# US 2019/0292642 A1 · Preparation of nanostructured titanium

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0292642 A1
- Document ID: US20190292642A1
- Status: Published application
- Kind: A1
- Application number: 16/439,757
- Filed: 2019-06-13
- Published: 2019-09-26
- Earliest claimed: 2015-11-03
- Assignees: The Hong Kong Polytechnic University
- Applicants: The Hong Kong Polytechnic University
- Inventors: Guangping ZHENG
- Web page: https://patentgrep.com/patent/US20190292642A1

## CPC

- C22F 1/183: {of titanium or alloys based thereon}
- B21B 3/00: Rolling materials of special alloys so far as the composition of the alloy requires or permits special rolling methods or sequences {; Rolling of aluminium, copper, zinc or other non-ferrous metals}(altering special metallurgical properties of alloys, other than structure consolidation or mechanical properties resulting therefrom C21D, C22F)
- B21B 45/0218: {for strips, sheets, or plates (B21B45/023, B21B45/0233 take precedence)}
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)

## Abstract

The present disclosure relates to the preparation of bulk nanostructured pure titanium at cryogenic temperatures using rolling, allowing the whole microstructures of pure titanium to be refined into the one that the mean grain size is smaller than 100 nm.

## Claims

### Claim 1

A method for preparing a bulk nanostructured pure titanium from a pure titanium plate comprising:
providing at least one roller;
injecting liquid nitrogen onto the pure titanium plate to cool down the pure titanium plate to a temperature between −125° C. and −50° C.; and
rolling the cooled pure titanium plate by the at least one roller to form the bulk nanostructured pure titanium.

### Claim 2 (depends on 1)

The method of claim 1, wherein the at least one roller includes two rollers respectively located on both sides of the pure titanium plate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the step of rolling has a rolling speed between 0.05 and 2 rad/min.

### Claim 4 (depends on 1)

The method of claim 1, wherein the cooled pure titanium plate is rolled 15 to 30 times.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pure titanium plate has a thickness between 2 mm and 10 mm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the bulk nanostructured pure titanium comprises grain sizes of less than 100 nm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the liquid nitrogen is injected from at least one liquid nitrogen sprayer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the at least one liquid nitrogen sprayer includes two liquid nitrogen sprayers respectively located on both sides of one of the at least one roller.