# US 2019/0244813 A1 · Process for producing a strained layer based on germanium-tin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0244813 A1
- Document ID: US20190244813A1
- Status: Published application
- Kind: A1
- Application number: 16/327,520
- Filed: 2017-08-23
- Published: 2019-08-08
- Earliest claimed: 2016-08-26
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Applicants: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Inventors: Vincent REBOUD; Jean-Michel HARTMANN; Alexei TCHELNOKOV; Vincent CALVO
- Web page: https://patentgrep.com/patent/US20190244813A1

## CPC

- H10P 14/2906: {including tin}
- H10D 30/791: {Arrangements for exerting mechanical stress on the crystal lattice of the channel regions}
- H10D 30/796: {having memorised stress for introducing strain in the channel regions, e.g. recrystallised polysilicon gates}
- H10D 64/0135: {by deposition of a layer, e.g. metal, metal compound or polysilicon, followed by transformation thereof into the insulator}
- H10D 64/01352: {with sacrificial oxide}
- H10H 20/01: Manufacture or treatment
- H10P 14/2902: {being Group IVA materials}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3404: {being Group IVA materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3412: {including tin}
- H10P 14/38: {characterised by treatments done after the formation of the materials}
- H10P 14/6304: {Formation by oxidation, e.g. oxidation of the substrate}
- H10P 14/6308: {of Group IV semiconductors}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

The invention pertains to a process for producing a strained layer based on germanium-tin (GeSn). The process includes a step of producing a semiconductor stack containing a layer based on GeSn and having an initial strain value that is non-zero; a step of structuring the semiconductor stack so as to form a structured portion and a peripheral portion, the structured portion including a central section linked to the peripheral portion by at least two lateral sections having an average width greater than an average width of the central section; and a step of suspending the structured portion, the central section then having a final strain value higher than the initial value.

## Claims

### Claim 1

A process for producing a tensionally strained layer based on germanium-tin, the process comprising:
a) producing a semiconductor stack resting on a supporting layer via a sacrificial layer, said semiconductor stack comprising a nucleation layer and a layer based on germanium-tin grown epitaxially from the nucleation layer, said semiconductor stack having a non-zero initial value of tensile stress;
b) structuring said semiconductor stack so as to form:
a structured part and a peripheral part, the structured part comprising a central portion joined to the peripheral part by at least two lateral portions opposite one another with respect to the central portion, and
the lateral portions having an average width greater than an average width of the central portion; and
c) suspending the structured part by etching the sacrificial layer located beneath the structured part, the suspended central portion then having a final value of tensile stress greater than the initial value.

### Claim 2 (depends on 1)

The process as claimed in claim 1, further comprising:
prior to the producing a), estimating a value of atomic proportion of tin and a first minimum value of tensile stress for which the layer based on germanium-tin has a direct electronic band structure; and
determining the semiconductor stack comprising the nucleation layer and said estimated layer based on germanium-tin, and having a second minimum value of tensile stress;
producing said semiconductor stack in such a way that it has said non-zero initial value of tensile stress and so that the layer based on germanium-tin has an initial value lower than said first minimum value;
determining the structuring in such a way that, after said suspending c), the central portion of the structured part has a final value of tensile stress greater than or equal to said second minimum value, said layer based on germanium-tin then having a final value of tensile stress greater than or equal to said first minimum value and then having a direct electronic band structure.

### Claim 3 (depends on 1)

The process as claimed in claim 1, wherein the nucleation layer is made of a semiconductor compound having a natural lattice parameter lower than that of the material of the layer based on germanium-tin.

### Claim 4 (depends on 1)

The process as claimed in claim 1, wherein the semiconductor stack comprises at least one layer located between the layer based on germanium-tin and the nucleation layer and made of a semiconductor compound having a natural lattice parameter less than or equal to that of the material of the layer based on germanium-tin.

### Claim 5 (depends on 1)

The process as claimed in claim 1, wherein the semiconductor stack has a thickness less than a critical thickness.

### Claim 6 (depends on 1)

The process as claimed in claim 1, wherein each layer of the semiconductor stack has a thickness less than a critical thickness.

### Claim 7 (depends on 1)

The process as claimed in claim 1, wherein the semiconductor stack comprises an upper and a lower layers based on germanium-tin, which are doped according to different types of conductivity and located on either side of the layer based on germanium-tin, which is not doped intentionally.

### Claim 8 (depends on 7)

The process as claimed in claim 7, wherein, between the upper and lower doped layers on the one hand and the layer based on germanium-tin on the other hand, there is at least one barrier layer based on germanium, or based on germanium-tin whose atomic proportion of tin is lower than an atomic proportion of tin in the layer based on germanium-tin.

### Claim 9 (depends on 1)

The process as claimed in claim 1, wherein an atomic proportion of tin in the layer based on germanium-tin is below 10%.

### Claim 10 (depends on 1)

The process as claimed in claim 1, further comprising
contacting the structured part with a freed surface of the supporting layer, so as to make the structured part integral with the supporting layer by molecular bonding.

### Claim 11 (depends on 10)

The process as claimed in claim 10, further comprising:
determining a minimum value of molecular bonding energy of the structured part on the supporting layer, as well as a minimum value of bonded surface area of the lateral portions, these minimum values being such that said energy of molecular bonding is greater than an elastic energy of the structured part;
consolidation annealing at an annealing temperature such that the energy of molecular bonding has a value greater than or equal to said previously determined minimum value; and then
etching a distal part of the lateral portions with respect to the central portion, in such a way that the bonded surface of the lateral portions has a value greater than or equal to said previously determined minimum value.

### Claim 12 (depends on 11)

The process as claimed in claim 11, wherein
said suspending and said contacting are carried out by etching the sacrificial layer with HF in a vapor phase optionally followed by deposition and then evaporation of a liquid between the suspended structured part and the supporting layer, and
in said consolidation annealing, the annealing temperature is greater than or equal to 200° C.

### Claim 13 (depends on 11)

The process as claimed in claim 11, wherein,
in said suspending, oxidation or nitriding of a freed surface of the supporting layer as well as of a lower surface of the structured part oriented towards the free surface is performed, and
in said consolidation annealing, the annealing temperature is greater than or equal to 100° C.

### Claim 14 (depends on 13)

The process as claimed in claim 13, wherein, at the end of said suspending, dielectric layers resulting from the oxidation or nitriding are formed at the level of the structured part and of the supporting layer.

### Claim 15 (depends on 1)

A process for producing a microelectronic or an optoelectronic device comprising a tensionally strained layer based on germanium-tin obtained by the process as claimed in claim 1, the process comprising:
producing a p-n junction in the tensionally strained layer, or a p-i-n junction at the level of the tensionally strained layer, the latter then not being doped intentionally.