# US 2019/0244882 A1 · Formation of Fine Pitch Traces Using Ultra-Thin PAA Modified Fully Additive Process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0244882 A1
- Document ID: US20190244882A1
- Status: Published application
- Kind: A1
- Application number: 15/887,346
- Filed: 2018-02-02
- Published: 2019-08-08
- Earliest claimed: 2018-02-02
- Assignees: Compass Technology Company Limited
- Applicants: Compass Technology Company Limited
- Inventors: Kelvin Po Leung Pun; Chee Wah Cheung
- Web page: https://patentgrep.com/patent/US20190244882A1

## CPC

- C23C 18/1651: {Two or more layers only obtained by electroless plating}
- C23C 18/1641: {Organic substrates, e.g. resin, plastic}
- C23C 18/1653: {Two or more layers with at least one layer obtained by electroless plating and one layer obtained by electroplating}
- C23C 18/1689: {After-treatment}
- C23C 18/1692: {Heat-treatment}
- C23C 18/2086: {with use of organic or inorganic compounds other than metals, first}
- C23C 18/30: Activating {or accelerating or sensitising with palladium or other noble metal}
- C23C 18/36: using hypophosphites
- C25D 3/38: of copper
- C25D 5/02: Electroplating of selected surface areas
- C25D 5/022: {using masking means}
- C25D 5/10: Electroplating with more than one layer of the same or of different metals (for bearings C25D7/10)
- C25D 5/611: {Smooth layers}
- C25D 5/617: {Crystalline layers}
- H10W 70/05: of insulating or insulated package substrates, or of interposers, or of redistribution layers (manufacture or treatment of leadframes H10W70/04)
- H10W 70/095: {of vias therein}
- H10W 70/611: {for connecting multiple chips together}
- H10W 70/635: {Through-vias}
- H10W 70/66: Conductive materials thereof
- H10W 70/685: comprising multiple insulating layers
- H10W 70/688: {Flexible insulating substrates}
- H10W 70/69: Insulating materials thereof
- H10W 99/00: Subject matter not provided for in other groups of this subclass
- H10W 72/072: {of bump connectors}
- H10W 72/07232: {Compression bonding, e.g. thermocompression bonding}
- H10W 72/073: {of die-attach connectors}
- H10W 72/075: {of bond wires}
- H10W 72/07532: {Compression bonding, e.g. thermocompression bonding}
- H10W 72/077: {Connecting of TAB connectors}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/387: {Flow barriers}
- H10W 72/5522: {comprising gold [Au]}
- H10W 72/884: {Die-attach connectors and bond wires}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/754: {between a chip and a stacked insulating package substrate, interposer or RDL}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method to produce a substrate suitable for diffusion bonding is described. A flexible dielectric substrate is provided. An alkaline modification is applied to the dielectric substrate to form a polyamic acid (PAA) anchoring layer on a surface of the dielectric substrate. A Ni—P seed layer is electrolessly plated on the PAA layer. Copper traces are plated within a photoresist pattern on the Ni—P seed layer. A surface finishing layer is electrolytically plated on the copper traces. The photoresist pattern and Ni—P seed layer not covered by the copper traces are removed to complete the substrate suitable for diffusion bonding.

## Claims

### Claim 1

A method of manufacturing a flexible substrate comprising:
providing a flexible dielectric substrate;
applying an alkaline modification to said dielectric substrrate to form a polyamic acid (PAA) anchoring layer on a surface of said dielectric substrate;
electrolessly plating a Ni—P seed layer on said PAA layer;
forming a photoresist pattern on said Ni—P seed layer;
plating copper traces within said photoresist pattern;
plating a surface finishing layer on said copper traces; and
removing said photoresist pattern and etching away said Ni—P seed layer not covered by said copper traces to complete said flexible substrate.

### Claim 2 (depends on 1)

The method according to claim 1 wherein said dielectric substrate comprises: any kind of polyimide (PI), including Kapton PI or Upisel PI, or liquid crystal polymer (LCP).

### Claim 3 (depends on 1)

The method according to claim 1 wherein said alkaline modification comprises applying a KOH/alkaline base chemical to said dielectric substrate wherein said PAA layer has a thickness of less than 100 nm and preferably less than 10 nm.

### Claim 4 (depends on 1)

The method according to claim 1 further comprising depositing a catalyst layer comprising Palladium (Pd) or Nickel (Ni) on said PAA layer by immersion into an ionic metal solution to activate said PAA layer for subsequent electroless Ni—P seed layer plating.

### Claim 5 (depends on 1)

The method according to claim 1 wherein said electrolessly plating said Ni—P seed layer is an autocatalytic process and wherein said Ni—P seed layer has a thickness of 0.1 μm+/−10% and a composition of Ni: 96.5˜97.5 wt % and P: 2.5˜3.5 wt %.

### Claim 6 (depends on 1)

The method according to claim 1 wherein said forming said photoresist pattern comprises:
applying a photoresist on said Ni—P seed layer; and
exposing and developing said photoresist to form a pattern for fine pitch traces for circuitization.

### Claim 7 (depends on 1)

The method according to claim 1 further comprising annealing said substrate after forming said Ni—P seed layer preferably at 200° C. for at least ten minutes to at most 2 hours.

### Claim 8 (depends on 1)

The method according to claim 1 wherein said plating said copper traces comprises electrolytically plating copper to a thickness of between about 2 to 18 μm wherein a ratio of the top to bottom widths of said copper traces is close to 1, wherein an elongation strength of said copper traces is over 15%, wherein a tensile strength of said copper traces is between about 290 and 340 N/mm2, and wherein a hardness of said copper traces is 100 in vicker hardness with a purity of more than 99.9%.

### Claim 9 (depends on 1)

The method according to claim 1 wherein said surface finishing layer comprises electrolytic Ni/Au, electroless Nickel/Immersion gold (ENIG), Electroless Nickel/Electroless Palladium/Immersion Gold (ENEPIG), electrolytic Palladium, electrolytic Titanium, electrolytic Tin, electrolytic Rhodium, Electroless Palladium/Autocatalytic Gold (EPAG), or Immersion Gold/Electroless Palladium/Immersion Gold (IGEPIG).

### Claim 10

A method of manufacturing a flexible substrate comprising:
providing a flexible dielectric substrate;
laser drilling at least one first via opening all the way through said dielectric substrate;
applying an alkaline modification to said dielectric substrate to form a first polyamic acid (PAA) anchoring layer on top and bottom surfaces of said dielectric substrate;
electrolessly plating a first Ni—P seed layer on top and bottom of said first PAA layers;
forming a first photoresist pattern on top and bottom of said first Ni—P seed layers;
plating first copper traces within said first photoresist patterns and through said at least one first via opening;
plating a surface finishing layer on said first copper traces; and
removing said first photoresist patterns and etching away said first Ni—P seed layers not covered by said first copper traces to complete said flexible substrate.

### Claim 11 (depends on 10)

The method according to claim 10 wherein said dielectric substrate comprises: any kind of polyimide (PI), such as Kapton PI or Upisel PI, and liquid crystal polymer (LCP).

### Claim 12 (depends on 10)

The method according to claim 10 wherein said alkaline modification comprises applying a KOH/alkaline base chemical to said dielectric substrate wherein said first PAA layers have a thickness of less than 100 nm and preferably less than 10 nm.

### Claim 13 (depends on 10)

The method according to claim 10 further comprising depositing catalyst layers comprising Palladium (Pd) or Nickel (Ni) on said top and bottom PAA layers by immersion into an ionic metal solution to activate said first PAA layers for subsequent electroless Ni—P seed layer plating.

### Claim 14 (depends on 10)

The method according to claim 10 wherein said electrolessly plating said first Ni—P seed layers is an autocatalytic process and wherein said first Ni—P seed layers have a thickness of 0.1 μm+/−10% and a composition of Ni: 96.5˜97.5 wt % and P: 2.5˜3.5 wt %.

### Claim 15 (depends on 10)

The method according to claim 10 further comprising annealing said substrate after forming said first Ni—P seed layers at 200° C. for at least 10 minutes to at most 2 hours.

### Claim 16 (depends on 10)

The method according to claim 10 wherein said plating said first copper traces comprises electrolytically plating copper to a thickness of between about 2 to 18 μm wherein a ratio of the top to bottom widths of said copper traces is close to 1, wherein an elongation strength of said copper traces is over 15%, wherein a tensile strength of said copper traces is between about 290 and 340 N/mm2, wherein a hardness of said copper traces is 100 in vicker hardness with a purity of more than 99.9%, and wherein a center to center distance between two adjacent said copper traces is less than 8 μm.

### Claim 17 (depends on 10)

The method according to claim 10 wherein said surface finishing layer comprises electrolytic Ni/Au, electroless Nickel/Immersion gold (ENIG), Electroless Nickel/Electroless Palladium/Immersion Gold (ENEPIG), electrolytic Palladium, electrolytic Titanium, electrolytic Tin, electrolytic Rhodium, Electroless Palladium/Autocatalytic Gold (EPAG), or Immersion Gold/Electroless Palladium/Immersion Gold (IGEPIG).

### Claim 18

A method of manufacturing a flexible substrate comprising:
providing a flexible dielectric substrate;
laser drilling at least one first via opening all the way through said dielectric substrate;
applying an alkaline modification to said dielectric substrate to form a first polyamic acid (PAA) anchoring layer on top and bottom surfaces of said dielectric substrate;
electrolessly plating a first Ni—P seed layer on top and bottom of said first PAA layers;
forming a first photoresist pattern on top and bottom of said first Ni—P seed layers;
plating first copper traces within said first photoresist patterns and through said at least one first via opening;
removing said first photoresist patterns and etching away said first Ni—P seed layers not covered by said first copper traces;
thereafter laminating a bonding film on top and bottom surfaces of said first copper traces;
laminating a dielectric layer on top and bottom of said bonding films;
laser drilling at least one second via opening all the way through said dielectric layer and said bonding film to contact said first copper traces on top and bottom of said substrate;
thereafter applying an alkaline modification to said dielectric layers to form a second polyamic acid (PAA) anchoring layer on top and bottom surfaces of said dielectric layers and within said at least one second via openings;
electrolessly plating a second Ni—P seed layer on top and bottom of said second PAA layers;
forming a second photoresist pattern on top and bottom of said second Ni—P seed layers;
plating second copper traces within said second photoresist patterns and through said at least one second via opening;
plating a surface finishing layer on said second copper traces; and
removing said second photoresist patterns and etching away said second Ni—P seed layers not covered by said second copper traces to complete said flexible substrate.

### Claim 19 (depends on 18)

The method according to claim 18 wherein said dielectric substrate comprises: any kind of polyimide (PI), such as Kapton PI or Upisel PI, and liquid crystal polymer (LCP).

### Claim 20 (depends on 18)

The method according to claim 18 wherein said alkaline modification comprises applying a KOH/alkaline base chemical to said dielectric substrate wherein said first and second PAA layers have a thickness of less than 100 nm and preferably less than 10 nm.

### Claim 21 (depends on 18)

The method according to claim 18 further comprising depositing catalyst layers comprising Palladium (Pd) or Nickel (Ni) on said top and bottom PAA layers by immersion into an ionic metal solution to activate said first and second PAA layers for subsequent electroless Ni—P seed layer plating.

### Claim 22 (depends on 18)

The method according to claim 18 wherein said electrolessly plating said first and second Ni—P seed layers is an autocatalytic process and wherein said first and second Ni—P seed layers have a thickness of 0.1 μm+/−10% and a composition of Ni: 96.5˜97.5 wt % and P: 2.5˜3.5 wt %.

### Claim 23 (depends on 18)

The method according to claim 18 further comprising annealing said substrate after forming said first and second Ni—P seed layers at 200° C. for at least 10 minutes to at most 2 hours.

### Claim 24 (depends on 18)

The method according to claim 18 wherein said plating said first and second copper traces comprises electrolytically plating copper to a thickness of between about 2 to 18 μm wherein a ratio of the top to bottom widths of said copper traces is close to 1, wherein an elongation strength of said copper traces is over 15%, wherein a tensile strength of said copper traces is between about 290 and 340 N/mm2, wherein a hardness of said copper traces is 100 in vicker hardness with a purity of more than 99.9%, and wherein a center to center distance between two adjacent said copper traces is less than 8 μm.

### Claim 25 (depends on 18)

The method according to claim 18 wherein said surface finishing layer comprises electrolytic Ni/Au, electroless Nickel/Immersion gold (ENIG), Electroless Nickel/Electroless Palladium/Immersion Gold (ENEPIG), electrolytic Palladium, electrolytic Titanium, electrolytic Tin, electrolytic Rhodium, Electroless Palladium/Autocatalytic Gold (EPAG), or Immersion Gold/Electroless Palladium/Immersion Gold (IGEPIG).

### Claim 26

A chip on film comprising:
a flexible dielectric substrate having a first polyamic acid (PAA) anchoring layer on its top surface;
at least one first copper trace on a first Ni—P seed layer on said first PAA layer and having a surface finishing layer on a top surface of said at least one first copper trace; and
at least one die mounted on said dielectric substrate to said at least one first copper trace.

### Claim 27 (depends on 26)

The chip on film according to claim 26, further comprising:
a second PAA layer on a bottom surface of said dielectric substrate; and
at least one second copper trace on a second Ni—P seed layer on said second PAA layer wherein said first and second copper traces are interconnected through a via through said dielectric substrate.