# US 2019/0276363 A1 · Cement composition and manufacturing method for cement cured body using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0276363 A1
- Document ID: US20190276363A1
- Status: Published application
- Kind: A1
- Application number: 16/423,498
- Filed: 2019-05-28
- Published: 2019-09-12
- Earliest claimed: 2014-08-25
- Assignees: Taiheiyo Cement Corporation
- Applicants: Taiheiyo Cement Corporation
- Inventors: Risa NAKAYAMA; Katsuya KONO; Katsuhiko TADA; Hiroaki MORI; Shingo SUGIYAMA; Shinpei MAEHORI
- Web page: https://patentgrep.com/patent/US20190276363A1

## CPC

- C04B 28/04: Portland cements
- B28B 1/14: by simple casting, the material being neither forcibly fed nor positively compacted (for molten material B28B1/54)
- B28B 1/52: specially adapted for producing articles from mixtures containing fibres, {e.g. asbestos cement}(by wrapping on to mandrels B28B1/42)
- B28B 11/245: {Curing concrete articles (B28B11/242 takes precedence)}
- B28B 11/246: {Underwater curing}
- B28B 11/247: {Controlling the humidity during curing, setting or hardening}
- C04B 7/02: Portland cement
- C04B 14/04: Silica-rich materials; Silicates
- C04B 14/38: Fibrous materials; Whiskers
- C04B 14/48: Metal
- C04B 16/06: fibrous
- C04B 18/02: Agglomerated materials {, e.g. artificial aggregates}
- C04B 18/14: from metallurgical processes (treatment of molten slag C04B5/00)
- C04B 18/146: {Silica fume}
- C04B 22/06: Oxides, Hydroxides (C04B22/0013 takes precedence)
- C04B 24/04: Carboxylic acids; Salts, anhydrides or esters thereof
- C04B 24/26: obtained by reactions only involving carbon-to-carbon unsaturated bonds {(C04B24/243 takes precedence)}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 40/02: Selection of the hardening environment
- C04B 40/0263: {Hardening promoted by a rise in temperature (C04B40/024 takes precedence)}
- C04B 2103/302: {Water reducers}
- C04B 2103/50: Defoamers, air detrainers
- C04B 2201/52: High compression strength concretes, i.e. with a compression strength higher than about 55 N/mm2, e.g. reactive powder concrete [RPC]
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Provided is a cement composition that has high fluidity (for example, a 0-drop flow value of 200 mm or more) before curing and exhibits high compressive strength (for example, 320 N/mm2 or more) after curing. The cement composition includes a cement, a silica fume having a BET specific surface area of from 10 m2/g to 25 m2/g, an inorganic powder having a 50% cumulative particle size of from 0.8 μm to 5 μm, a fine aggregate having a maximum particle size of 1.2 mm or less, a water reducing agent, an antifoaming agent, and water. The ratio of the cement is from 55 vol % to 65 vol %, the ratio of the silica fume is from 5 vol % to 25 vol %, and the ratio of the inorganic powder is from 15 vol % to 35 vol % in the total amount of 100 vol % of the cement, the silica fume, and the inorganic powder.

## Claims

### Claim 1

A method of producing a cementitious cured body made of a cement composition, the cement composition comprising:
cement;
silica fume having a BET specific surface area of from 10 m2/g to 25 m2/g;
an inorganic powder having a 50% cumulative particle size of from 0.8 μm to 5 μm;
a fine aggregate having a maximum particle size of 1.2 mm or less;
a water reducing agent;
an antifoaming agent; and
water,
wherein a ratio of the cement is from 55 vol % to 65 vol %, a ratio of the silica fume is from 5 vol % to 25 vol %, and a ratio of the inorganic powder is from 15 vol % to 35 vol % in a total amount of 100 vol % of the cement, the silica fume, and the inorganic powder,
the method comprising:
a molding step of setting the cement composition into a mold to provide an uncured molded body;
a room temperature curing step of subjecting the uncured molded body to sealed curing or atmospheric curing at from 10° C. to 40° C. for 24 hours or more, followed by demolding the molded body from the mold, to thereby provide a cured molded body;
a water absorbing step of immersing the cured molded body into boiling and non-pressurized water, and then cooling the water to 40° C. or less while keeping the cured molded body immersed in the water;
a heat curing step of subjecting the cured molded body after being immersed in the water to steam curing or hot water curing at from 70° C. to 95° C. for 24 hours or more, to thereby provide a cured body after heat curing; and
a high-temperature heating step of heating the cured body after the heat curing at from 150° C. to 200° C. for 24 hours or more, to thereby provide the cementitious cured body.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the cement is a cement which is not subjected to polishing treatment, and the BET specific surface area of the silica fume is from 15 m2/g to 25 m2/g.

### Claim 3 (depends on 1)

The method according to claim 1, wherein
the cement comprises coarse particles each having a particle size of 20 μm or more, in which an angular surface portion is deformed into a rounded shape, obtained by subjecting particles forming moderate-heat Portland cement or low-heat Portland cement to polishing treatment, and fine particles each having a particle size of less than 20 μm generated by the polishing treatment; and
the cement has a 50% weight cumulative particle size of from 10 μm to 18 μm and a Blaine specific surface area of from 2,100 cm2/g to 2,900 cm2/g.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising one or more kinds of fibers selected from the group consisting of metal fibers, organic fibers, and carbon fibers, in which a ratio of the fibers in the cement composition is 3 vol % or less.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the cement composition has a compressive strength after curing of 320 N/mm2 or more.

### Claim at position 6

6-9. (canceled)

### Claim 10 (depends on 1)

The method according to claim 1, wherein the room temperature curing step comprises demolding the cured molded body from the mold at a time when the cured molded body exhibits a compressive strength of from 20 N/mm2 to 100 N/mm2.