# US 2019/0245074 A1 · Semiconductor structure, hemt structure and method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245074 A1
- Document ID: US20190245074A1
- Status: Published application
- Kind: A1
- Application number: 16/390,543
- Filed: 2019-04-22
- Published: 2019-08-08
- Earliest claimed: 2016-06-03
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Ltd.
- Inventors: YAO-CHUNG CHANG; PO-CHIH CHEN; JIUN-LEI JERRY YU; CHUN LIN TSAI
- Web page: https://patentgrep.com/patent/US20190245074A1

## CPC

- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 30/014: {of FETs having zero-dimensional [0D] or one-dimensional [1D] channels, e.g. quantum wire FETs, single-electron transistors [SET] or Coulomb blockade transistors}
- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/021: {of FETs having insulated gates [IGFET]}
- H10D 30/47: having two-dimensional [2D] charge carrier gas channels, e.g. nanoribbon FETs or high electron mobility transistors [HEMT]
- H10D 30/472: {having lower bandgap active layer formed on top of wider bandgap layer, e.g. inverted HEMT}
- H10D 30/473: {having confinement of carriers by multiple heterojunctions, e.g. quantum well HEMT}
- H10D 30/4732: {using Group III-V semiconductor material}
- H10D 30/4755: {having wide bandgap charge-carrier supplying layers, e.g. modulation doped HEMTs such as n-AlGaAs/GaAs HEMTs}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D 62/852: being Group III-V materials comprising three or more elements, e.g. AlGaN or InAsSbP
- H10P 95/904: {of Group III-V semiconductors}
- H10D 64/68: characterised by the insulator, e.g. by the gate insulator
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor structure includes: a channel layer; an active layer over the channel layer, wherein the active layer is configured to form a two-dimensional electron gas (2DEG) to be formed in the channel layer along an interface between the channel layer and the active layer; a gate electrode over a top surface of the active layer; and a source/drain electrode over the top surface of the active layer; wherein the active layer includes a first layer and a second layer sequentially disposed therein from the top surface to a bottom surface of the active layer, and the first layer possesses a higher aluminum (Al) atom concentration compared to the second layer. An HEMT structure and an associated method are also disclosed.

## Claims

### Claim 1

A method for forming a semiconductor structure, comprising:
providing a channel layer having an active layer formed thereon;
performing an anneal upon the top surface of the active layer with a first temperature;
depositing an aluminum nitride (AlN) film over the top surface of the active layer; and
performing an anneal upon the AlN film with a second temperature, and the second temperature is higher than the first temperature.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
wet cleaning the top surface of the active layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein performing the anneal upon the AlN comprises
performing the anneal upon the AlN film to diffuse Al atoms from the AlN film into the active layer, wherein a concentration of Al in the AlN film is higher than a concentration of Al in the active layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the performing the anneal upon the top surface of the active layer comprises:
supplying a nitrogen-based ambient atmosphere to the top surface of the active layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the deposition of the AlN film over the active layer comprises:
depositing the AlN film over the active layer through an atomic layer deposition (ALD).

### Claim 6 (depends on 1)

The method of claim 1, wherein the deposition of the AlN film over the active layer comprises:
blanket depositing the AlN film over the active layer to a thickness of about the length of 3 to 20 Al atoms.

### Claim 7 (depends on 3)

The method of claim 3, wherein a ratio of the concentration of Al in the AlN film to the concentration of Al in the active layer is from about 1.1 to 2.5.

### Claim 8

A method for forming a semiconductor structure, comprising:
providing a channel layer having an active layer formed thereon;
supplying a nitrogen-based ambient atmosphere to the top surface of the active layer;
depositing an aluminum nitride (AlN) film over the top surface of the active layer; and
performing an anneal upon the AlN film.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
wet cleaning the top surface of the active layer.

### Claim 10 (depends on 8)

The method of claim 8, wherein performing the anneal upon the AlN film comprises:
performing the anneal upon the AlN film with a second temperature, and the second temperature is higher than the first temperature.

### Claim 11 (depends on 8)

The method of claim 8, wherein performing the anneal upon the AlN film comprises
performing the anneal upon the AlN film to diffuse Al atoms from the AlN film into the active layer, wherein a concentration of Al in the AlN film is higher than a concentration of Al in the active layer.

### Claim 12 (depends on 8)

The method of claim 8, wherein the deposition of the AlN film over the active layer comprises:
depositing the AlN film over the active layer through an atomic layer deposition (ALD).

### Claim 13 (depends on 8)

The method of claim 8, wherein the deposition of the AlN film over the active layer comprises:
blanket depositing the AlN film over the active layer to a thickness of about the length of 3 to 20 Al atoms.

### Claim 14 (depends on 11)

The method of claim 11, wherein a ratio of the concentration of Al in the AlN film to the concentration of Al in the active layer is from about 1.1 to 2.5.

### Claim 15

A method for forming a semiconductor structure, comprising:
providing a channel layer having an active layer formed thereon;
performing a surface treatment upon a top surface of the active layer;
depositing an aluminum nitride (AlN) film over the top surface of the active layer; and
performing an anneal upon the AlN film to diffuse Al atoms from the AlN film into the active layer, wherein a concentration of Al in the AlN film is higher than a concentration of Al in the active layer.

### Claim 16 (depends on 15)

The method of claim 15, further comprising:
forming a gate structure over the active layer.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
forming a source electrode and a drain electrode on each side of the gate structure, respectively.

### Claim 18 (depends on 16)

The method of claim 16, wherein the forming the gate structure over the active layer comprises:
forming the gate structure over and in contact with the high Al diffusion layer.

### Claim 19 (depends on 15)

The method of claim 15, wherein the deposition of the AlN film over the active layer comprises:
depositing the AlN film over the active layer through an atomic layer deposition (ALD).

### Claim 20 (depends on 15)

The method of claim 15, wherein the deposition of the AlN film over the active layer comprises:
blanket depositing the AlN film over the active layer to a thickness of about the length of 3 to 20 Al atoms.