# US 2019/0245246 A1 · Tool and Method of Fabricating a Self-Aligned Solid State Thin Film Battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245246 A1
- Document ID: US20190245246A1
- Status: Published application
- Kind: A1
- Application number: 15/892,399
- Filed: 2018-02-08
- Published: 2019-08-08
- Earliest claimed: 2018-02-08
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Frank Robert Libsch; Ghavam G. Shahidi; Ko-Tao Lee; Stephen M. Rossnagel
- Web page: https://patentgrep.com/patent/US20190245246A1

## CPC

- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- C23C 14/06: characterised by the coating material ({C23C14/0021} , C23C14/04 take precedence)
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/08: Oxides (C23C14/10 takes precedence)
- C23C 14/542: {Controlling the film thickness or evaporation rate}
- C23C 14/545: {using measurement on deposited material}
- H01M 4/0426: {Sputtering}
- H01M 10/0404: {Machines for assembling batteries}
- H01M 10/0562: Solid materials
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A solid state electrochemical battery fabrication device and a method of creating the solid state electrochemical battery are provided. There is a first chamber comprising a first magnetron and a second chamber comprising a second magnetron, coupled to the first chamber. There is a third chamber comprising a vapor source for a polymer deposition, coupled to the second chamber. A Knudsen cell is coupled to the third chamber and configured to deposit lithium on a battery being fabricated. A linear hollow shaft connects the first, second, and third chambers, and provides a hermetic seal. A first telescopic arm having a housing is coupled to a first end of the hollow shaft and configured to extend out of its housing from the first chamber to the second chamber.

## Claims

### Claim 1

A solid state electrochemical battery fabrication device, comprising:
a first chamber comprising a first magnetron;
a second chamber comprising a second magnetron, coupled to the first chamber;
a third chamber comprising a vapor source for a polymer deposition, coupled to the second chamber;
a Knudsen cell coupled to the third chamber and configured to deposit lithium on a battery being fabricated;
a hollow shaft configured to connect the first, second, and third chambers, and provide a hermetic seal between the first, second, and third chambers; and
a first telescopic arm having a housing coupled to a first end of the hollow shaft and configured to extend out of its housing from the first chamber to the second chamber.

### Claim 2 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, wherein the first chamber further comprises a pump configured to evacuate at least the first chamber and the second chamber via the hollow shaft.

### Claim 3 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, further comprising a pump coupled to the Knudsen cell and configured to evacuate the third chamber of at least lithium (Li) particles.

### Claim 4 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, further comprising a conflat gate valve coupled between the third chamber and the Knudsen cell.

### Claim 5 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, further comprising a conflat gate valve coupled between the second chamber and the third chamber.

### Claim 6 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, wherein the vapor source for the polymer deposition is configured to deposit at least one layer of passivation over a second polar conductor layer of the battery being fabricated.

### Claim 7 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, further comprising a heat element positioned in the hollow shaft between the first chamber and the second chamber and configured to control a temperature in the first, second, and third chambers.

### Claim 8 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, wherein the heat element is a heat lamp configured to align molecules that are deposited to a microstructure orientation of 101.

### Claim 9 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, wherein the first magnetron is a direct current (DC) sputtering gun configured to provide LiCoO2 particles during a first polar conductor deposition step.

### Claim 10 (depends on 9)

The solid state electrochemical battery fabrication device of claim 9, wherein:
the first chamber further comprises a first collimator coupled between the first magnetron and the battery being fabricated, and
the first collimator together with the first telescopic arm, are configured to provide a two-dimensional control of a deposition angle of particles of the first magnetron.

### Claim 11 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, wherein the second magnetron is a radio frequency (RF) sputtering gun configured to provide Li3PO4 particles during an electrolyte deposition step.

### Claim 12 (depends on 11)

The solid state electrochemical battery fabrication device of claim 11, wherein
the second chamber further comprises a second collimator coupled between the magnetron and the battery,
the second collimator together with the first telescopic arm, are configured to provide a two-dimensional control of a deposition angle of particles of the second magnetron.

### Claim 13 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, wherein the second chamber further comprises a gauge configured to track a lithium phosphorous oxynitride (LiPON) deposition thickness on the battery being fabricated.

### Claim 14 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, wherein the first telescopic arm is further configured to extend into the third chamber.

### Claim 15 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, further comprising a second telescopic arm having a housing coupled to a second end of the hollow shaft and configured to extend out of its housing from the third chamber to the second chamber to receive the battery being fabricated from the first arm and carry the battery being fabricated to the third chamber.

### Claim 16 (depends on 1)

The solid state electrochemical battery fabrication device of claim 1, wherein the first telescopic arm is further configured to rotate on its axis to provide one dimensional control of a deposition angle onto the battery being fabricated.

### Claim 17

A method of creating a solid state electrochemical battery using a fabrication device having a plurality of chambers, the method comprising:
depositing a first conductive electrode layer on top of a substrate;
depositing a first polar conductor layer on top of a portion of the conductive electrode layer in a first chamber of the fabrication device;
depositing a first solid electrolyte layer after the first polar conductor layer in a second chamber of the fabrication device;
depositing a lithium layer after the first solid electrolyte layer in a third chamber of the fabrication device;
depositing a second conductive electrode layer after the lithium layer; and
depositing at least one passivation layer after the second conductive electrode layer in the third chamber of the fabrication device, wherein the plurality of chambers is atmosphere controlled.

### Claim 18 (depends on 17)

The method of claim 17, wherein the deposition of the first polar conductor layer is via a direct current (DC) sputtering gun providing LiCoO2 particles that are deposition controlled via a first collimator.

### Claim 19 (depends on 18)

The method of claim 18, wherein the deposition of first solid electrolyte layer is via a radio frequency (RF) sputtering gun providing Li3PO4 particles that are deposition controlled via a second collimator.

### Claim 20 (depends on 17)

The method of claim 17, wherein the deposition of lithium layer is via a Knudsen cell.