# US 2019/0244847 A1 · Heater for semiconductor manufacturing apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0244847 A1
- Document ID: US20190244847A1
- Status: Published application
- Kind: A1
- Application number: 16/222,001
- Filed: 2018-12-17
- Published: 2019-08-08
- Earliest claimed: 2018-02-08
- Assignees: NGK Insulators, Ltd.
- Applicants: Ngk Insulators, Ltd
- Inventors: Keita YAMANA; Kazuhiro NOBORI; Kengo TORII
- Web page: https://patentgrep.com/patent/US20190244847A1

## CPC

- H10P 72/72: using electrostatic chucks
- C04B 35/581: based on aluminium nitride
- C04B 35/645: Pressure sintering
- H05B 3/10: Heating elements characterised by the composition or nature of the materials or by the arrangement of the conductor
- H05B 3/74: Non-metallic plates {, e.g. vitroceramic, ceramic or glassceramic hobs, also including power or control circuits}
- H10P 72/0432: {mainly by conduction}
- H10P 72/0434: {mainly by convection}
- H10P 72/7616: {characterised by a coating, a hardness or a material}
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3222: Aluminates other than alumino-silicates, e.g. spinel (MgAl2O4)
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3232: Titanium oxides or titanates, e.g. rutile or anatase
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/6567: Treatment time
- C04B 2235/658: Atmosphere during thermal treatment
- C04B 2235/72: Products characterised by the absence or the low content of specific components, e.g. alkali metal free alumina ceramics
- C04B 2235/721: Carbon content
- C04B 2235/723: Oxygen content
- C04B 2235/725: Metal content
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C04B 2235/81: Materials characterised by the absence of phases other than the main phase, i.e. single phase materials
- C04B 2235/95: Products characterised by their size, e.g. microceramics
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL

## Abstract

A heater for a semiconductor manufacturing apparatus, the heater includes an AlN ceramic substrate and a heating element embedded inside the AlN ceramic substrate. The AlN ceramic substrate contains O, C, Ti, Ca, and Y as impurity elements, includes an yttrium aluminate phase as a crystal phase, and has a Ti/Ca mass ratio of 0.13 or more, and a TiN phase is not detected in an XRD profile measured with Cu K-α radiation.

## Claims

### Claim 1

A heater for a semiconductor manufacturing apparatus, the heater comprising:
an AlN ceramic substrate and a heating element embedded inside the AlN ceramic substrate,
wherein the AlN ceramic substrate contains O, C, Ti, Ca, and Y as impurity elements, includes an yttrium aluminate phase as a crystal phase, and has a Ti/Ca mass ratio of 0.13 or more, and a TiN phase is not detected in an XRD profile measured with Cu K-α radiation.

### Claim 2 (depends on 1)

The heater for a semiconductor manufacturing apparatus according to claim 1,
wherein the Ti/Ca mass ratio is 0.5 or less.

### Claim 3 (depends on 1)

The heater for a semiconductor manufacturing apparatus according to claim 1,
wherein the AlN ceramic substrate has a Ti content of 18 mass ppm or more and 95 mass ppm or less.

### Claim 4 (depends on 1)

The heater for a semiconductor manufacturing apparatus according to claim 1,
wherein the AlN ceramic substrate contains YAM and YAL and has an YAM/YAL mass ratio of 2.8 or more and 5.3 or less.

### Claim 5 (depends on 1)

The heater for a semiconductor manufacturing apparatus according to claim 1,
wherein an O/C mass ratio in the AlN ceramic substrate is 48 or more and 65 or less.

### Claim 6 (depends on 1)

The heater for a semiconductor manufacturing apparatus according to claim 1,
wherein the AlN ceramic substrate has a volume resistivity of 1.0×109 Ωcm or more at 540° C.

### Claim 7 (depends on 1)

The heater for a semiconductor manufacturing apparatus according to claim 1,
wherein the AlN ceramic substrate has a flexural strength of 300 MPa or more.

### Claim 8 (depends on 1)

The heater for a semiconductor manufacturing apparatus according to claim 1,
wherein the AlN ceramic substrate has a thermal conductivity of 170 W/m·K or more.