# US 2019/0245111 A1 · Ultra-Thin Flexible Rear-Contact Si Solar Cells and Methods for Manufacturing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245111 A1
- Document ID: US20190245111A1
- Status: Published application
- Kind: A1
- Application number: 16/264,845
- Filed: 2019-02-01
- Published: 2019-08-08
- Earliest claimed: 2018-02-02
- Assignees: The Government of the United States of America, as represented by the Secretary of the Navy
- Applicants: The Government of the United States of America, as represented by the Secretary of the Navy
- Inventors: Woojun Yoon; David Scheiman; Phillip Jenkins; Robert J. Walters
- Web page: https://patentgrep.com/patent/US20190245111A1

## CPC

- H10F 71/129: {Passivating}
- H10F 10/146: {Back-junction photovoltaic cells, e.g. having interdigitated base-emitter regions on the back side}
- H10F 71/00: Manufacture or treatment of devices covered by this subclass (patterning processes to connect thin photovoltaic cells in integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/33; manufacture or treatment of encapsulations or containers for integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/80; manufacture or treatment of integrated devices, or assemblies of multiple devices, comprising at least one element in which radiation controls the flow of current H10F39/00)
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/139: {using temporary substrates}
- H10F 77/219: {Arrangements for electrodes of back-contact photovoltaic cells}
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for making an ultra-thin, flexible crystalline silicon solar cell from thick, inflexible cells. A thick, inflexible cell having a plurality of electrical contacts on the back side thereof is adhered to a mount by means of a temporary bonding adhesive tape and a thickness of the mounted stack. A thickness of the bonding tape and the back-side contacts is determined and compared to a desired thickness of the final cell. Excess material is ground from the front side of the stack to obtain a thinned stack having the desired thickness and the thinned stack is removed from the mount to produce an ultra-thin, flexible rear-contact Si solar cell having a total thickness of less than 80 μm and a bending radius of less than 20 mm. The front surface can be textured, with a passivation layer and/or a dielectric layer being deposited thereon.

## Claims

### Claim 1

A method for manufacturing an ultra-thin flexible rear-contact solar cell, comprising:
providing a pre-existing rear-contact solar cell having a Si material layer with a thickness of about 200 μm and a bending radius of about 50 mm to 60 mm,
the pre-existing solar cell having a plurality of interdigitated n- and p-doped regions on a back side thereof, a plurality of metal grids having a thickness of about 20 μm to about 40 μm forming a corresponding plurality of interdigitated metal contacts to the n- and p-doped regions on the backside of the pre-existing solar cell;
providing a temporary bonding adhesive tape comprising an adhesive layer on a carrier support film, the temporary bonding adhesive tape having a thickness of about 300 μm to 500 μm;
mounting the pre-existing solar cell to the temporary bonding adhesive tape to form a mounted stack that includes the pre-existing solar cell, the metal grids, and the temporary bonding adhesive tape;
measuring a thickness of the mounted stack, comparing the thickness of the mounted stack to a predetermined thickness of a desired final solar cell, and determining a thickness of material to be removed from the pre-existing solar cell to achieve the predetermined desired thickness of the final solar cell;
grinding a front side of the pre-existing solar cell to remove material from the Si material layer to produce a thinned solar cell preferably having a Si material layer with a thickness of about 10 μm to about 20 μm, and more preferably having a Si materials layer with a thickens of about 1 μm to about 10 μm, wherein the mounted stack has a thickness equal to the predetermined desired thickness of the solar cell plus the thickness of metal grids and the thickness of the temporary bonding adhesive tape; and
heating the stack with the thinned solar cell to a melting point of the adhesive in the temporary bonding adhesive tape, the thinned solar cell immediately disengaging from the temporary bonding adhesive tape when the melting point of the adhesive is reached;
wherein the final solar cell has a thickness of less than about 60 μm, more preferably has a thickness of less than about 50 μm and a bending radius of less than 20 mm, and more preferably of less than 10 mm.

### Claim 2 (depends on 1)

The method according to claim 1, further including the steps of chemically etching the front surface of the final solar cell to form a textured front surface.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the textured front surface comprises a plurality of random upright pyramids.

### Claim 4 (depends on 2)

The method according to claim 2, further including the step of depositing a passivating semiconductor material layer onto the textured front surface of the final solar cell.

### Claim 5 (depends on 2)

The method according to claim 2, w herein the passivating semiconductor material layer has a thickness of about 1 nm to about 20 nm.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the Si material layer is n-doped, and further wherein the passivating semiconductor material layer is an n-type semiconductor layer.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the passivating semiconductor material layer comprises TiOx, or hydrogenated amorphous Si doped with phosphorus.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the Si material layer is p-doped, and further wherein the passivating semiconductor material layer is an p-type semiconductor layer.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the passivating semiconductor material layer comprises MoOx, NiOx, or hydrogenated amorphous Si doped with boron.

### Claim 10 (depends on 2)

The method according to claim 2, further including the step of depositing one or more layers of dielectric material as an anti-reflective coating on the textured front surface of the final solar cell.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the dielectric material comprises Al2O3, SiO2, SiNx, SiONx, or MgF.