# US 2019/0292620 A1 · Manual tool and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0292620 A1
- Document ID: US20190292620A1
- Status: Published application
- Kind: A1
- Application number: 16/465,086
- Filed: 2017-11-06
- Published: 2019-09-26
- Earliest claimed: 2017-11-06
- Assignees: Hangzhou United Tools Co., Ltd.; Hangzhou Great Star Industrial Co., Ltd.
- Applicants: Hangzhou United Tools Co., Ltd.; Hangzhou Great Star Industrial Co., Ltd.
- Inventors: Yueming Li
- Web page: https://patentgrep.com/patent/US20190292620A1

## CPC

- C21D 9/32: for gear wheels, worm wheels, or the like
- B25B 7/02: Jaws
- B25B 13/462: {the ratchet parts engaging in a direction radial to the tool operating axis}
- B25B 15/04: with ratchet action
- C21D 9/0068: {for particular articles not mentioned below}
- Y02P 10/25: Process efficiency
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B25B: TOOLS OR BENCH DEVICES NOT OTHERWISE PROVIDED FOR, FOR FASTENING, CONNECTING, DISENGAGING, OR HOLDING
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention discloses a method for manufacturing a manual tool, comprising: performing dual-frequency induction quenching on a first surface of a moment output part or a moment transmission part of the manual tool such that a quench-hardened layer is formed within a first depth range from the first surface of the moment output part to the interior of the moment output part or within a first depth range from the first surface of the moment transmission part to the interior of the moment transmission part, the hardness of the quench-hardened layer being higher than that of the body of the moment output part or the moment transmission part; the dual-frequency induction quenching being configured to simultaneously feed or introduce a high-frequency current and an intermediate-frequency current to the same induction coil to simultaneously heat the first surface of the moment output part or the first surface of the moment transmission part by the high-frequency current and the intermediate-frequency current, and then the moment output part or the moment transmission part being cooled and quenched. The present invention also discloses a manual tool manufactured by the above method. The manual tool subjected to double-frequency induction quenching according to the present invention has good abrasion resistance.

## Claims

### Claim 1

A method for manufacturing a manual tool, comprising the steps of:
performing dual-frequency induction quenching on a first surface of a moment output part or a first surface of a moment transmission part of the manual tool such that a quench-hardened layer is formed within a first depth range from the first surface of the moment output part to the interior of the moment output part or within a first depth range from the first surface of the moment transmission part to the interior of the moment transmission part, the hardness of the quench-hardened layer being higher than that of the body of the moment output part or the moment transmission part;
wherein the dual-frequency induction quenching is configured to simultaneously feed or introduce a high-frequency current and an intermediate-frequency current to the same induction coil to simultaneously heat the first surface of the moment output part or the first surface of the moment transmission part by the high-frequency current and the intermediate-frequency current and then the moment output part or the moment transmission part is cooled and quenched.

### Claim 2 (depends on 1)

The method for manufacturing a manual tool according to claim 1, wherein the first depth is 0.3-8.0 mm.

### Claim 3 (depends on 1)

The method for manufacturing a manual tool according to claim 1, wherein the dual-frequency induction quenching is such that a transition zone is formed between the quench-hardened layer and the body of the moment output part, and the hardness of the transition zone is lower than that of the body of the moment output part and not higher than that of the quench-hardened layer.

### Claim 4 (depends on 3)

The method for manufacturing a manual tool according to claim 3, wherein after the first surface of the moment output part is subjected to dual-frequency induction quenching, the body of the moment output part maintains the original hardness unchanged except for the quench-hardened layer and the transition zone.

### Claim 5 (depends on 1)

The method for manufacturing a manual tool according to claim 1, wherein the dual-frequency induction quenching is such that a transition zone is formed between the quench-hardened layer and the body of the moment transmission part, and the hardness of the transition zone is lower than that of the body of the moment transmission part and not higher than that of the quench-hardened layer.

### Claim 6 (depends on 5)

The method for manufacturing a manual tool according to claim 5, wherein after the first surface of the moment transmission part is subjected to dual-frequency induction quenching, the body of the moment transmission part maintains the original hardness unchanged except for the quench-hardened layer and the transition zone.

### Claim 7 (depends on 1)

The method for manufacturing a manual tool according to claim 1, wherein the first surface of the moment output part or the first surface of the moment transmission part is heated using an induction heating device, and the induction heating device includes the induction coil.

### Claim 8 (depends on 7)

The method for manufacturing a manual tool according to claim 7, wherein in the induction heating device, the high-frequency current has a frequency range of 100 to 500 KHz and a power range of 5 to 1500 KW.

### Claim 9 (depends on 7)

The method for manufacturing a manual tool according to claim 7, wherein in the induction heating device, the intermediate-frequency current has a frequency range of 0.2-25 KHz and a power range of 5-1500 KW.

### Claim 10

(canceled)

### Claim 11 (depends on 1)

The method for manufacturing a manual tool according to claim 1, wherein the method further comprises tempering the manual tool after dual-frequency induction quenching, the tempering temperature is 160-400° C., and the temperature-holding time is 2-8 h.

### Claim at position 12

12-14. (canceled)

### Claim 15

A method for manufacturing a manual tool, comprising the steps of:
providing a metal raw material;
machining the metal raw material according to the requirements of a manual tool so that the manual tool has a moment output part or a moment transmission part;
performing dual-frequency induction quenching on a first surface of the moment output part or a first surface of the moment transmission part such that a quench-hardened layer is formed within a first depth range from the first surface of the moment output part to the interior of the moment output part or within a first depth range from the first surface of the moment transmission part to the interior of the moment transmission part, the quench-hardened layer having a hardness higher than that of the body of the moment output part or the moment transmission part;
wherein the dual-frequency induction quenching is configured to simultaneously feed or introduce a high-frequency current and an intermediate-frequency current to the same induction coil to simultaneously heat the first surface of the moment output part or the first surface of the moment transmission part by the high-frequency current and the intermediate-frequency current, and then the moment output part or the moment transmission part is cooled and quenched; and
tempering the manual tool, after dual-frequency induction quenching.

### Claim 16

A manual tool, comprising at least a moment output part or a moment transmission part, wherein
a quench-hardened layer is formed within a first depth from a first surface of the moment output part to the interior of the moment output part or within a first range from a first surface of the moment transmission part to the interior of the moment transmission part, and
the formation process of the quench-hardened layer is: the first surface of the moment output part or the moment transmission part being simultaneously heated by the high-frequency current and the intermediate-frequency current fed or introduced to the same induction coil, and then the moment output part or the moment transmission part being cooled and quenched.

### Claim 17 (depends on 16)

The manual tool according to claim 16, wherein the hardness of the quench-hardened layer is higher than that of the body of the moment output part or the moment transmission part.

### Claim 18 (depends on 16)

The manual tool according to claim 16, wherein the first depth is 0.3 to 8.0 mm.

### Claim 19 (depends on 16)

The manual tool according to claim 16, wherein a transition zone is formed between the quench-hardened layer and the body of the moment output part, and the hardness of the transition zone is lower than that of the quench-hardened layer and not higher than that of the body of the moment output part;
wherein a contact face between the transition zone and the quench-hardened layer extends along the surface of the quench-hardened layer.

### Claim 20 (depends on 16)

The manual tool according to claim 16, wherein the dual-frequency induction quenching is such that a transition zone is formed between the quench-hardened layer and the body of the moment transmission part, and the hardness of the transition zone is lower than that of the body of the moment transmission part and not higher than that of the quench-hardened layer;
wherein the contact face between the transition zone and the quench-hardened layer extends along the surface of the quench-hardened layer.

### Claim 21

(canceled)

### Claim 22 (depends on 19)

The manual tool according to claim 19, wherein the depth of the transition zone is not greater than 3.0 mm.

### Claim 23 (depends on 16)

The manual tool according to claim 16, wherein the hardness of the quench-hardened layer is greater than 50 HRC.

### Claim 24 (depends on 16)

The manual tool according to claim 16, wherein the quench-hardened layer extends along the first surface of the moment output part or the first surface of the moment transmission part.

### Claim 25 (depends on 24)

The manual tool according to claim 24, wherein the manual tool is a pliers tool, the pliers head of the pliers tool is the moment output member, an outer surface of a tooth part of the pliers head is the first surface, the tooth part is simultaneously heated by the high-frequency current and the intermediate-frequency current, then cooled and quenched, the quench-hardened layer is formed within a first depth range from the outer surface of the tooth part to the interior of the tooth part and evenly distributed along the outer profile of the tooth part.

### Claim 26 (depends on 24)

The manual tool according to claim 24, wherein the manual tool is a wrench, the wrench comprises a handle and a moment output part disposed at a first end of the handle, an outer surface of the moment output part is simultaneously heated by the high-frequency current and the intermediate-frequency current, then cooled and quenched, the quench-hardened layer is formed within a first depth range from the outer surface of the moment output part to the interior of the moment output part, and the quench-hardened layer is concentric with the outer surface of the moment output part and evenly distributed along the outer surface of the moment output part.

### Claim 27 (depends on 24)

The manual tool according to claim 24, wherein the manual tool is a clamp, the clamp comprises a lever having a first working face and a second working face, the first working face and the second working face are simultaneously heated by the high-frequency current and the intermediate-frequency current, then cooled and quenched, the quench-hardened layer is formed within a first depth range from the first working face to the interior of the lever and within a first depth range from the second working face to the interior of the lever, and the quench-hardened layer is substantially parallel to the first working face and the second working face and evenly distributed along the first working face and the second working face.

### Claim 28 (depends on 27)

The manual tool according to claim 27, wherein the first working face is located opposite to the second working face, and a first clamping body and a second clamping body can move toward or away from each other along the first working face and the second working face.

### Claim 29 (depends on 24)

The manual tool according to claim 24, wherein the manual tool is a wrench having a ratchet ring, an outer surface of the ratchet ring is simultaneously heated by the high-frequency current and the intermediate-frequency current, then cooled and quenched, the quench-hardened layer is formed within a first depth range from the outer surface of the ratchet ring to the interior of the ratchet ring, and the quench-hardened layer is concentric with the outer surface of the ratchet ring and evenly distributed along the outer surface of the ratchet ring.

### Claim 30 (depends on 24)

The manual tool according to claim 24, wherein the manual tool is a ratchet screwdriver having a ratchet device including a ratchet and a pawl, an outer surface of the ratchet and an outer surface of the pawl are simultaneously heated by the high-frequency current and the intermediate-frequency current, then cooled and quenched, the quench-hardened layer is formed within a first depth range from the outer surface of the ratchet to the interior of the ratchet and within a first depth range from the outer surface of the pawl to the interior of the pawl; the quench-hardened layer on the ratchet is concentric with the outer surface of the ratchet and evenly distributed along the outer surface of the ratchet; and the quench-hardened layer on the pawl is concentric with the outer surface of the pawl and evenly distributed along the outer surface of the pawl.

### Claim 31 (depends on 30)

The manual tool according to claim 30, wherein the ratchet screwdriver further comprises an acceleration planetary gear mechanism including a ring gear, a sun gear and a planetary gear, an outer surface of the ring gear, an outer surface of the sun gear, and an outer surface of the planetary tooth are simultaneously heated by the high-frequency current and the intermediate-frequency current, then cooled and quenched, the quench-hardened layer is formed within a first depth range from the respective outer surface of the ring gear, the sun gear, and the planetary gear to the respective interior thereof; the quench-hardened layer on the ring gear is concentric with the outer surface of the ring gear and evenly distributed along the outer surface of the ring gear; the quench-hardened layer on the sun gear is concentric with the outer surface of the sun gear and evenly distributed along the outer surface of the sun gear; and the quench-hardened layer on the planetary gear is concentric with the outer surface of the planetary gear and evenly distributed along the outer surface of the planetary gear.