# US 2019/0292654 A1 · Anti-aging periodic variable reaction black chromium coating film and forming method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0292654 A1
- Document ID: US20190292654A1
- Status: Published application
- Kind: A1
- Application number: 16/223,346
- Filed: 2018-12-18
- Published: 2019-09-26
- Earliest claimed: 2018-03-21
- Assignees: CITIC Dicastal Co., Ltd.
- Applicants: CITIC Dicastal CO., LTD.
- Inventors: Zaide WANG; Huanming MA; Junfu LI; Shengchao ZHANG; Qingwang WEI; Meng LIU
- Web page: https://patentgrep.com/patent/US20190292654A1

## CPC

- C23C 14/0057: {using reactive gases other than O2, H2O, N2, NH3 or CH4}
- B05D 1/06: Applying particulate materials
- B05D 3/0218: {Pretreatment, e.g. heating the substrate}
- B05D 3/0254: {After-treatment}
- B05D 3/102: {Pretreatment of metallic substrates (C23C takes precedence)}
- B05D 7/57: {the last layer being a clear coat}
- C23C 14/0015: {characterized by the colour of the layer}
- C23C 14/024: {Deposition of sublayers, e.g. to promote adhesion of the coating (C23C14/027 takes precedence)}
- C23C 14/0635: {Carbides}
- C23C 14/0688: {Cermets, e.g. mixtures of metal and one or more of carbides, nitrides, oxides or borides}
- C23C 14/205: {by cathodic sputtering}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/352: {using more than one target (C23C14/56 takes precedence)}
- C23C 22/78: Pretreatment of the material to be coated
- B05D 2202/25: based on Al
- B05D 2451/00: Type of carrier, type of coating (Multilayers)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

The disclosure provides an anti-aging periodic variable reaction black chromium coating film, sequentially comprising: an aluminum alloy matrix, a silane conversion film, a high-gloss organic resin coating, a metal compound and metal element periodic variable content alloy coating film, and a transparent resin coating. The disclosure simultaneously provides a method for forming the anti-aging periodic variable reaction black chromium coating film.

## Claims

### Claim 1

An anti-aging periodic variable reaction black chromium coating film, sequentially comprising: an aluminum alloy matrix, a silane conversion film, a high-gloss organic resin coating, a metal compound and metal element periodic variable content alloy coating film and a transparent resin coating;
wherein the silane conversion film is obtained using a silane pretreatment passivation process, the high-gloss organic resin coating film is made of an epoxy resin powder coating, the metal compound and metal element periodic variable content alloy coating film contains 0-90% of nickel, 10%-100% of chromium, 0-90% of chromium carbide and 0-90% of nickel carbide, the transparent resin coating is a pure acrylic resin coating having a thickness of 80-150 μm, and the high-gloss organic resin coating has a thickness of 120-250 μm.

### Claim 2

A method for forming an anti-aging periodic variable reaction black chromium coating film, comprising a process flow of: silane pretreatment, spraying of high-gloss medium powder, coating, and spraying of transparent powder
(1) the silane pretreatment on a surface of an aluminum alloy or other metal comprises steps of hot water washing, de-greasing and alkaline washing, hot water washing, water washing, acid washing, pure water washing, pure water washing, silane passivation, pure water washing, sealing, pure water washing, and moisture drying;
(2) the spraying of a high-gloss powder coating in the process flow refers to electro-statically spraying an epoxy powder coating or polyester powder coating onto a metal surface of a hub and curing same;
(3) the coating refers to high-vacuum magnetron sputtering on the surface of the hub after curing the medium powder, sputtering targets include a pure chromium target and a nickel-chromium metal target, the two targets are set with different power according to colors and opened for coating according to the process sequence, the hub can auto-rotate and revolve in an equipment, premixed gas of argon and acetylene is introduced during coating to form a chromium and chromium carbide coating film primer having a thickness of 5-10 nm, the formed coating film has good adhesion to the high-gloss organic coating, then the nickel-chromium alloy target is opened, the double targets work together to form a chromium, nickel, nickel-chromium alloy, chromium carbide and nickel carbide deposited film having a thickness of 80-150 nm, finally, only the chromium target is opened to form a chromium and chromium carbide coating film having a thickness of 5-10 nm, and an entire reaction coating film thickness is 120-250 nm; the surface of the hub is sputtered in a certain order and proportion;
(4) the spraying of transparent powder in the process flow refers to spraying transparent powder onto the surface of the coated hub and curing same, the transparent powder is an acrylic resin or polyester powder coating.

### Claim 3 (depends on 2)

The method for forming the anti-aging periodic variable reaction black chromium coating film according to claim 2, wherein in step (1) of pretreatment on the surface, the passivation is for a silane conversion film, a baking temperature of a moisture oven is 150° C., and a baking time is 30 min.

### Claim 4 (depends on 2)

The method for forming the anti-aging periodic variable reaction black chromium coating film according to claim 2, wherein in step (2), the high-gloss medium powder is sprayed with a thickness of 80 to 150 μm, a spoke surface curing temperature is 220° C., a curing time is 20 min, epoxy resin is preferred, and a hardness of the cured coating is 2-3 H; and after curing, the coated surface reaches a mirror finish, and a glass transition temperature of the coating is 80-120° C.

### Claim 5 (depends on 2)

The method for forming the anti-aging periodic variable reaction black chromium coating film according to claim 2, wherein in step (3), a temperature of the coated workpiece is 80-150° C., a flow rate of the working gas argon is 40-80 cc/min, a coating current for the chromium target and the nickel-chromium alloy target is 15-30 A, and a voltage is more than or equal to 550 v and less than 800 v; a vacuum degree is (2-8)×10−3 Pa, a double target coating time is 15-40 s, the working gas is 99.999% argon, and the reaction gas is acetylene having the purity of 99.999%; a coating environment humidity is less than or equal to 50%; in the coating sequence, the premixed gas of argon and acetylene is introduced first, then a pure chromium power supply is turned on for coating 3-7 seconds, the double targets are simultaneously opened for 14-24 seconds, finally a pure chromium is separately coated for 3-7 seconds, the hub rotates while being sputtered, a periodic variable alloy black chromium coating film is formed, and the targets are cooled at a temperature of 15-20° C.

### Claim 6 (depends on 2)

The method for forming the anti-aging periodic variable reaction black chromium coating film according to claim 2, wherein in step (3), argon and acetylene are premixed in advance, a percentage of the acetylene in the mixed gas is from 0 to 90%, and a total gas flow is 120-400 cc/min; and a brightness color L value is between 55 and 85.

### Claim 7 (depends on 2)

The method for forming the anti-aging periodic variable reaction black chromium coating film according to claim 2, wherein in step (4), the pure acrylic transparent powder is sprayed with a thickness of 80-150 μm, a surface curing temperature of the hub is 177° C., a curing time is 20 min, and a hardness of the coating is H level.