Novel Modified Acid Compositions as Alternatives to Conventional Acids in the Oil and Gas Industry
AssigneeFluid Energy Group Ltd.
InventorsClay Purdy, Markus Weissenberger
Life of this patent
Estimating the term…
Abstract
An aqueous modified acid composition for use in oil industry activities, said composition comprising: an amino acid, an alkanolamine and strong acid wherein the mineral acid:alkanolamine/amino acid are present in a molar ratio of not more than 15:1, preferably not more than 10:1; it can also further comprise a metal iodide or iodate. Said composition demonstrates advantages over known conventional acids and modified acids.
Claims22
An aqueous modified acid composition comprising:
- a mineral acid;
- an amino acid;
- and
- an alkanolamine;
- wherein the mineral acid:alkanolamine/amino acid are present in a molar ratio of not more than 15:1.
The use of an aqueous modified acid composition in an oil industry activity, said composition comprising:
- a mineral acid;
- an amino acid;
- and
- an alkanolamine;
- wherein the mineral acid:alkanolamine/amino acid are present in a molar ratio of not more than 15:1, and wherein the use comprises an activity selected from the group consisting of:
- stimulate formations;
- assist in reducing breakdown pressures during downhole pumping operations;
- treat wellbore filter cake post drilling operations;
- assist in freeing stuck pipe;
- descale pipelines and/or production wells;
- increase injectivity of injection wells;
- lower the pH of a fluid;
- remove undesirable scale on a surface selected from the group consisting of:
- equipment, wells and related equipment and facilities;
- fracture wells;
- complete matrix stimulations;
- conduct annular and bullhead squeezes & soaks;
- pickle tubing, pipe and/or coiled tubing;
- increase effective permeability of formations;
- reduce or remove wellbore damage;
- clean perforations;
- and solubilize limestone, dolomite, calcite and combinations thereof.
Method of treating a metal surface with a composition comprising
- a mineral acid;
- an amino acid;
- and
- an alkanolamine;
- wherein the mineral acid:alkanolamine/amino acid are present in a molar ratio of not more than 15:1, said method comprising the steps of:
- providing said composition;
- exposing said metal surface to said composition;
- allowing said composition a sufficient period of time to act upon said surface;
- and
- optionally, removing the acid composition when the exposure time has been determined to be sufficient for the operation to be complete or sufficiently complete.
Dependencies are inferred from the claim text.