# US 2019/0294090 A1 · Fixing member, fixing device, and electrophotographic image forming apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0294090 A1
- Document ID: US20190294090A1
- Status: Published application
- Kind: A1
- Application number: 16/351,994
- Filed: 2019-03-13
- Published: 2019-09-26
- Earliest claimed: 2018-03-22
- Assignees: Canon Kabushiki Kaisha
- Applicants: Canon Kabushiki Kaisha
- Inventors: Yasuharu Notoya; Yohei Miyauchi; Kimihiro Yoshimura
- Web page: https://patentgrep.com/patent/US20190294090A1

## CPC

- G03G 15/2057: {relating to the chemical composition of the heat element and layers thereof}
- G03G 15/206: {Structural details or chemical composition of the pressure elements and layers thereof}
- G03G 2215/2048: Surface layer material
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

Provided is a fixing member in which hot offset of a toner is difficult to be generated. The fixing member has a substrate and a release layer as a surface layer, wherein the release layer includes PFPE and a second fluororesin, the second fluororesin being at least one selected from PFA and FEP, and in a 19F-NMR spectrum of the release layer measured at a temperature of 200° C., a relaxation time T1 of longitudinal relaxation of a peak derived from PFPE is 0.5 seconds or more and 3.5 seconds or less.

## Claims

### Claim 1

A fixing member for electrophotography, comprising:
a substrate; and
a release layer as a surface layer,
wherein the release layer includes:
a first fluororesin and a second fluororesin,
the first fluororesin being perfluoropolyether (PFPE),
the second fluororesin being at least one selected from a tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer (PFA) and a tetrafluoroethylene-hexafluoropropylene copolymer (FEP), and
wherein, when
a longitudinal relaxation time of PFPE in a form of a simple substance derived from a 19F-NMR measured at a temperature of 200° C. is defined as T1−1, and a longitudinal relaxation time of PFPE contained in the release layer derived from a 19F-NMR of the release layer measured at a temperature of 200° C. is defined as T1−2,
T1−1, and T1−2 satisfy a relationship represented by Equation (1) below:
[(T1−1)−(T1−2)]/(T1−1)≥0.1. Equation (1)

### Claim 2 (depends on 1)

The fixing member according to claim 1, wherein the longitudinal relaxation time T1−2 is 0.5 seconds or more and 3.5 seconds or less.

### Claim 3 (depends on 1)

The fixing member according to claim 1, wherein the longitudinal relaxation time T1−2 is 0.5 seconds or more and 2.0 seconds or less.

### Claim 4 (depends on 1)

The fixing member according to claim 1, wherein the release layer includes the second fluororesin in a ratio of 1 mass % or more and 30 mass % or less with respect to a total amount of the first fluororesin and the second fluororesin.

### Claim 5 (depends on 1)

The fixing member according to claim 1, wherein the release layer includes the second fluororesin in a ratio of 3 mass % or more and 20 mass % or less with respect to a total amount of the first fluororesin and the second fluororesin.

### Claim 6 (depends on 1)

The fixing member according to claim 1, wherein the perfluoropolyether has at least one structure selected from structures represented by Structural Formulas (1) and (2) below:

### Claim 7 (depends on 1)

The fixing member according to claim 1, wherein the perfluoropolyether has at least one structure selected from structures represented by Structural Formulas (3) to (5) below:

### Claim 8

An electrophotographic fixing device comprising a fixing member and a heating unit of the fixing member,
wherein the fixing member is an electrophotographic fixing member including:
a substrate, and
a release layer as a surface layer,
the release layer includes
a first fluororesin and a second fluororesin,
the first fluororesin being perfluoropolyether (PFPE),
the second fluororesin being at least one selected from a tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer (PFA), and a tetrafluoroethylene-hexafluoropropylene copolymer (FEP), and
wherein, when
a longitudinal relaxation time of PFPE in a form of a simple substance derived from a 19F-NMR measured at a temperature of 200° C. is defined as T1−1, and a longitudinal relaxation time of PFPE contained in the release layer derived from a 19F-NMR of the release layer measured at a temperature of 200° C. is defined as T1−2, T1−1, and T1−2 satisfy a relationship represented by Equation (1) below:
[(T1−1)−(T1−2)]/(T1−1)≥0.1. Equation (1)

### Claim 9 (depends on 8)

The fixing device according to claim 8, wherein the fixing member is a fixing belt having an endless belt shape, and the heating unit includes a heater arranged in contact with an inner peripheral surface of the fixing belt.

### Claim 10

An electrophotographic image forming apparatus comprising a fixing device,
wherein the fixing device includes an electrophotographic fixing member,
the fixing member is an electrophotographic fixing member including:
a substrate; and
a release layer as a surface layer,
the release layer includes
a first fluororesin and a second fluororesin,
the first fluororesin being perfluoropolyether (PFPE),
the second fluororesin being at least one selected from a tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer (PFA) and a tetrafluoroethylene-hexafluoropropylene copolymer (FEP), and
wherein, when
a longitudinal relaxation time of PFPE in a form of a simple substance derived from a 19F-NMR measured at a temperature of 200° C. is defined as T1−1, and a longitudinal relaxation time of PFPE contained in the release layer derived from a 19F-NMR of the release layer measured at a temperature of 200° C. is defined as T1−2, T1−1, and T1−2 satisfy a relationship represented by Equation (1) below:
[(T1−1)−(T1−2)]/(T1−1)≥0.1. Equation (1)