# US 2019/0245049 A1 · Self-limiting fin spike removal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0245049 A1
- Document ID: US20190245049A1
- Status: Published application
- Kind: A1
- Application number: 15/890,671
- Filed: 2018-02-07
- Published: 2019-08-08
- Earliest claimed: 2018-02-07
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Kangguo Cheng; Choonghyun Lee; Juntao Li; Peng Xu
- Web page: https://patentgrep.com/patent/US20190245049A1

## CPC

- H10D 30/6219: {characterised by the source or drain electrodes}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/0243: {using dummy structures having essentially the same shapes as the semiconductor bodies, e.g. to provide stability}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 30/751: {having composition variations in the channel regions}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10W 10/0143: {comprising concurrently refilling multiple trenches having different shapes or dimensions}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a method for forming a semiconductor structure. In embodiments of the invention, the method includes laterally forming a spacer on a side of the semiconductor structure. The method further includes performing a thermal anneal on the semiconductor structure. The method further includes performing an etch to remove materials formed by the thermal anneal.

## Claims

### Claim 1

A method for forming a semiconductor structure, the method comprising:
forming a silicon fin on a silicon germanium strain relaxed buffer (SRB) layer;
laterally forming a spacer on a side of the silicon fin;
performing a thermal anneal; and
performing an etch to remove material formed by the thermal anneal;
wherein the spacer comprises germanium oxide at least partially formed on at least part of the silicon fin.

### Claim 2 (depends on 1)

The method of claim 1, wherein:
the thermal anneal is performed in an inert gas environment.

### Claim 3

(canceled)

### Claim 4 (depends on 1)

The method of claim 1, wherein:
the thermal anneal converts at least part of the silicon germanium in the SRB layer to silicon oxide.

### Claim 5 (depends on 4)

The method of claim 4, wherein:
performing the etch comprises performing on isotropic etch to remove the silicon oxide.

### Claim 6 (depends on 5)

The method of claim 5, wherein:
the isotropic etch comprises a hydrofluoric acid wet etch or dry etch.

### Claim 7 (depends on 4)

The method of claim 4, wherein:
performing the etch comprises removing a water-soluble germanium oxide using a water solution.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
filling areas of the semiconductor with a shallow trench isolation area; and
performing a recess to expose one or more fins of the semiconductor structure.

### Claim 9

(canceled)

### Claim 10

(canceled)

### Claim 11 (depends on 1)

The method of claim 1, wherein:
the thermal anneal is performed at a temperature of approximately 450 to 700 degrees Celsius.

### Claim 12 (depends on 1)

The method of claim 1, wherein:
the thermal anneal is performed in a nitrogen atmosphere.

### Claim 13 (depends on 1)

The method of claim 1, further comprising:
placing a mask over one or more fin regions; and
performing an etch of areas of the semiconductor structure exposed by the mask;
wherein the etch is configured to remove exposed shallow trench isolation material and exposed fin material.

### Claim 14

A semiconductor structure, comprising:
a substrate;
one or more fin regions contacting the substrate and extending in a first direction, the fin region at least partially comprising silicon germanium and silicon oxide converted from silicon germanium; and
a shallow trench isolation region contacting the substrate and between the one or more fin regions.

### Claim 15 (depends on 14)

The semiconductor structure of claim 14, wherein the fin region is formed by:
laterally forming a spacer on a side of the semiconductor structure, in the first direction;
performing a thermal anneal on the semiconductor structure; and
performing an etch to remove materials formed by the thermal anneal.

### Claim 16 (depends on 15)

The semiconductor structure of claim 15 wherein;
the thermal anneal is performed in an inert gas environment.

### Claim 17 (depends on 14)

The semiconductor structure of claim 14, wherein:
the spacer comprises germanium oxide and is at least partially formed on at least part of the silicon germanium fin.

### Claim 18 (depends on 17)

The semiconductor structure of claim 17, wherein:
the thermal anneal converts at least part of the silicon germanium in the fin to silicon oxide.

### Claim 19 (depends on 14)

The semiconductor structure of claim 14, wherein:
performing the etch comprises performing on isotropic etch to remove the silicon oxide.

### Claim 20

A semiconductor structure, comprising:
a substrate;
one or more fin regions each overlaying a silicon germanium strain relaxed buffer region contacting the substrate and extending in a first direction, the fin region at least partially comprising silicon germanium and silicon oxide converted from silicon germanium; and
a shallow trench isolation region contacting the substrate and between the one or more fin regions; wherein the fin region is formed by:
laterally forming a germanium oxide spacer on a side of the silicon fin region, in the first direction;
performing a thermal anneal on the semiconductor structure; and
performing an etch to remove silicon oxide and a silicon germanium area with a high percentage of germanium formed by the thermal anneal.