# US 2019/0244803 A1 · Method of post-deposition treatment for silicon oxide film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0244803 A1
- Document ID: US20190244803A1
- Status: Published application
- Kind: A1
- Application number: 15/890,037
- Filed: 2018-02-06
- Published: 2019-08-08
- Earliest claimed: 2018-02-06
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Toshiya Suzuki
- Web page: https://patentgrep.com/patent/US20190244803A1

## CPC

- H10P 14/6532: {by exposure to a plasma}
- C23C 16/402: {Silicon dioxide}
- H01J 37/32192: {Microwave generated discharge (H01J37/32357, H01J37/32366, H01J37/32394, H01J37/32403 take precedence)}
- H01J 37/3222: {Antennas}
- H01J 37/32623: {Mechanical discharge control means}
- H10B 69/00: Erasable-and-programmable ROM [EPROM] devices not provided for in groups H10B41/00 - H10B63/00, e.g. ultraviolet erasable-and-programmable ROM [UVEPROM] devices
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6687: {the compound comprising silicon and nitrogen}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 50/283: {by chemical means}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- C23C 16/401: {containing silicon}
- C23C 16/56: After-treatment
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A method of post-deposition treatment for silicon oxide film includes: providing in a reaction space a substrate having a recess pattern on which a silicon oxide film is deposited; supplying a reforming gas for reforming the silicon oxide film to the reaction space in the absence of a film-forming precursor, said reforming gas being composed primarily of He and/or H2; and irradiating the reforming gas with microwaves in the reaction space having a pressure of 200 Pa or less to generate a direct microwave plasma to which the substrate is exposed, thereby reforming the silicon oxide film.

## Claims

### Claim 1

A method of post-deposition treatment for silicon oxide film, which is conducted upon completion of all deposition processes of the silicon oxide film and comprises:
(i) providing in a reaction space a substrate on which the silicon oxide film is deposited;
(ii) supplying a reforming gas for reforming the silicon oxide film to the reaction space in the absence of a film-forming precursor, said reforming gas being composed primarily of He and/or H2; and
(iii) irradiating the reforming gas with microwaves in the reaction space having a pressure of 200 Pa or less to generate a direct microwave plasma to which the substrate is exposed, thereby reforming the silicon oxide film, wherein the microwaves have a frequency of 800 MHz or higher.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the substrate has a recess pattern on which the silicon oxide film is deposited.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in step (ii), only the reforming gas is supplied to the reaction space.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the reforming gas contains 0.1% to 99.9% by volume of He.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the reforming gas consists of He.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the reforming gas consists of H2.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the reforming gas contains less H2 than He by volume.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the microwaves have a frequency of 800 MHz to 10 GHz.

### Claim 9 (depends on 1)

The method according to claim 1, wherein microwave power of emitting the microwaves is 500 W to 10,000 W.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the substrate is placed on a susceptor, and the microwaves are emitted from an antenna provided above the susceptor in the reaction space.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the antenna is a pole-type antenna, and no RF power is supplied to the susceptor in step (iii).

### Claim 12 (depends on 1)

The method according to claim 1, wherein the pressure in step (iii) is 1 Pa to 30 Pa.

### Claim 13 (depends on 1)

The method according to claim 1, wherein step (iii) is conducted at a temperature of 20° C. to 400° C.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the silicon oxide film has a thickness of 3 nm or more, and step (iii) continues until the silicon oxide film is reformed from its surface to a depth of 3 nm or more.

### Claim 15 (depends on 1)

The method according to claim 1, wherein in step (iii), reforming the silicon oxide is conducted by desorbing and releasing hydrogen from the silicon oxide film.

### Claim 16 (depends on 1)

The method according to claim 1, wherein in step (i), the silicon oxide film on the substrate provided in the reaction space is a silicon oxide film deposited by plasma-enhanced ALD (PEALD) in a PEALD apparatus, and then transferred to the reaction space in a microwave plasma apparatus without exposing the substrate to air.

### Claim 17 (depends on 15)

The method according to claim 15, wherein steps (i) to (iii) are continuously repeated until a desired thickness of the reformed silicon oxide film is obtained.

### Claim 18 (depends on 2)

The method according to claim 2, wherein the recess pattern is constituted by trenches, each having a width of 10 nm to 60 nm, a depth of 30 nm to 300 nm, and an aspect ratio of 3 to 10.

### Claim 19 (depends on 1)

The method according to claim 1, further comprising, after step (iii), subjecting the reformed silicon oxide film to wet etching.

### Claim 20 (depends on 1)

The method according to claim 1, which is conducted during a process of forming a 3D NAND flash memory.