# US 2019/0244828 A1 · Method for removing silicon oxide and integrated circuit manufacturing process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0244828 A1
- Document ID: US20190244828A1
- Status: Published application
- Kind: A1
- Application number: 16/372,849
- Filed: 2019-04-02
- Published: 2019-08-08
- Earliest claimed: 2016-10-08
- Assignees: Beijing Naura Microelectronics Equipment Co., Ltd.
- Applicants: Beijing Naura Microelectronics Equipment Co., Ltd.
- Inventors: Zhenguo MA
- Web page: https://patentgrep.com/patent/US20190244828A1

## CPC

- H10P 50/283: {by chemical means}
- H10P 70/20: {Cleaning during device manufacture}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 50/28: of insulating materials
- H10P 72/0421: {for drying etching}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/0143: {comprising concurrently refilling multiple trenches having different shapes or dimensions}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10B 41/42: Simultaneous manufacture of periphery and memory cells
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A method for removing silicon oxide from a wafer and an integrated circuit manufacturing process are provided. The method includes: introducing a dehydrated hydrogen fluoride gas and a dehydrated alcohol gas into a process chamber; mixing the dehydrated hydrogen fluoride gas with the dehydrated alcohol gas to generate gaseous etchants; allowing reactions between the etchants and the wafer in the process chamber under a high pressure maintained in the process chamber to improve an etching selectivity; and pumping out reaction products from the process chamber.

## Claims

### Claim 1

A method for removing silicon oxide from a wafer, comprising:
introducing a dehydrated hydrogen fluoride gas and a dehydrated alcohol gas into a process chamber;
mixing the dehydrated hydrogen fluoride gas with the dehydrated alcohol gas to generate gaseous etchants;
allowing reactions between the etchants and the wafer in the process chamber under a high pressure maintained in the process chamber to improve an etching selectivity; and
pumping out reaction products from the process chamber.

### Claim 2 (depends on 1)

The method according to claim 1, wherein:
the high pressure in the process chamber is about 30 torr to 300 torr.

### Claim 3 (depends on 2)

The method according to claim 2, wherein:
the high pressure in the process chamber is about 200 torr.

### Claim 4 (depends on 1)

The method according to claim 1, wherein:
a temperature in the process chamber is about 20° C. to 80° C.

### Claim 5 (depends on 4)

The method according to claim 4, wherein:
the temperature in the process chamber is about 40° C.

### Claim 6 (depends on 1)

The method according to claim 1, wherein:
a flow rate of the dehydrated hydrogen fluoride gas is about 100 sccm to 500 sccm; and
a flow rate of the dehydrated alcohol gas is about 100 sccm to 1000 sccm.

### Claim 7 (depends on 6)

The method according to claim 6, wherein:
the flow rate of the dehydrated hydrogen fluoride gas is about 150 sccm to 225 sccm; and
the flow rate of the dehydrated alcohol gas is about 200 sccm to 450 sccm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein:
a ratio of the flow rate of the dehydrated hydrogen fluoride gas to the flow rate of the dehydrated alcohol gas is about (0.8-1.2):1.

### Claim 9 (depends on 8)

The method according to claim 8, wherein:
the ratio of the flow rate of the dehydrated hydrogen fluoride gas to the flow rate of the dehydrated alcohol gas is about 1:1.

### Claim 10 (depends on 1)

The method according to claim 1, wherein:
the dehydrated alcohol gas is at least one of C1 to C8 monohydric alcohol gases.

### Claim 11 (depends on 10)

The method according to claim 10, wherein:
the dehydrated alcohol gas is at least one of methanol, ethanol, and isopropyl alcohol.

### Claim 12

An integrated circuit manufacturing process, comprising:
removing silicon oxide from a wafer by a removal method, the removal method including:
introducing a dehydrated hydrogen fluoride gas and a dehydrated alcohol gas into a process chamber;
mixing the dehydrated hydrogen fluoride gas with the dehydrated alcohol gas to generate gaseous etchants;
allowing reactions between the etchants and the wafer in the process chamber under a high pressure maintained in the process chamber to improve an etching selectivity; and
pumping out reaction products from the process chamber.

### Claim 13 (depends on 12)

The process according to claim 12, further including:
a sub-process for a profile modification of a shallow trench isolation (STI) high aspect ratio process (HARP) gap-fill deposition,
the sub-process including:
performing an HARP deposition by a chemical vapor deposition process for forming a STI structure having a certain thickness;
etching the STI structure having the certain thickness to provide an enlarged opening; and
repeatedly performing the HARP deposition and the etching of the STI structure in the enlarged opening, till a complete STI structure is formed;
wherein:
the etching of the STI structure is performed by the removal method.

### Claim 14 (depends on 12)

The process according to claim 12, further including:
a sub-process for removing a native oxide layer formed on a hard mask layer of a shallow trench isolation (STI) structure, wherein the mask layer of the STI structure is silicon nitride,
the sub-process including:
using the removal method to remove the native oxide layer on the hard mask layer of the STI structure; and
controlling an etching selectivity of the native oxide layer over a STI high aspect ratio process (HARP) deposition to remove the native oxide layer with an increased speed, avoiding excessive etching of the STI HARP deposition.

### Claim 15 (depends on 12)

The process according to claim 12, further including:
a sub-process for removing a pad oxide layer formed by oxidizing a substrate surface using a heating method, wherein the pad oxide layer is a buffer layer of a hard mask layer of a shallow trench isolation (STI) structure which is silicon nitride,
the sub-process including:
using the removal method to remove the pad oxide layer; and
controlling an etching selectivity of the pad oxide layer over a STI high aspect ratio process (HARP) deposition to remove the pad oxide layer with an increased speed, avoiding excessive etching of the STI HARP deposition.

### Claim 16 (depends on 12)

The process according to claim 12, further including:
a sub-process for removing a native oxide layer on a silicon substrate before depositing silicon germanium,
the sub-process including:
using the removal method to remove the native oxide layer on the silicon substrate, the silicon substrate is made of polysilicon; and
controlling an etching selectivity of the native oxide layer over the polysilicon to remove the native oxide layer with an increased speed, avoiding excessive damage to the silicon substrate.

### Claim 17 (depends on 12)

The process according to claim 12, further including:
a sub-process for removing a native oxide layer on a substrate surface and a polysilicon gate surface before forming a silicide,
the sub-process including:
using the removal method to remove the native oxide layer on the substrate surface and the polysilicon gate surface; and
controlling an etching selectivity of the native oxide layer over the polysilicon gate structure to remove the native oxide layer with an increased speed, avoiding excessive damage to the silicon substrate.

### Claim 18 (depends on 12)

The process according to claim 12, further including:
a shallow trench isolation (STI) recess sub-process in a 2-dimensional NAND memory manufacturing process, wherein:
the NAND memory includes:
floating gates and STI high aspect ratio process (HARP) depositions in a dense pattern region, and
control switch gates and STI HARP depositions in a sparse pattern region;
the floating gates and the control switch gates are made of polysilicon;
the STI HARP depositions in the dense and sparse pattern regions are made of silicon oxide; and
the sub-process includes:
using the removal method to remove the STI HARP depositions in the dense and sparse pattern regions; and
controlling an etching selectivity of the STI HARP depositions over the floating gate or the control switch gate to remove the STI HARP depositions with an increased speed, avoiding excessive damage to the floating gates and the control switch gates.

### Claim 19 (depends on 12)

The process according to claim 12, wherein:
a high pressure in the process chamber is about 30 torr to 300 torr.

### Claim 20 (depends on 12)

The process according to claim 12, wherein:
the dehydrated alcohol gas is at least one of C1 to C8 monohydric alcohol gases.