# US 2019/0245234 A1 · Proton-conductive membrane and fuel cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245234 A1
- Document ID: US20190245234A1
- Status: Published application
- Kind: A1
- Application number: 16/256,186
- Filed: 2019-01-24
- Published: 2019-08-08
- Earliest claimed: 2018-02-05
- Assignees: Toyota Jidosha Kabushiki Kaisha; National University Corporation Nagoya University
- Applicants: Toyota Jidosha Kabushiki Kaisha; National University Corporation Nagoya University
- Inventors: Naoki NAKAMURA; Atsushi NORO; Takato KAJITA; Haruka TANAKA; Yushu MATSUSHITA
- Web page: https://patentgrep.com/patent/US20190245234A1

## CPC

- H01M 8/1048: Ion-conducting additives, e.g. ion-conducting particles, heteropolyacids, metal phosphate or polybenzimidazole with phosphoric acid
- H01M 8/1023: having only carbon, e.g. polyarylenes, polystyrenes or polybutadiene-styrenes
- H01M 8/103: having nitrogen, e.g. sulfonated polybenzimidazoles [S-PBI], polybenzimidazoles with phosphoric acid, sulfonated polyamides [S-PA] or sulfonated polyphosphazenes [S-PPh]
- H01M 8/1069: characterised by the manufacturing processes
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- H01M 2300/0082: Organic polymers
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

[OBJECT] To provide a proton-conductive membrane which exhibits high proton conductivity even in an anhydrous environment. [SOLVING MEANS] Provided is a proton-conductive membrane including a crosslinked polymer and a plasticizer, wherein the crosslinked polymer includes a proton acceptor group in an amount equal to not less than 10 mol % of repeating units constituting the crosslinked polymer, the plasticizer includes a proton donor compound having a pKa value of not more than 2.5, and the plasticizer is a viscoelastic solid in a temperature range of 50° C. to 120° C.

## Claims

### Claim 1

A proton-conductive membrane, comprising:
a crosslinked polymer and a plasticizer,
wherein the crosslinked polymer includes a proton acceptor group in an amount equal to 10 mol % or more of repeating units constituting the crosslinked polymer,
wherein the plasticizer includes a proton donor compound having a pKa value 2.5 or less, and
wherein the proton-conductive membrane is a viscoelastic solid in a temperature range of 50° C. to 120° C.

### Claim 2 (depends on 1)

The proton-conductive membrane according to claim 1, wherein when the total of the crosslinked polymer and the plasticizer is 100 parts by mass, the content of the plasticizer is 60 parts by mass to 90 parts by mass.

### Claim 3 (depends on 1)

The proton-conductive membrane according to claim 1, wherein the proton donor compound is one or more selected from sulfuric acid and phosphoric acid.

### Claim 4 (depends on 1)

The proton-conductive membrane according to claim 1, wherein the proton acceptor group is a nitrogen-containing heterocyclic group.

### Claim 5 (depends on 1)

The proton-conductive membrane according to claim 1, wherein the glass transition point of the proton-conductive membrane is 30° C. or less.

### Claim 6 (depends on 1)

The proton-conductive membrane according to claim 1, wherein the crosslinked polymer is a copolymer of a first monomer, which is a vinyl-based monomer including a proton acceptor group, and a second monomer, which is a crosslinkable vinyl monomer.

### Claim 7 (depends on 1)

The proton-conductive membrane according to claim 1, wherein the proton conductivity of the proton-conductive membrane is 7.4 mS/cm or more at 50° C.

### Claim 8 (depends on 1)

The proton-conductive membrane according to claim 1, wherein the molar ratio of the proton donor compound to the proton acceptor group is in a range of 1.0 to 10.0.

### Claim 9 (depends on 1)

A fuel cell comprising the proton-conductive membrane according to claim 1.

### Claim 10

A method for the production of a proton-conductive membrane comprising a crosslinked polymer and a plasticizer,
wherein the crosslinked polymer includes a proton acceptor group in an amount equal to 10 mol % or more of repeating units constituting the crosslinked polymer,
wherein the plasticizer includes a proton donor compound having a pKa value of 2.5 or less,
wherein the proton-conductive membrane is a viscoelastic solid in a temperature range of 50° C. to 120° C., and
wherein the method comprises: polymerizing a first monomer, which is a vinyl monomer including a proton acceptor group, to obtain a precursor polymer, then adding a crosslinking agent to the precursor polymer, and then crosslinking the precursor polymer to obtain the crosslinked polymer.

### Claim 11

A method for the production of a proton-conductive membrane comprising a crosslinked polymer and a plasticizer,
wherein the crosslinked polymer includes a proton acceptor group in an amount equal to 10 mol % or more of repeating units constituting the crosslinked polymer,
wherein the plasticizer includes a proton donor compound having a pKa value of 2.5 or less,
wherein the proton-conductive membrane is a viscoelastic solid in a temperature range of 50° C. to 120° C., and
wherein the method comprises: polymerizing and crosslinking a first monomer, which is a vinyl-based monomer including a proton acceptor group, and a second monomer, which is a crosslinkable vinyl monomer, to obtain the crosslinked polymer.