# US 2019/0241750 A1 · Anticorrosion Layer and Process for Production Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0241750 A1
- Document ID: US20190241750A1
- Status: Published application
- Kind: A1
- Application number: 16/386,463
- Filed: 2019-04-17
- Published: 2019-08-08
- Earliest claimed: 2013-11-08
- Assignees: Epg (Engineered Nanoproducts Germany) AG
- Applicants: EPG Engineered nanoProducts Germany AG
- Inventors: Edwin Kroke; Stefan Pfeiffer
- Web page: https://patentgrep.com/patent/US20190241750A1

## CPC

- C09D 5/08: Anti-corrosive paints
- B05D 1/02: performed by spraying
- B05D 1/18: performed by dipping
- B05D 1/28: performed by transfer from the surfaces of elements carrying the liquid or other fluent material, e.g. brushes, pads, rollers
- C09D 183/04: Polysiloxanes
- C09D 183/06: containing silicon bound to oxygen-containing groups (C09D183/12 takes precedence)
- C23C 18/122: {Inorganic polymers, e.g. silanes, polysilazanes, polysiloxanes}
- C23C 18/1225: {Deposition of multilayers of inorganic material}
- C23C 18/1254: {Sol or sol-gel processing}
- C23C 18/1295: {with after-treatment of the deposited inorganic material}
- C08G 77/04: Polysiloxanes
- C08G 77/18: to alkoxy or aryloxy groups
- C23C 18/1241: {Metallic substrates}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

An anti-corrosion coating to protect against corrosion, comprising: a high-density protective coating on a substrate which is prone to corrosion, preferably metals and/or alloys thereof, containing pre-condensed coat-forming alkoxysilane precursors, wherein the molecules of the pre-condensed coat-forming alkoxysilane precursors are built up from monomer units selected from the group formed by coat-forming alkoxysilane precursors, wherein the molecules of the pre-condensed coat-forming alkoxysilane precursors are cross-linked with each other, wherein the high-density protective coating has a coating thickness of at least 50 μm. The high-density protective coating formed by an inorganic-organic hybrid material, which is preferably produced without solvents (i.e. without the addition of solvents, in particular organic solvents), is comprised of at least one coat-forming alkoxysilane precursor, in particular selected from the group formed by trialkoxysilane precursors.

## Claims

### Claim 1

A method for producing an anti-corrosion coating with a high-density protective coating on a substrate which is prone to corrosion, comprising the following steps:
a) providing an anti-corrosion protection formulation
b) wherein at least one coat-forming alkoxysilane precursor is reacted, without the addition of solvents, by adding water in a molar ratio of 3:1 to 1:1, under acidic pH conditions and at a temperature in the range 0° C. to 10° C., in order to form a pre-condensed coat-forming alkoxysilane precursor,
c) applying the anti-corrosion protection formulation to a substrate, and
d) curing the applied anti-corrosion protection formulation to form a high-density protective coating.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the acidic pH conditions for the production of a high-density protective coating are adjusted by adding hydrochloric acid, nitric acid, phosphoric acid or acetic acid as the acidic catalyst.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the alkoxysilane precursor used is methyltriethoxysilane and/or tetraethoxyorthosilicate and/or tetramethoxyorthosilicate and/or methyltrimethoxysilane and/or dimethyldiethoxysilane and/or phenyltriethoxysilane.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the anticorrosion protection formulation is applied by dip coating, drop application, trowelling or brush application.

### Claim 5 (depends on 1)

The method according to claim 1, wherein prior to application, the anti-corrosion protection formulation is mixed directly with spores of anti-MIC organisms.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the anti-corrosion protection formulation is cured by means of thermal curing at a temperature between 60° C. and 200° C. to form a high-density protective coating.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the anti-corrosion protection formulation is cured by means of chemically initiated curing by adding bases to a high-density protective coating.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the anti-corrosion protection formulation is applied by means of spray coating in an atomized spray.

### Claim 9 (depends on 1)

The method according to claim 1, wherein water is added in a stoichiometric ratio with respect to hydrolysable alkoxy groups of the coat forming alkokysilane precursor or added in a below-stoichiometric quantity, wherein the minimum quantity of water in this regard is not less than 50% of the maximum quantity, wherein the maximum molar quantity of water corresponds to the number of hydrolysable alkoxy groups.

### Claim 10 (depends on 1)

The method according to claim 1, wherein a porous coating system is applied to the protective coating by means of the following steps:
a) providing a formulation for the porous coating system
b) wherein an ammoniacal solution is added to at least one coat-forming alkoxysilane precursor without the addition of solvents, adding water in a molar ratio of 1:1 to 1:3, at ambient temperature and with stirring,
c) applying the formulation for the porous coating system to the protective coating and
d) curing the applied formulation for the porous coating system.

### Claim 11 (depends on 10)

The method according to claim 10, wherein water is added in a stoichiometric ratio with respect to hydrolysable alkoxy groups of the coat forming alkokysilane precursor or added in a below-stoichiometric quantity, wherein the minimum quantity of water in this regard is not less than 50% of the maximum quantity, wherein the maximum molar quantity of water corresponds to the number of hydrolysable alkoxy groups.

### Claim 12 (depends on 10)

The method according to claim 10, wherein prior to application, the formulation for the porous coating system is mixed directly with anti-MIC organisms.

### Claim 13 (depends on 10)

The method according to claim 10, wherein after curing the formulation for the porous coating system, a bacterial suspension is applied to the porous coating system.

### Claim 14 (depends on 10)

The method according to claim 10, wherein a porous top coat is applied to the porous coating system by means of the following steps:
a) acidifying the formulation for the porous coating system as defined in step a) in claim 10,
b) applying the formulation for the porous top coat to the porous coating system, and
c) curing the applied formulation to form the porous top coat.

### Claim 15

A solvent-free anti-corrosion protection formulation comprising at least one pre-condensed coat-forming alkoxysilane precursor obtained by reacting:
at least one coat-forming alkoxysilane precursor without the addition of solvents,
by adding water in a molar ratio of 1:1 to 1:3,
under acidic pH conditions,
at a temperature in the range 0° C. to 10° C.

### Claim 16 (depends on 15)

The solvent-free anti-corrosion protection formulation according to claim 15, wherein the alkoxysilane precursor is methyltriethoxysilane and/or tetraethoxyorthosilicate and/or tetramethoxyorthosilicate and/or methyltrimethoxysilane and/or dimethyldiethoxysilane and/or phenyltriethoxysilane.

### Claim 17 (depends on 15)

The solvent-free anti-corrosion protection formulation according to claim 15, wherein after mixing all of the individual components and subsequent formation of the pre-condensed coat-forming alkoxysilane precursors, the volatile components of the formulation are removed from the anti-corrosion protection formulation.

### Claim 18 (depends on 15)

An anti-corrosion protection formulation comprising:
a) a solvent-free anti-corrosion protection formulation under acidic conditions as defined in claim 15 as component A, and
b) a component B containing a base, for chemically initiated curing.

### Claim 19 (depends on 18)

The anti-corrosion protection formulation according to claim 18, wherein the proportion by volume of the base in the component B is preferably 1% to 50% by volume.

### Claim 20 (depends on 18)

The anti-corrosion protection formulation according to claim 18, wherein the base for component B is an ammonium hydroxide solution, an amino-functionalized alkoxysilane, a basic amino acid or a primary, secondary or tertiary amine.