# US 2019/0292053 A1 · METHOD FOR DRYING AND PURIFYING LiFSI

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0292053 A1
- Document ID: US20190292053A1
- Status: Published application
- Kind: A1
- Application number: 16/331,242
- Filed: 2017-12-07
- Published: 2019-09-26
- Earliest claimed: 2016-12-08
- Assignees: Arkema France
- Applicants: Arkema France
- Inventors: Grégory Schmidt; Rémy Teissier
- Web page: https://patentgrep.com/patent/US20190292053A1

## CPC

- C01B 21/086: containing one or more sulfur atoms
- B01D 1/22: by bringing a thin layer of the liquid into contact with a heated surface {(B01D1/065 takes precedence)}
- C01B 21/0935: {Imidodisulfonic acid; Nitrilotrisulfonic acid; Salts thereof}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0568: characterised by the solutes
- B01D 11/0492: {Applications, solvents used}
- C01P 2006/40: Electric properties
- H01M 2300/0025: Organic electrolyte
- Y02E 60/10: Energy storage using batteries
- Y02P 20/133: Renewable energy sources, e.g. sunlight
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to a method for drying and purifying a lithium bis(fluorosulfonyl)imide salt in solution in an organic solvent S1, said method comprising the following steps: a) adding deionised water to dissolve and extract the lithium bis(fluorosulfonyl)imide salt, forming an aqueous solution of said salt; b) extracting the lithium bis(fluorosulfonyl)imide salt from said aqueous solution, using an organic solvent S2, said step being repeated at least once; c) concentrating the lithium bis(fluorosulfonyl)imide salt by evaporating said organic solvent S2 and the water, in a short-path thin-film evaporator, under the following conditions: temperature of 30° C. to 95° C., pressure of 10−3 mbar abs to 5 mbar abs, residence time no longer than 15 min; and d) optionally crystallising the lithium bis(fluorosulfonyl)imide salt. The present invention likewise relates to a composition made of lithium bis(fluorosulfonyl)imide salt, and the uses thereof in Li-ion batteries.

## Claims

### Claim 1

A process for drying and purifying a lithium bis(fluorosulfonyl)imide salt in solution in an organic solvent S1, said process comprising the following steps:
a) addition of deionized water to dissolve and extract the lithium bis(fluorosulfonyl)imide salt, forming an aqueous solution of said salt;
a′) optional concentration of said aqueous solution of said salt;
b) extraction of the lithium bis(fluorosulfonyl)imide salt from said aqueous solution, with an organic solvent S2, this step being repeated at least once;
c) concentration of said lithium bis(fluorosulfonyl)imide salt by evaporation of said organic solvent S2 and of the water, in a short-path thin-film evaporator, under the following conditions:
temperature of between 30° C. and 95° C.;
pressure between 10−3 mbar abs and 5 mbar abs; and
residence time of less than or equal to 15 min;
d) optionally, crystallization of the lithium bis(fluorosulfonyl)imide salt.

### Claim 2 (depends on 1)

The process as claimed in claim 1, comprising step a′) of concentration of said aqueous solution.

### Claim 3 (depends on 1)

The process as claimed in claim 1, in which step a) is such that the mass of deionized water is greater than or equal to a third of the mass of the initial solution of the lithium bis(fluorosulfonyl)imide salt in the organic solvent S1.

### Claim 4 (depends on 1)

The process as claimed in claim 1, in which the organic solvent S2 is chosen from the group constituted of organic carbonates, ethers and esters, and mixtures thereof.

### Claim 5 (depends on 1)

The process as claimed in claim 1, in which the organic solvent S1 is chosen from the group constituted of esters, nitriles, ethers, chlorinated solvents and aromatic solvents, and mixtures thereof.

### Claim 6 (depends on 1)

The process as claimed in claim 1, in which the organic solvent S2/water mass ratio, during an extraction, ranges from 1/6 to 1/1.

### Claim 7 (depends on 1)

The process as claimed in claim 1, also comprising, between step b) and step c), a step c′) of concentration of the organic solution obtained on conclusion of step b), to obtain an organic solution with a mass content of LiFSI of between 20% and 60%.

### Claim 8 (depends on 1)

The process as claimed in claim 1, in which the concentration step c) is performed at a pressure of between 10−2 mbar abs and 5 mbar abs.

### Claim 9 (depends on 1)

The process as claimed in claim 1, in which step c) is performed at a temperature of between 30° C. and 95° C.

### Claim 10 (depends on 1)

The process as claimed in claim 1, in which step c) is performed with a residence time of less than or equal to 5 minutes.

### Claim 11 (depends on 1)

The process as claimed in claim 1, in which the organic phase separated from the aqueous solution extracted in step a) is not reintroduced into the subsequent steps b) to d) of the process.

### Claim 12 (depends on 1)

The process as claimed in claim 1, in which, during step d), the lithium bis(fluorosulfonyl)imide salt is crystallized under cold conditions at a temperature of less than or equal to 25° C., optionally in an organic solvent S3 chosen from chlorinated solvents, and aromatic solvents, said salt optionally being recovered by filtration.

### Claim 13 (depends on 1)

The process as claimed in claim 1, wherein it leads to a lithium bis(fluorosulfonyl)imide salt comprising water in a content of less than or equal to 45 ppm relative to the total mass of said salt.

### Claim 14 (depends on 1)

A process for manufacturing a lithium bis(fluorosulfonyl)imide salt, comprising the following steps:
i. synthesis of bis(chlorosulfonyl)imide from sulfamic acid;
ii. fluorination of bis(chlorosulfonyl)imide to bis(fluorosulfonyl)imide; and
iii. preparation of the alkali metal or alkaline-earth metal salt of bis(fluorosulfonyl)imide by neutralization of the bis(fluorosulfonyl)imide;
iv. cation exchange to obtain a lithium bis(fluorosulfonyl)imide salt; and
v. drying and purification process as claimed in claim 1.

### Claim 15

A composition C comprising:
at least 99.80% by weight of lithium bis(fluorosulfonyl)imide salt relative to the total weight of said composition C;
between 5 ppm and 45 ppm by mass of water relative to the total mass of composition C; and
a mass content of sulfate ions of less than or equal to 100 ppm by mass relative to the total mass of composition C.

### Claim 16 (depends on 15)

The composition C as claimed in claim 15, comprising a mass content of sulfate ions of between 2 and 100 ppm by mass relative to the total mass of said composition C.

### Claim 17 (depends on 15)

The composition C as claimed in claim 15, comprising:
a mass content of water of between 5 and 45 ppm by mass relative to the total mass of said composition C;
a mass content of sulfate ions of less than or equal to 100 ppm relative to the total mass of said composition C;
a mass content of Cl− of less than or equal to 50 ppm by mass relative to the total mass of said composition C.

### Claim 18 (depends on 15)

The composition C as claimed in claim 15, wherein the sum of the water content and of the sulfate content is less than or equal to 100 ppm.

### Claim 19 (depends on 15)

A Li-ion battery comprising a composition C as claimed in claim 15.

### Claim 20 (depends on 19)

The Li-ion battery as claimed in claim 19, wherein the Li-ion battery is in a mobile device, an electric vehicle, or a renewable energy generation system.