# US 2019/0245112 A1 · Metal organic chemical vapor depostion (mocvd) tunnel junction growth in iii-nitride devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245112 A1
- Document ID: US20190245112A1
- Status: Published application
- Kind: A1
- Application number: 16/270,177
- Filed: 2019-02-07
- Published: 2019-08-08
- Earliest claimed: 2018-02-07
- Assignees: The Regents of the University of California; King Abdulaziz City for Science and Technology (KACST)
- Applicants: The Regents of the University of California
- Inventors: Abdullah Ibrahim Alhassan; James S. Speck; Steven P. DenBaars
- Web page: https://patentgrep.com/patent/US20190245112A1

## CPC

- H10H 20/0137: {the light-emitting regions comprising nitride materials}
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C30B 25/02: Epitaxial-layer growth
- C30B 25/04: Pattern deposit, e.g. by using masks
- C30B 29/406: {Gallium nitride}
- H10H 20/812: within the light-emitting regions, e.g. having quantum confinement structures
- H10H 20/8252: {characterised by the dopants}
- H10H 20/832: characterised by their material
- H10H 20/825: containing nitrogen, e.g. GaN
- H10H 20/831: characterised by their shape
- H10H 20/872: {Periodic patterns for optical field-shaping, e.g. photonic bandgap structures}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A method for fabricating an (Al,Ga,In,B)N or III-nitride semiconductor device, including performing a growth of III-nitride or (Al,Ga,In,B)N material including a p-n junction with an active region and using metal-organic chemical vapor deposition (MOCVD) or chemical vapor deposition; and performing a subsequent regrowth of n-type (Al,Ga,In,B)N or III-nitride material using MOCVD or chemical vapor deposition while utilizing a pulsed delta n-type doping scheme to realize an abrupt, smoother surface of the n-type material and a higher carrier concentration in the n-type material. In another example, the method comprises forming a mesa having a top surface; and activating magnesium in the p-type GaN of the (Al,Ga,In,B)N material through openings in the top surface that expose the p-type GaN's surface. The openings are formed before or after the subsequent regrowth of the tunnel junction.

## Claims

### Claim 1

A device, comprising:
a mesa including:
a III-nitride p-n junction, the p-n junction including an active region between a first p-type layer and a first n-type layer; and
a III-nitride region patterned on the III-nitride p-n junction, the III-nitride region including a second n-type layer, a second p-type layer, and a tunnel junction formed at an interface between the second n-type layer and the second p-type layer; and
an array of openings in the III-nitride region exposing the second p-type layer on a top surface of the mesa; and wherein the mesa has one or more lateral dimensions that are larger than 50 μm.

### Claim 2 (depends on 1)

The device of claim 1, wherein each of the openings have a width W and 0.1 μm≤W≤100 μm.

### Claim 3 (depends on 3)

The device of claim 3, wherein a spacing S between the openings is 0.5 μm≤S≤400 μm.

### Claim 4 (depends on 1)

The device of claim 1, further comprising a patterned dielectric on a top surface of the mesa, wherein the patterned dielectric comprises the openings exposing the second p-type layer.

### Claim 5 (depends on 1)

The device of claim 1, wherein the first p-type layer, the second p-type layer, the first n-type layer, and the second n-type layer comprise GaN.

### Claim 6 (depends on 1)

The device of claim 1, wherein the second n-type layer comprises an n-type GaN layer having an n-type dopant concentration of at least 1.1E20 cm−3.

### Claim 7 (depends on 1)

The device of claim 1, wherein the interface has a surface roughness of 2.2 nm or less over an area of 5 micrometers by 5 micrometers.

### Claim 8 (depends on 1)

The device of claim 1, wherein:
a current density of at least 5 A/cm2 flows in response to a voltage of 2.5 V applied across the device between a first metal contact to the first n-type layer and a second metal contact to the second n-type layer, and
the device outputs light with a power of at least 0.5 mW in response to a current density of 2.25 A/cm2 flowing between the first metal contact and the second metal contact.

### Claim 9

A method for fabricating a III-nitride semiconductor device, comprising:
growing a III-nitride p-n junction with an active region and using metal-organic chemical vapor deposition (MOCVD) or chemical vapor deposition, the III-nitride p-n junction including the active region between a p-type layer and an n-type layer; and
growing subsequent III-nitride material including an n-type material using MOCVD or chemical vapor deposition, utilizing a pulsed delta n-type doping scheme to realize an abrupt, smoother surface of the n-type material and a higher carrier concentration in the n-type material; and
wherein the subsequent III-nitride material forms a tunnel junction.

### Claim 10 (depends on 9)

The method of claim 9, wherein the pulsed delta n-type doping scheme is used at a regrowth interface with the p-n junction or for the entire growth of the subsequent III-nitride material including the tunnel junction.

### Claim 11 (depends on 10)

The method of claim 10, wherein the pulsed delta n-type doping scheme is achieved by injecting a precursor containing n-type dopant for 40 seconds or less per cycle and forms a continuous layer growth by keeping the precursors comprising Group V and Group III precursors uninterrupted.

### Claim 12 (depends on 10)

The method of claim 10, wherein the pulsed delta n-type doping scheme is achieved by injecting precursors containing n-type dopant and Group V/III materials for a period of time in cycles.

### Claim 13

A method for fabricating a semiconductor device, comprising:
growing a III-nitride p-n junction with an active region using metal-organic chemical vapor deposition (MOCVD) and/or chemical vapor deposition (CVD), wherein the III-nitride p-n junction includes a first p-type layer, a first n-type layer, and the active region between the first n-type layer and the first p-type layer;
growing a subsequent III-nitride material comprising a second p-type layer using MOCVD or chemical vapor deposition (CVD);
forming a mesa in the III-nitride p-n junction and the subsequent III-nitride material, wherein the mesa has one or more lateral dimensions that are larger than 50 μm; and
reactivating or activating a second p-type layer in the subsequent III-nitride material through lateral and vertical diffusion of hydrogen through the mesa's sidewalls and top surface; and
wherein the subsequent III-nitride material forms a tunnel junction.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first n-type layer in the p-n junction and the active region are grown using the MOCVD, and the first p-type layer, the second p-type layer, and the tunnel junction are grown using the CVD.

### Claim 15 (depends on 13)

The method of claim 13, wherein delta-doping is used at a regrowth interface between the III-nitride p-n junction and the subsequent III-nitride material.

### Claim 16 (depends on 13)

The method of claim 13, wherein the subsequent III-nitride material forms layers of III-nitride material and a magnesium (Mg) concentration in the layers of the III-nitride material is suppressed through exposure to an acid or through flow modulation epitaxy.

### Claim 17 (depends on 13)

The method of claim 13, wherein the reactivating or the activating activates magnesium (Mg) through the lateral and vertical diffusion of hydrogen through the sidewalls and the top surface at an elevated temperature above 800 degrees Celsius.

### Claim 18 (depends on 13)

The method of claim 13, wherein the activating or the reactivating through the top surface occurs through openings that expose a surface of the second p-type layer comprising a p-type GaN layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein a width of the openings is between about 0.1 μm to about 100 μm wide and a spacing between each of the openings is about 0.5 μm to about 400 μm.

### Claim 20 (depends on 18)

The method of claim 18, wherein the first p-type layer and the second p-type layer comprise p-GaN and the openings are formed before the subsequent III-nitride material including the tunnel junction by first depositing a pattern of a dielectric on a surface of the first p-GaN layer such that the subsequent III-nitride material occurs selectively only on the exposed area of the first p-type layer.