# US 2019/0245139 A1 · Semiconductor structure and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245139 A1
- Document ID: US20190245139A1
- Status: Published application
- Kind: A1
- Application number: 16/385,756
- Filed: 2019-04-16
- Published: 2019-08-08
- Earliest claimed: 2017-02-24
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Ltd.
- Inventors: HARRY-HAK-LAY CHUANG; SHENG-HUANG HUANG; HUNG CHO WANG
- Web page: https://patentgrep.com/patent/US20190245139A1

## CPC

- H10N 50/10: Magnetoresistive devices
- H10N 50/01: Manufacture or treatment
- H10N 50/80: Constructional details
- H10N 50/85: Materials of the active region
- H10B 61/20: {comprising components having three or more electrodes, e.g. transistors}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor structure is disclosed. The semiconductor structure includes: an Nth metal layer; a bottom electrode over the Nth metal layer; a magnetic tunneling junction (MTJ) over the bottom electrode; a top electrode over the MTJ; a spacer, including: a first spacer layer including SiN with a first atom density, the first spacer layer laterally encompassing the MTJ; and a second spacer layer including SiN with a second atom density different from the first atom density, the second spacer layer laterally encompassing at least a portion of the first spacer layer; and an (N+1)th metal layer over the top electrode. A method for manufacturing a semiconductor structure is also disclosed.

## Claims

### Claim 1

A method for manufacturing a semiconductor structure, comprising:
forming a bottom electrode;
forming a magnetic tunneling junction (MTJ) layer over the bottom electrode;
blanket depositing a first spacer layer with a first temperature over the bottom electrode and the MTJ;
blanket depositing a second spacer layer with a second temperature over the first spacer layer, the second temperature being different from the first temperature;
removing a portion of the first spacer layer and a portion of the second spacer layer to expose a portion of a top surface of the bottom electrode; and
removing the exposed portion of the bottom electrode.

### Claim 2 (depends on 1)

The method of claim 1, wherein the second temperature is higher than the first temperature.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
blanket depositing an oxide layer over the second spacer layer; and
wherein the removing of the portion of the first spacer layer and the portion of the second spacer layer to expose the portion of the top surface of the bottom electrode comprises:
removing a portion of the oxide layer, the portion of the first spacer layer and the portion of the second spacer layer to expose the portion of the top surface of the bottom electrode.

### Claim 4 (depends on 1)

The method of claim 1, wherein the blanket depositing the first spacer layer comprises:
blanket depositing a SiN layer with a first atom density over the bottom electrode and the MTJ.

### Claim 5 (depends on 4)

The method of claim 4, wherein the blanket depositing the second spacer layer comprises:
blanket depositing a SiN layer with a second atom density over the first spacer layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the second atom density is greater than the first atom density.

### Claim 7 (depends on 1)

The method of claim 1, wherein the removing the portion of the first spacer layer and the portion of the second spacer layer comprises:
removing the portion of the first spacer layer and the portion of the second spacer layer to expose the first spacer layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the forming the bottom electrode comprises:
forming the bottom electrode to have an uneven thickness, wherein a thickness of the bottom electrode directly below the MTJ is greater than a thickness of the bottom electrode directly below the second spacer layer, and a diameter of a top surface of the bottom electrode is wider than a diameter of a bottom surface of the bottom electrode.

### Claim 9 (depends on 1)

The method of claim 1, wherein the removing the exposed portion of the bottom electrode comprises:
removing the exposed portion of the bottom electrode to align a sidewall of the first spacer layer, a sidewall of the second spacer layer with a sidewall of the bottom electrode.

### Claim 10

A method for manufacturing a semiconductor structure, comprising:
forming a bottom electrode;
forming a magnetic tunneling junction (MTJ) over the bottom electrode;
blanket depositing an inner SiN layer with a first dielectric constant to encompass the MTJ; and
blanket depositing an outer SiN layer with a second dielectric constant different from the first dielectric constant to encompass the inner SiN layer; and
forming a top electrode over the MTJ.

### Claim 11 (depends on 11)

The method of claim 11, wherein the second dielectric constant is greater than the first dielectric constant.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
etching a portion of the inner SiN layer and a portion of the outer SiN layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein a height of the etched inner SiN layer is greater than a height of the etched outer SiN layer.

### Claim 14 (depends on 11)

The method of claim 11, further comprising blanket depositing an oxide layer encompassing the outer SiN layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein a thickness of the inner SiN layer is greater than a thickness of the outer SiN layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein a thickness of the inner SiN layer is greater than a thickness of the oxide layer.

### Claim 17

A method for manufacturing a semiconductor structure, comprising:
forming a bottom electrode;
forming a magnetic tunneling junction (MTJ) over the bottom electrode;
blanket depositing a first spacer layer including SiN with a first dielectric constant over the MTJ; and
blanket depositing a second spacer layer including SiN with a second dielectric constant different from the first dielectric constant over the first spacer layer;
wherein a thickness of the bottom electrode directly below the MTJ is greater than a thickness of the bottom electrode directly below the second spacer layer, and a diameter of a top surface of the bottom electrode is wider than a diameter of a bottom surface of the bottom electrode.

### Claim 18 (depends on 17)

The method of claim 17, wherein the second dielectric constant is greater than the first dielectric constant.

### Claim 19 (depends on 17)

The method of claim 17, further comprising removing a portion of the first spacer layer and a portion of the second spacer layer.

### Claim 20 (depends on 17)

The method of claim 17, further comprising forming a top electrode over the MTJ.