# US 2019/0244922 A1 · Nickel-tin microbump structures and method of making same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0244922 A1
- Document ID: US20190244922A1
- Status: Published application
- Kind: A1
- Application number: 16/386,195
- Filed: 2019-04-16
- Published: 2019-08-08
- Earliest claimed: 2016-09-15
- Assignees: Intel Corporation
- Applicants: Intel Corporation
- Inventors: Rahul JAIN; Kyu Oh LEE; Amanda E. SCHUCKMAN; Steve S. CHO
- Web page: https://patentgrep.com/patent/US20190244922A1

## CPC

- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/30: Die-attach connectors
- H10W 70/695: Organic materials
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/072: {of bump connectors}
- H10W 72/07236: {Soldering or alloying}
- H10W 72/073: {of die-attach connectors}
- H10W 72/07331: {Connecting techniques}
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/354: {comprising polymers}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/725: {between a chip and a laterally-adjacent insulating package substrate, interposer or RDL}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Techniques and mechanisms for providing effective connectivity with surface level microbumps on an integrated circuit package substrate. In an embodiment, different metals are variously electroplated to form a microbump which extends through a surface-level dielectric of a substrate to a seed layer including copper. The microbump includes nickel and tin, wherein the nickel aids in mitigating an absorption of seed layer copper. In another embodiment, the microbump has a mass fraction of tin, or a mass fraction of nickel, that is different in various regions along a height of the microbump.

## Claims

### Claim 1

A method for forming microbumps on a substrate, the method comprising:
patterning a dielectric layer, wherein a copper contact is exposed by an opening formed in the dielectric layer;
performing a deposition of a seed layer on the copper contact, the seed layer comprising copper;
electroplating nickel of a first microbump directly on the seed layer; and
electroplating tin of the first microbump directly on the nickel.

### Claim 2 (depends on 1)

The method of claim 1, wherein performing the deposition of the seed layer includes performing an electroless plating of the seed layer directly on the copper contact.

### Claim 3 (depends on 1)

The method of claim 1, wherein a bottom 10% of a volume of the first microbump has a first tin mass fraction, wherein a top 10% of a volume of the first microbump has a second tin mass fraction and wherein the second tin mass fraction differs from the first tin mass fraction by at least 5% of the first tin mass fraction.

### Claim 4 (depends on 3)

The method of claim 3, wherein the second tin mass fraction differs from the first tin mass fraction by at least 10% of the first tin mass fraction.

### Claim 5 (depends on 1)

The method of claim 1, wherein a total volume of tin of the first microbump is equal to at least 75% of a total volume of nickel of the first microbump.

### Claim 6 (depends on 1)

The method of claim 1, wherein a total tin mass fraction of the first microbump is in a range of 50% to 90%.

### Claim 7 (depends on 1)

The method of claim 1, further comprising forming a surface finish on the copper contact, wherein the seed layer is deposited on the surface finish.

### Claim 8

A method of fabricating an integrated circuit (IC) package substrate, the method comprising:
forming a dielectric layer above a sub-surface-level metal layer, the sub-surface-level metal layer including copper contacts;
forming via holes in the dielectric layer, the via holes exposing the copper contacts;
forming a seed layer in the via holes and above the copper contacts, the seed layer including copper; and
forming microbumps on the seed layer, the microbumps including tin and nickel, wherein a bottom ten percent of a volume of each of the microbumps has a first tin mass fraction, wherein a top ten percent of the volume of each of the microbumps has a second tin mass, and wherein the second tin mass fraction differs from the first tin mass fraction by at least five percent of the first tin mass fraction.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
prior to forming the seed layer, forming a surface finish on the copper contacts, wherein the seed layer is formed on the surface finish.

### Claim 10 (depends on 8)

The method of claim 8, wherein the seed layer is formed directly on the copper contacts.

### Claim 11 (depends on 8)

The method of claim 8, wherein nickel of each of the microbumps is directly on the seed layer.

### Claim 12 (depends on 8)

The method of claim 8, wherein the second tin mass fraction differs from the first tin mass fraction by at least ten percent of the first tin mass fraction.

### Claim 13 (depends on 8)

The method of claim 8, wherein a total tin mass fraction of each of the microbumps is in a range of 50% to 90%.

### Claim 14

A method of fabricating an integrated circuit (IC) package substrate, the method comprising:
forming a dielectric layer above a sub-surface-level metal layer, the sub-surface-level metal layer including copper contacts;
forming via holes in the dielectric layer, the via holes exposing the copper contacts;
forming a seed layer in the via holes and above the copper contacts, the seed layer including copper; and
forming microbumps on the seed layer, the microbumps including tin and nickel, wherein a total volume of tin of each of the microbumps is equal to at least 75% of a total volume of nickel of each of the microbumps.

### Claim 15 (depends on 14)

The method of claim 14, further comprising:
prior to forming the seed layer, forming a surface finish on the copper contacts, wherein the seed layer is formed on the surface finish.

### Claim 16 (depends on 14)

The method of claim 14, wherein the seed layer is formed directly on the copper contacts.

### Claim 17 (depends on 14)

The method of claim 14, wherein nickel of each of the microbumps is directly on the seed layer.

### Claim 18 (depends on 14)

The method of claim 14, wherein a total tin mass fraction of each of the microbumps is in a range of 50% to 90%.

### Claim 19 (depends on 14)

The method of claim 14, wherein a bottom ten percent of a volume of each of the microbumps has a first tin mass fraction, wherein a top ten percent of the volume of each of the microbumps has a second tin mass, and wherein the second tin mass fraction differs from the first tin mass fraction by at least five percent of the first tin mass fraction.

### Claim 20 (depends on 19)

The method of claim 19, wherein the second tin mass fraction differs from the first tin mass fraction by at least ten percent of the first tin mass fraction.