# US 2019/0245069 A1 · Lateral insulated-gate bipolar transistor and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245069 A1
- Document ID: US20190245069A1
- Status: Published application
- Kind: A1
- Application number: 16/311,276
- Filed: 2017-06-21
- Published: 2019-08-08
- Earliest claimed: 2016-06-21
- Assignees: Csmc Technologies Fab2 Co., Ltd.
- Applicants: Csmc Technologies Fab2 Co., Ltd.
- Inventors: Shukun QI
- Web page: https://patentgrep.com/patent/US20190245069A1

## CPC

- H10D 12/411: {Insulated-gate bipolar transistors [IGBT]}
- H10D 12/00: Bipolar devices controlled by the field effect, e.g. insulated-gate bipolar transistors [IGBT]
- H10D 12/031: {of IGBTs}
- H10D 12/421: {on insulating layers or insulating substrates, e.g. thin-film IGBTs}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 62/142: {Anode regions of thyristors or collector regions of gated bipolar-mode devices}
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10D 64/231: {Emitter or collector electrodes for bipolar transistors}
- H10D 62/107: {Buried supplementary regions, e.g. buried guard rings (multi-RESURF H10D62/111)}
- H10D 64/117: {Recessed field plates, e.g. trench field plates or buried field plates}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A lateral insulated-gate bipolar transistor and a manufacturing method therefor. The lateral insulated-gate bipolar transistor comprises a substrate, an anode terminal and a cathode terminal on the substrate, and a drift region and a gate electrode located between the anode terminal and the cathode terminal. The anode terminal comprises an N-shaped buffer zone on the substrate, a P well in the N-shaped buffer zone, an N+ zone in the P well, a groove located above the N+ zone and partially encircled by the P well, polycrystalline silicon in the groove, P+ junctions at two sides of the groove, and N+ junctions at two sides of the P+ junctions.

## Claims

### Claim 1

A lateral insulated-gate bipolar transistor, comprising:
a substrate;
a cathode terminal located on the substrate;
an anode terminal located on the substrate, the anode terminal comprising an N-type buffer region located on the substrate, a P well located in the N-type buffer region, an N+ region located in the P well, a trench located above the N+ region and partially surrounded by the P well, a polysilicon located in the trench, P+ junctions located at both sides of the trench, and N+ junctions located at both sides of the P+ junction;
a drift region located between the anode terminal and the cathode terminal; and
a gate located between the anode terminal and the cathode terminal.

### Claim 2 (depends on 1)

The lateral insulated-gate bipolar transistor according to claim 1, wherein the trench is a structure gradually increased in width from bottom to top to form a slope and having a narrow bottom and a wide top.

### Claim 3 (depends on 1)

The lateral insulated-gate bipolar transistor according to claim 1, wherein a dopant concentration of the N-type buffer region is less than a dopant concentration of the P well, and the dopant concentration of the P well is less than dopant concentrations of the P+ junction and the N+ junction.

### Claim 4 (depends on 3)

The lateral insulated-gate bipolar transistor according to claim 3, wherein the dopant concentration of the N-type buffer region ranges from 2E15 to 5E15 cm−3, the dopant concentration of the P well ranges from 4E17 to 8E17 cm−3, and the dopant concentrations of the P+ junction and the N+ junction range from 5E20 to 10E20 cm−3.

### Claim 5 (depends on 1)

The lateral insulated-gate bipolar transistor according to claim 1, wherein the anode terminal further comprises an oxide layer located on an inner surface of the trench, the oxide layer comprises an oxide film located on a sidewall of the trench and a spacer structure located at both sides of a bottom of the trench, the oxide layer has a void at a position corresponding to a middle portion of the bottom of the trench, such that the polysilicon is in direct contact with the N+ region below.

### Claim 6 (depends on 1)

The lateral insulated-gate bipolar transistor according to claim 1, wherein a dopant concentration of the polysilicon ranges from 1E21 to 10E22 cm−3.

### Claim 7 (depends on 1)

The lateral insulated-gate bipolar transistor according to claim 1, wherein the lateral insulated-gate bipolar transistor is a silicon-on-insulator type lateral insulated-gate bipolar transistor; the lateral insulated-gate bipolar transistor further comprises a buried oxide layer located between the substrate and the drift region; the substrate is a P-type substrate, and the drift region is an N-type drift region.

### Claim 8

A method of manufacturing a lateral insulated-gate bipolar transistor, comprising:
implanting N-type ions into a silicon wafer, and performing a drive-in to form an N-type buffer region;
depositing a hard mask layer on a surface of the silicon wafer, and performing trench lithography and etching using a photoresist to etch the hard mask layer to form a trench window;
etching silicon below the trench window to form a trench;
performing a liner oxidation to form a liner oxide layer on an inner surface of the trench; wherein
a thickness of the liner oxide layer at a sidewall of the trench is greater than a thickness of the liner oxide layer at a bottom of the trench;
implanting P-type ions through the trench window, and the ions pass through the oxide layer and form a P well within an N-type buffer region around the trench;
depositing an oxide layer in the trench, and forming an oxide film on the sidewall of the trench and a spacer structure at both sides of the bottom of the trench after etching the oxide layer;
implanting N-type ions into the trench, and forming an N+ region by a self-aligned implantation under a blocking of the oxide film and the spacer;
depositing a polysilicon in the trench, peeling off the hard mask layer after etching the polysilicon;
performing annealing to the P well and the N+ region; and
forming P+ junctions at both sides of the trench and N+ junctions at both sides of the P+ junction by lithography and etching.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the hard mask layer is a silicon nitride layer.

### Claim 10 (depends on 8)

The method according to claim 8, wherein during the step of depositing the oxide layer in the trench, and forming the oxide film on the sidewall of the trench and the spacer structure at both sides of the bottom of the trench after etching the oxide layer, a chemical vapor deposition is performed using ethyl orthosilicate as a reactant, and an anisotropic etching is performed.

### Claim 11 (depends on 8)

The method according to claim 8, wherein, prior to the step of depositing the polysilicon in the trench, and after the step of implanting the N-type ions into the trench, the method further comprises a step of rinsing the oxide layer.

### Claim 12 (depends on 8)

The method according to claim 8, wherein during the step of implanting the P-type ions through the trench window, and the ions pass through the oxide layer and form the P well within the N-type buffer region around the trench, multiple implantations are performed to obtain a dopant concentration gradient with slower varying.

### Claim 13 (depends on 8)

The method according to claim 8, wherein a dopant concentration of the N-type buffer region is less than a dopant concentration of the P well, and the dopant concentration of the P well is less than dopant concentrations of the P+ junction and the N+ junction.

### Claim 14 (depends on 8)

The method according to claim 8, wherein a dopant concentration of the N-type buffer region ranges from 2E15 to 5E15 cm−3, a dopant concentration of the P well ranges from 4E17 to 8E17 cm−3, and dopant concentrations of the P+ junction and the N+ junction range from 5E20 to 10E20 cm−3.

### Claim 15 (depends on 8)

The method according to claim 8, wherein the lateral insulated-gate bipolar transistor is a silicon-on-insulator type lateral insulated-gate bipolar transistor; a substrate is a P-type substrate, and a drift region is an N-type drift region.

### Claim 16 (depends on 8)

The method according to claim 8, wherein prior to the step of depositing the hard mask layer on the surface of the silicon wafer, the method further comprises a step of forming a pad oxide layer.

### Claim 17 (depends on 8)

The method according to claim 8, wherein prior to the step of implanting the N-type ions into the trench, the method further comprises a step of forming a void of the oxide layer in a middle portion of the bottom of the trench; the N-type ions are implanted through the void of the oxide layer into the trench.

### Claim 18 (depends on 8)

The method according to claim 8, wherein the N+ region formed by the self-aligned implantation, the P well, and the N-type buffer region form a longitudinal vertical NPN structure.

### Claim 19 (depends on 8)

The method according to claim 8, wherein during the step of forming the P+ junctions at both sides of the trench and the N+ junctions at both sides of the P+ junction by lithography and etching, N-type ions are implanted to form the N+ junction, and P-type ions are implanted to form the P+ junction.

### Claim 20 (depends on 8)

The method according to claim 8, wherein after the step of forming the P+ junctions at both sides of the trench and the N+ junctions at both sides of the P+ junction by lithography and etching, the method further comprises a step of performing annealing to the N+ junction and the P+ junction.