree of carboxylation of 10-25%, and a degree of polymerization of 10-250; the hemostatic fiber material comprises fiber filaments having a linear density of 0.8-4.5 dtex; and the fiber filaments have a dry strength of 10-150 cN/tex.

### Claim 2 (depends on 1)

The degradable and absorbable hemostatic fiber material of claim 1, wherein the hemostatic fiber material has a maximum water absorption that is more than 10 times of the weight of the hemostatic fiber material.

### Claim 3 (depends on 1)

A hemostatic fiber product, comprising the degradable and absorbable hemostatic fiber material of claim 1.

### Claim 4 (depends on 3)

The hemostatic fiber product of claim 3, wherein more than 50% by quantity of the fiber filaments of the hemostatic fiber material have a length greater than 10 mm.

### Claim 5 (depends on 3)

The hemostatic fiber product of claim 3, wherein the hemostatic fiber product comprises a fiber layer of the hemostatic fiber material.

### Claim 6 (depends on 5)

The hemostatic fiber product of claim 5, wherein the fabric weight ratio per fiber layer is 1×10−3-8×10−3 g/cm2.

### Claim 7 (depends on 3)

The hemostatic fiber product of claim 3, wherein the hemostatic fiber material in the hemostatic fiber product has a porosity greater than 50%.

### Claim 8 (depends on 3)

The hemostatic fiber product of claim 3, wherein the hemostatic fiber product has softness of 100-1500 mN.

### Claim 9 (depends on 1)

A preparation method for the degradable and absorbable hemostatic fiber material of claim 1, wherein the method comprises the following steps:
a step of carboxylation: performing activation processing on a fiber raw material, and then conducting a carboxylation reaction in a chloroacetic acid solution to obtain a carboxylated fiber; and
a step of oxidation: placing the carboxylated fiber in a mixed solution of TEMPO-sodium bromide-an organic solvent-water, then adding sodium hypochlorite, and conducting an oxidation reaction to obtain the hemostatic fiber material.

### Claim 10 (depends on 9)

The preparation method for the degradable and absorbable hemostatic fiber material of claim 9, wherein the chloroacetic acid solution is obtained by dissolving chloroacetic acid in a mixed solvent of water and an alcohol.

### Claim 11 (depends on 9)

The preparation method for the degradable and absorbable hemostatic fiber material of claim 9, wherein, in the step of oxidation, the volumetric ratio of water to the organic solvent in the mixed solution of TEMPO-sodium bromide-the organic solvent-water is 1:0.5-2; and the mass ratio of TEMPO to sodium bromide to the mixed solvent of water and the organic solvent is 1: 10-20:30-3000.

### Claim 12 (depends on 11)

The preparation method for the degradable and absorbable hemostatic fiber material of claim 11, wherein, in the step of oxidation, the mass ratio of TEMPO to sodium bromide to the carboxylated fiber to the sodium hypochlorite solution is 1: 10-20:30-100: 100-800.

### Claim 13 (depends on 9)

The preparation method for the degradable and absorbable hemostatic fiber material of claim 9, wherein, in the step of oxidation, the organic solvent comprises one or more of acetone, petroleum ether, dimethyl sulfoxide, dimethylformamide, and 1,4-dioxane.

### Claim 14 (depends on 9)

The preparation method for the degradable and absorbable hemostatic fiber material of claim 9, wherein the preparation method for the hemostatic fiber material further comprises a post-processing step for cleaning, centrifuging, and/or oven-drying the hemostatic fiber material.

### Claim 15 (depends on 3)

A preparation method for the hemostatic fiber product of claim 3, comprising willowing, and/or carding, and/or lapping, and/or cutting the hemostatic fiber material to obtain the hemostatic fiber product.

### Claim 16

(canceled)

### Claim 17 (depends on 1)

The degradable and absorbable hemostatic fiber material of claim 1, wherein the hemostatic fiber material has a degree of polymerization of 20-150.

### Claim 18 (depends on 1)

The degradable and absorbable hemostatic fiber material of claim 1, wherein the linear density of the fiber filaments is 1.2-3 dtex, and the dry strength of the fiber filaments is 15-120 cN/tex.

### Claim 19 (depends on 3)

The hemostatic fiber product of claim 3, wherein 60-85%, by quantity, of the fiber filaments of the hemostatic fiber material have a length greater than 10 mm.

### Claim 20 (depends on 3)

The hemostatic fiber product of claim 3, wherein the hemostatic fiber product comprises 1-15 layers of the fiber layer, and the thickness per fiber layer is 0.25-1 mm.

### Claim 21 (depends on 10)

The preparation method for the degradable and absorbable hemostatic fiber material of claim 10, wherein the alcohol comprises one or more of methanol, ethanol, propanol, or isopropanol.