# US 2019/0245196 A1 · Electrolytic copper foil for secondary battery and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245196 A1
- Document ID: US20190245196A1
- Status: Published application
- Kind: A1
- Application number: 16/343,527
- Filed: 2017-03-28
- Published: 2019-08-08
- Earliest claimed: 2016-11-11
- Assignees: Iljin Materials Co., Ltd.
- Applicants: Iljin Materials Co., Ltd.
- Inventors: Sun Hyoung Lee; Tae Jin Jo; Seul-Ki Park; Ki Deok Song
- Web page: https://patentgrep.com/patent/US20190245196A1

## CPC

- H01M 4/0407: {by coating on an electrolyte layer}
- C22C 9/00: Alloys based on copper
- C25D 1/04: Wires; Strips; Foils
- C25D 3/38: of copper
- C25D 17/12: Shape or form (C25D17/14 takes precedence)
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/66: Selection of materials
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/02: Details (of electrodes H01M4/00; of non-active parts H01M50/00)
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to an electrolytic copper foil for a secondary battery, and a method of producing the same. The electrolytic copper foil for a secondary battery exhibits a little change in a physical property caused by a difference in a crosshead speed when tensile strength and an elongation percentage of the electrolytic copper foil are measured, thereby achieving excellent charging and discharging characteristics of a battery and preventing exfoliation of an active material. The electrolytic copper foil for a secondary battery is produced from a plating solution containing Total Organic Carbon (TOC), cobalt, and iron by using a drum, in which a ratio of the TOC to the cobalt and the iron contained in the electrolytic copper foil follows Formula 1 below. TOC/(cobalt+iron)=1.3 to 1.5 [Formula 1]

## Claims

### Claim 1

An electrolytic copper foil for a secondary battery, which is produced from a plating solution containing Total Organic Carbon (TOC), cobalt, and iron by using a drum, and is coated with a negative electrode active material,
wherein a ratio of the TOC to the cobalt and the iron contained in the electrolytic copper foil follows Formula 1 below.
TOC/(cobalt+iron)=1.3 to 1.5 [Formula 1]

### Claim 2 (depends on 1)

The electrolytic copper foil of claim 1, wherein a difference in a crosshead speed for measuring tensile strength at a room temperature and 110° C. (six hours) follows Formula 2, and
a difference in a crosshead speed for measuring an elongation percentage at a room temperature and 110° C. (six hours) follows Formula 3.
(Tensile strength at 1 mm/min crosshead speed)/(Tensile strength at 50 mm/min crosshead speed)≥0.9 [Formula 2]
(Elongation percentage at 1 mm/min crosshead speed)/(Elongation percentage at 50 mm/min crosshead speed)≥0.8 [Formula 3]

### Claim 3 (depends on 1)

The electrolytic copper foil of claim 1, wherein a concentration of the TOC contained in the plating solution is equal to or larger than 100 ppm.

### Claim 4 (depends on 1)

The electrolytic copper foil of claim 1, wherein tensile strength of the electrolytic copper foil at a room temperature is 40 kgf/mm2 to 51 kgf/mm2.

### Claim 5 (depends on 1)

The electrolytic copper foil of claim 1, wherein a thickness of the electrolytic copper foil is 4 μm to 12 μm.

### Claim 6 (depends on 1)

The electrolytic copper foil of claim 1, wherein an elongation percentage of the electrolytic copper foil is 2% to 18%.

### Claim 7

A method of producing an electrolytic copper foil for a secondary battery, the method comprising:
preparing a plating solution containing copper, Total Organic Carbon (TOC), cobalt, and iron;
applying a current density of 30 Ampere per Square Deci-metre (ASD) to 150 ASD under a temperature condition of 30° C. to 70° C. and performing electroplating by using a drum; and
coating an electrolytic copper foil formed by the electroplating with a negative electrode active material,
wherein a ratio of the TOC to the cobalt and the iron contained in the electrolytic copper foil follows Formula 1 below.
TOC/(cobalt+iron)=1.3 to 1.5 [Formula 1]

### Claim 8 (depends on 7)

The method of claim 7, wherein a difference in a crosshead speed for measuring tensile strength at a room temperature and 110° C. (six hours) follows Formula 2, and
a difference in a crosshead speed for measuring an elongation percentage at a room temperature and 110° C. (six hours) follows Formula 3.
(Tensile strength at 1 mm/min crosshead speed)/(Tensile strength at 50 mm/min crosshead speed)≥0.9 [Formula 2]
(Elongation percentage at 1 mm/min crosshead speed)/(Elongation percentage at 50 mm/min crosshead speed)≥0.8. [Formula 3]

### Claim 9 (depends on 7)

The method of claim 7, wherein a concentration of the TOC contained in the plating solution is equal to or larger than 100 ppm.

### Claim 10 (depends on 7)

The method of claim 7, wherein tensile strength of the electrolytic copper foil at a room temperature is 40 kgf/mm2 to 51 kgf/mm2.

### Claim 11 (depends on 7)

The method of claim 7, wherein a thickness of the electrolytic copper foil is 4 μm to 12 μm.

### Claim 12 (depends on 7)

The method of claim 7, wherein an elongation percentage of the electrolytic copper foil is 2% to 18%.