# US 2019/0245509 A1 · Method for fabricating single crystal piezoelectric rf resonators and filters with improved cavity definition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245509 A1
- Document ID: US20190245509A1
- Status: Published application
- Kind: A1
- Application number: 15/888,358
- Filed: 2018-02-05
- Published: 2019-08-08
- Earliest claimed: 2018-02-05
- Assignees: Zhuhai Crystal Resonance Technologies Co., Ltd.
- Applicants: Zhuhai Crystal Resonance Technologies Co., Ltd.
- Inventors: Dror Hurwitz
- Web page: https://patentgrep.com/patent/US20190245509A1

## CPC

- H03H 3/02: for the manufacture of piezoelectric or electrostrictive resonators or networks (H03H3/08 takes precedence)
- H03H 9/02031: {consisting of ceramic}
- H03H 9/02102: {of temperature influence (cutting angles H03H9/02015)}
- H03H 9/02401: {by annealing}
- H03H 9/1014: {the enclosure being defined by a frame built on a substrate and a cap, the frame having no mechanical contact with the BAW device}
- H03H 9/132: {characterized by a particular shape}
- H03H 9/173: {Air-gaps}
- H03H 9/584: {Coupled Resonator Filters [CFR]}
- H03H 9/587: {Air-gaps}
- H03H 9/588: {Membranes}
- H03H 9/605: {consisting of a ladder configuration}
- H03H 2003/021: {the resonators or networks being of the air-gap type}
- H03H 2003/023: {the resonators or networks being of the membrane type}
- H03H 2003/027: {the resonators or networks being of the microelectro-mechanical [MEMS] type}
- Y10T 29/42: Piezoelectric device making
- Y10T 29/49005: Acoustic transducer
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of fabricating an FBAR filter device including an array of resonators, each resonator comprising a single crystal piezoelectric film sandwiched between a first metal electrode and a second metal electrode, wherein the first electrode is supported by a support membrane over an air cavity, the air cavity embedded in a silicon dioxide layer over a silicon handle, with through-silicon via holes through the silicon handle and into the air cavity, the side walls of said air cavity in the silicon dioxide layer being defined by perimeter trenches that are resistant to a silicon oxide etchant.

## Claims

### Claim 1

A method of fabricating an FBAR filter device comprising an array of resonators, each resonator comprising a single crystal piezoelectric film sandwiched between a first metal electrode and a second metal electrode, wherein the first electrode is supported by a support membrane over an air cavity, the air cavity embedded in a silicon dioxide layer over a silicon handle, with through-silicon via holes through the silicon handle and into the air cavity, the side walls of said air cavity in the silicon dioxide layer being defined by perimeter trenches that are resistant to a silicon oxide etchant, comprising the stages of:
A. Fabricating a support membrane over a silicon dioxide box on a silicon handle, having through support membrane filled barriers that traverse the silicon oxide layer, and wherein the support membrane is coated with at least a bonding layer of a first metal electrode coupled to the support membrane by an adhesion layer;
B. Fabricating a piezoelectric layer coupled to a detachable carrier substrate and coated with at least a bonding layer of the first metal electrode coupled to the piezoelectric film by an adhesion layer;
C. Bonding the support membrane to the piezoelectric film by bonding the two bonding layers together to sandwich the first metal electrode between the piezoelectric film and the support membrane;
D. Processing the piezoelectric layer coupled to the support membrane from the piezoelectric layer side by removing the carrier substrate, trimming the piezoelectric layer into piezoelectric films, first electrode layers and exposed surface of the support membrane, and by surrounding the piezoelectric films with a passivation material and coating with a second electrode, and building up base parts of seal rings and contact stacks;
E. Fabricating an array of lids with external terminations on an outer surface and upper sections of seal rings and contact stacks on an inner surface, such that the external terminations are coupled to the contact stacks by through lid vias, and fabricating upper sections of seal ring and contact stacks for coupling to the base section of contact stacks by a bonding layer;
F. Attaching the array of filters to the array of caps by coupling the base sections of the seal ring and contact stacks to the upper sections of the seal ring and contact stacks with bonding layers;
G. Thinning the handle and drilling holes through the thinned handle to the silicon oxide layer, etching away silicon oxide and optionally etching away at least part of the supporting membrane and sealing the etch holes; and
H. Dicing the array into individual filters.

### Claim 2 (depends on 1)

The method of claim 1 wherein stage B is performed prior to stage A.

### Claim 3 (depends on 1)

The method of claim 1 wherein at least some of the processing steps of stage G precede Stage D.

### Claim 4 (depends on 1)

The method of claim 1 wherein at least some of the processing steps of stage G precede Stage F.

### Claim 5 (depends on 1)

The method of claim 1 wherein at least some of the processing steps of stage E precede any of stages A to D.

### Claim 6 (depends on 1)

The method of claim 1 wherein stage A comprises the steps of:
obtaining a support membrane attached to a silicon handle by a silicon oxide layer;
creating trenches through the support membrane, the silicon dioxide layer and into the silicon handle;
depositing a silicon nitride coating over the membrane surface and into the trenches that optionally fills said trenches;
optionally depositing polysilicon over the silicon nitride coated membrane surface and coated trenches to fill the trenches and then removing polysilicon from the surface thereby exposing the silicon nitride coating over the membrane surface;
removing the silicon nitride coating to exposing the membrane surface, and
depositing a first adhesion layer followed by a first part of the first electrode over the membrane surface terminating with a bonding layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein the support membrane attached to a silicon handle by a silicon oxide layer of Stage A comprises single crystal silicon with an orientation of <110>, <111> or <100> and said support membrane is a wafer sliced from a single crystal of silicon and optionally subsequently polished.

### Claim 8 (depends on 1)

The method of claim 1, wherein the support membrane attached to a silicon handle by a silicon oxide layer of Stage A comprises: single crystal lithium niobate or single crystal lithium tantalate and is obtained by a process comprising the steps of:
bombarding a single crystal donor wafer with hydrogen or helium ions to a depth of less than 1.5 microns to generate a membrane that is weakly coupled to the single crystal donor wafer;
Attaching side of the wafer with weakly coupled membrane to the silicon handle by a silicon dioxide layer that is either thermally grown or pre-deposited onto the silicon handle and/or onto the weakly coupled side of single crystal donor wafer;
exposing the single crystal donor wafer to elevated temperature thereby rupturing bonds holding the membrane to the donor wafer and leaving the single crystal support membrane coupled to the silicon handle by the silicon dioxide layer, and
optionally polishing to remove damage, and annealing if necessary, to cause atomic rearrangement.

### Claim 9 (depends on 1)

The method of fabricating a filter device of claim 1 wherein the barriers through the membrane, the silicon dioxide layer and into the silicon handle fabricating are fabricated by creating trenches by deep reactive ion etch (DRIE) using BOSCH process, lining the trenches with SiN and filling the trenches with a filler material consisting of SiN or silicon poly-crystal.

### Claim 10 (depends on 1)

The method of fabricating a filter device of claim 1 wherein the first adhesion layer of Step A is selected from the group comprising titanium, chromium and titanium-tungsten and the first part of first electrode layer is selected from the group comprising tungsten, titanium-tungsten, molybdenum, aluminum and gold and the first adhesion layer and first part of the electrode layer are deposited by physical vapor deposition.

### Claim 11 (depends on 1)

The method of fabricating a filter device of claim 1 wherein the first adhesion layer of Step A comprises titanium or chromium or titanium-tungsten and an outer layer of the first part of the first electrode is a thin gold layer having a thickness range of 10 to 25 nanometers deposited by physical vapor deposition.

### Claim 12 (depends on 1)

The method of fabricating a filter device of claim 1 wherein Step B comprises depositing a single crystal piezoelectric layer onto a release layer coupled to a carrier substrate, wherein the piezoelectric layer is deposited to a thickness of up to 1.5 microns by sputtering or Molecular Beam Epitaxy (MBE) and is selected from the group comprising:
BaxSr(1-x)TiO3 in a <111> orientation where x<0.5;
AlN in a C-Axis orientation;
AlxGa1-xN in a C-Axis orientation where x>0.85;
ScxAl1-xN in a C-Axis orientation where 0.05<x<0.25

### Claim 13 (depends on 1)

The method of fabricating a filter device of claim 1 wherein Step B comprises depositing a single crystal piezoelectric layer coupled by a release layer to a detachable carrier substrate, wherein the piezoelectric layer comprises a layer of single crystal lithium niobate or single crystal lithium tantalate having a thickness of up to 1.5 microns and is obtained by a process comprising:
bombarding a facet of a single crystal donor wafer of the piezoelectric with hydrogen or helium ions to a depth of less than 1.5 microns to generate a membrane that is weakly coupled to the facet of the single crystal donor wafer;
Attaching outer surface of the weakly coupled membrane onto the release layer coupled to the carrier substrate by a surface activated wafer bonding process (SAB) or by fusing a silicon dioxide layer, pre-deposited onto the weakly coupled membrane and said release layer;
exposing the single crystal donor wafer to an elevated temperature thereby rupturing bonds holding the piezoelectric layer to the donor wafer and leaving the single crystal piezoelectric layer coupled to the release layer coupled to the carrier substrate; and
optionally polishing to remove damage, and annealing if necessary, to cause atomic rearrangement.

### Claim 14 (depends on 1)

The method of fabricating a filter device of claim 1 wherein stage B is characterized by at least one of the following limitations:
the removable carrier comprises sapphire;
the release layer comprises GaN;
the removable carrier and release layer are C-axis <0001> with maximum tolerance of ±0.5 degrees.

### Claim 15 (depends on 1)

The method of fabricating a filter device of claim 1 wherein in Stage C, the first electrode comprises a first adhesion layer attached to the support membrane, a second adhesion layer attaching second and third coating layers and a third adhesion layer for attaching the third coating layer to the piezoelectric layer; wherein the adhesion layers are selected from the group of titanium, chromium and titanium-tungsten and one of the first and second coating layers is selected from the group of tungsten, titanium-tungsten, molybdenum and aluminum and the other of the first and second coating layers is a bonding layer of gold having a thickness range of 20 to 50 nanometer, and all layers of the first electrode are deposited by physical vapor deposition.

### Claim 16 (depends on 1)

The method of fabricating a filter device of claim 1 wherein stage C comprises bonding the first and second parts of the first electrode together by a surface activated bonding process with at least one of the following limitations:
the process is performed between two identical materials selected from the group of tungsten, molybdenum, aluminum and titanium-tungsten;
the process is performed between two metals having an average surface roughness of less than 0.5 nanometers with or without pre polishing the surface by CMP;
the process is performed by pre-activating the to be bonded surfaces by plasma, the plasma gas selected from the group of argon and nitrogen;
the process is performed under vacuum;
the process is performed under pressure range of 5 MPa to 50 MPa;
the process is performed under temperature range from room temperature to less than 300° C.

### Claim 17 (depends on 1)

The method of fabricating a filter device of claim 1, wherein stage C comprises the steps of:
providing a single crystal piezoelectric layer coupled to a detachable substrate by a release layer from its first side and further comprising a second part of the first electrode layer attached to the single crystal piezoelectric layer from its second side by a second adhesion layer;
bonding the first part of the electrode to the second part of the electrode to form a first electrode that couples the support membrane to the piezoelectric layer.

### Claim 18 (depends on 1)

The method of fabricating a filter device of claim 1, wherein stage D comprises the steps of:
processing from the detachable substrate side by removing the detachable substrate and release layer;
trimming the piezoelectric layer and selectively removing the piezoelectric layer, first electrode and support membrane to fabricate resonator stacks comprising the piezoelectric layer on the first electrode;
surrounding the resonator stacks with a passivation material;
depositing an upper electrode over the piezoelectric layer with upper and lower electrodes pad terminations over the passivation layer, and a first part of a metal seal ring around the perimeter of each FBAR filter unit over the passivation layer.

### Claim 19 (depends on 18)

The process of claim 18 wherein the step of removing the detachable carrier substrate in stage D is performed by a laser lift off process.

### Claim 20 (depends on 18)

The method of fabricating a filter device of claim 18 wherein the detachable substrate in stage D comprises a sapphire single crystal wafer coated with GaN and the laser lift off process comprises irradiating the GaN through the sapphire using 248 nm excimer square waveform laser.

### Claim 21 (depends on 18)

The method of fabricating a filter device of claim 18 wherein removing the release layer in stage D is performed by an exposing to an induction coupled plasma.

### Claim 22 (depends on 18)

The method of fabricating the filter device of claim of claim 18 wherein trimming the piezoelectric layer comprises applying a scanning surface ion milling process over the surface of the piezoelectric membrane.

### Claim 23 (depends on 18)

The method of fabricating the filter device of claim 18 wherein the process of selectively removing the piezoelectric layer, first electrode and support membrane to fabricate resonator stacks in Step D comprises the process steps of applying photo-resist followed by selectably exposing through windows in the photo-resist and applying an induction coupled plasma to etch the said piezoelectric, first electrode and support membrane layers through said windows.

### Claim 24 (depends on 18)

The method of fabricating the filter device of claim 18, wherein the passivation material surrounding the resonator stacks is selected from the group comprising SiO2, silicon nitride, Ta2O5, polyimide and Benzocyclobutene (BCB).

### Claim 25 (depends on 18)

The method of fabricating the filter device of claim 18, wherein the upper electrode over the piezoelectric layer, pad terminations over the passivation layer and a first part of a metal seal ring in the perimeter of the FBAR filter device are selected from the group of tungsten, molybdenum, aluminum and gold and are deposited by sputtering or physical vapor deposition.

### Claim 26 (depends on 18)

The method of fabricating the filter device of claim 18, wherein the adhesion layers are selected from the group of titanium, chromium and titanium-tungsten, and are deposited by PVD
onto the piezoelectric layer prior to deposition of the upper electrode;
over the passivation layer prior to deposition of the upper and lower electrodes pad terminations, and
over the passivation layer prior to deposition of the first part of a metal seal ring around the perimeter of the FBAR filter device.

### Claim 27 (depends on 1)

The method of fabricating the filter device of claim 1 wherein Stage E comprises:
Fabricating an array of lids having an inner and outer surface having through metal vias electrically connecting terminations pads on the outer surface to capture pads under the inner surface of the array of lids, and further comprising an array of second metal seal rings on the inner surface of the cap such that the second metal seal rings have similar shape and size to the first metal seal rings around the perimeter of each filter unit in the FBAR filter array.

### Claim 28 (depends on 27)

The method of fabricating the filter device of claim 27 wherein the stage E of providing an array of lids comprises the steps of:
e. obtaining a silicon wafer with an inner and an outer surface;
f. drilling blind via holes having blind ends from the outer surface by deep reactive ion etch (DRIE) using BOSCH process;
g. depositing a silicon nitride or silicon dioxide liner layer into the blind vias holes and over the outer surface of the silicon cap;
h. depositing a titanium-copper seed layer over the silicon nitride surface and into the blind vias holes;
i. pattern electroplating copper to fill the blind vias holes and to generate copper termination pads over the filled blind vias;
j. etching away the titanium copper seed layer;
k. depositing a metal finish selected from the group of gold, ENIG and ENEPIG over the termination pads;
l. grinding away the inner surface of the silicon cap to within 25 microns of the blind ends of the copper filled blind vias;
m. thinning down the silicon with plasma to remove an additional 25˜30 microns of silicon, thereby exposing about 5 microns of the ends of the silicon nitride or silicon dioxide lined copper filled vias without damaging the silicon nitride or silicon dioxide liner or copper filling;
n. depositing silicon nitride or silicon dioxide over the inner surface of the silicon cap and exposed silicon nitride or silicon dioxide coated copper vias;
o. Removing the silicon nitride and protruding copper by chemical mechanical polishing (CMP), thereby exposing the ends of the copper vias in the silicon nitride or silicon dioxide layer coating the inner surface of the silicon cap;
p. depositing an adhesion layer selected from the group of titanium, chromium and titanium-tungsten followed by a gold seed layer over inner surface of the silicon cap;
q. terminating the inner surface by either:
applying a photo-resist and patterning with trenches over the gold seed layer; filling the trenches with a layer of gold or gold-tin mix. by electroplating; stripping away the resist and etching away the seed layer, thereby generating a gold or a gold-tin bonding layer over the gold capture pads and seal ring defining the perimeter of each device on the inner surface of the cap, and
applying a photo-resist and patterning with capture pads and a seal ring defining the perimeter of each cap device and filling the pattern by screen printing nano-sized gold particles in an organic binder in a paste form; sintering the paste at 200° C. to remove the binder, and stripping away the photo-resist.

### Claim 29 (depends on 27)

The method of fabricating the filter device of claim 27 wherein the stage E of providing a cap comprises the steps of:
obtaining a glass having an inner and an outer surface;
laser drilling through via holes through the glass wafer;
sputtering a Ti/Cu seed layer into the through via holes and over the inner and outer surfaces of the glass wafer;
Depositing a layer of photo-resist on both inner and outer surfaces of the glass wafer and patterning to form an array of seal rings defining the perimeter of each lid for each filter unit in the array of lids and an array of pad shapes over each through hole, and patterning an array of termination pad shapes adjacent to ends of the through vias on the outer surface of the glass wafer;
Filling the pattern with copper by electroplating;
stripping away the photo-resist, and
terminating the cap by:
etching the Ti/Cu seed layer from both cap's surfaces and
depositing a metal finish over the termination pads on the outer surface, said metal finish being selected from the group of gold, ENIG and ENEPIG;
processing the inner surface by applying and patterning a thicker layer of photo-resist over the array of capture pads and seal rings; filling the thicker pattern by either (i) screen printing nano-sized gold particles and organic binder in a paste form; sintering the paste at 200° C. and stripping away the photo-resist, thereby fabricating a bond layer, or by (ii) electroplating gold or a gold tin mix into the photo-resist trenches and stripping away the photo-resist.

### Claim 30 (depends on 29)

The method of fabricating the filter device of claim 29 wherein the through via holes are fabricated in the glass wafer by laser drilling from both sides.

### Claim 31 (depends on 1)

The method of fabricating the filter device of claim 1 wherein step F of attaching the array of lids to the array of filters comprises the steps of:
depositing a metal bonding layer on at least one of the array of second metal seal rings and capture pads coupled to the inner side of the cap, and
the said first metal seal ring and pads coupled to the first and second electrodes of the FBAR filter device;
Bonding the array of lids to the wafer FBAR filter by reflowing the metal bonding layer such that the seal ring and the inner surface of the caps define a cavity over each filter array.

### Claim 32 (depends on 31)

The method of fabricating the filter device of claim 31 wherein the step of bonding the wafer cap to the wafer FBAR filter is performed by reflowing the bond layer under vacuum and temperature range of 150° C. to 300° C. and pressure of 50 MPa to 100 MPa.

### Claim 33 (depends on 1)

The method of fabricating the filter device of claim 1 wherein stage G of processing from the handle side comprises the steps of:
thinning the handle;
drilling via holes through the handle to the silicon oxide layer within areas defined by the perimeter trenches, and

### Claim 33 (depends on 33)

The method of fabricating the filter device of claim 33 wherein etching away the silicon oxide within the perimeter trenches in the membrane silicon oxide layer and handle to form individual cavities under each resonator stack, the perimeter barriers serve as etch stops.

### Claim 34 (depends on 33)

The method of claim 33 further comprising at least one of the following steps:
trimming the support membrane through the via holes and the air cavity to a thickness of between zero and the thickness of the piezoelectric layer.
plugging the through silicon vias by depositing a layer of polysilicon under the wafer handle side;

### Claim 35 (depends on 33)

The method of fabricating the filter device of claim 33 wherein the step of drilling via holes through the handle to the silicon dioxide layer within the perimeter trenches comprises by deep reactive ion etch process (DRIE) using BOSCH process.

### Claim 36 (depends on 33)

The method of fabricating the filter device of claim 33 wherein the step of etching away the silicon oxide within the perimeter barriers in the membrane, silicon oxide layer and handle comprises exposing to liquid or vapor HF.

### Claim 37 (depends on 34)

The method of fabricating the filter device of claim 34 wherein the step of thinning the support membrane through the silicon vias and the air cavity to a thickness of between zero and the thickness of the piezoelectric layer is achieved by photo-resist masking the silicon handle surface to only expose the through silicon vias, and exposing the silicon handle and photo-resist to inductive coupling or microwave sourced a plasma fabricated from a XeF2 and Ar gas mixture.